Fatigue resistance of monolithic CAD/CAM ceramic crowns on human premolars

被引:36
|
作者
Homaei, Ehsan [1 ,5 ]
Farhangdoost, Khalil [1 ,5 ]
Pow, Edmond Ho Nang [2 ,6 ]
Matinlinna, Jukka Pekka [3 ,6 ]
Akbari, Majid [4 ]
Tsoi, James Kit-Hon [3 ,6 ]
机构
[1] Ferdowsi Univ Mashhad, Dept Mech Engn, Mashhad, Iran
[2] Univ Hong Kong, Oral Rehabil, Fac Dent, Hong Kong, Hong Kong, Peoples R China
[3] Univ Hong Kong, Dent Mat Sci, Fac Dent, Hong Kong, Hong Kong, Peoples R China
[4] Mashhad Univ Med Sci, Dent Res Ctr, Fac Dent, Azadi Sq, Mashhad, Iran
[5] Ferdowsi Univ Mashhad, Dept Mech Engn, Fac Engn, Azadi Sq, Mashhad, Iran
[6] Prince Philip Dent Hosp, 4-F,34 Hosp Rd, Hong Kong, Hong Kong, Peoples R China
关键词
Dental crowns; CAD/CAM ceramics; Cerec; Fatigue; Lithium disilicate; Polymer infiltrated ceramics; COMPOSITE RESIN; FRACTURE-RESISTANCE; FAILURE MODES; VENEERING PORCELAIN; OCCLUSAL VENEERS; NETWORK MATERIAL; CYCLIC FATIGUE; DENTAL CROWNS; CAD-CAM; RESTORATIONS;
D O I
10.1016/j.ceramint.2016.07.029
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The aim of this study was to determine the fatigue strength of two contemporary crown ceramics, lithium disilicate e.max (R) CAD (LD) and polymer-infiltrated ceramic Enamic (R) (PIC) and examine their failure mode. Twenty extracted human maxillary premolars were divided into two groups. The teeth were prepared and restored with either LD or PIC crowns. The restored teeth were subjected to cyclic chewing simulation (9 Hz). The sinusoidal loading was started with 500 N followed by a stepwise increase of 100 N for every 100,000 cycles until fracture occurred or, alternatively, after one million cycles. The Kaplan-Meier survival analysis was applied on fatigue loadings. Differences in the failure modes were analyzed by Fisher Exact tests. The average failure load of LD group was 1400 N (904,728 cycles) with 70% survival rate, while the average failure load of PIC group was 870 N (378,167 cycles) with 0% survival. Regarding the failure mode in both test groups, the crowns tended to fail above the cementoenamel junction (CEJ) and both combined adhesive and cohesive failure mode were commonly observed rather than cohesive failure. No significant difference was found between the test groups. The failures were initiated from a contact point or central fossa. The fatigue resistance of LD crowns on premolars was significantly higher than the PIC ceramic crowns. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:15709 / 15717
页数:9
相关论文
共 50 条
  • [1] Numerical fatigue analysis of premolars restored by CAD/CAM ceramic crowns
    Homaei, Ehsan
    Jin, Xiao-Zhuang
    Pow, Edmond Ho Nang
    Matinlinna, Jukka Pekka
    Tsoi, James Kit-Hon
    Farhangdoost, Khalil
    DENTAL MATERIALS, 2018, 34 (07) : E149 - E157
  • [2] Fatigue Resistance and Microleakage of CAD/CAM Ceramic and Composite Molar Crowns
    Kassem, Amr S.
    Atta, Osama
    El-Mowafy, Omar
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2012, 21 (01): : 28 - 32
  • [3] The Marginal Fit of CAD/CAM Monolithic Ceramic and Metal-Ceramic Crowns
    Freire, Yolanda
    Gonzalo, Esther
    Lopez-Suarez, Carlos
    Suarez, Maria J.
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2019, 28 (03): : 299 - 304
  • [4] The aesthetics of all-ceramic veneered and monolithic CAD/CAM crowns
    Herrguth, M
    Wichmann, M
    Reich, S
    JOURNAL OF ORAL REHABILITATION, 2005, 32 (10) : 747 - 752
  • [5] Fatigue resistance of anterior monolithic crowns produced from CAD-CAM materials: An in vitro study
    Choo, Seung-Sik
    Ko, Kyung-Ho
    Huh, Yoon-Hyuk
    Park, Chan-Jin
    Cho, Lee-Ra
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 130 (04): : 620 - 628
  • [6] Fatigue resistance of CAD/CAM resin composite molar crowns
    Shembish, Fatma A.
    Tong, Hui
    Kaizer, Marina
    Janal, Malvin N.
    Thompson, Van P.
    Opdam, Niek J.
    Zhang, Yu
    DENTAL MATERIALS, 2016, 32 (04) : 499 - 509
  • [7] Fracture Load of Monolithic CAD/CAM Ceramic Crowns Placed on Different Implant Abutments
    Meneghetti, Priscila Ceolin
    Pittas do Canto, Paulo Eduardo
    Spohr, Ana Maria
    Burnett Junior, Luiz Henrique
    INTERNATIONAL JOURNAL OF ORAL & MAXILLOFACIAL IMPLANTS, 2022, 37 (06) : 1217 - 1222
  • [8] The flexural strength of CAD/CAM polymer crowns and the effect of artificial ageing on the fracture resistance of CAD/CAM polymer and ceramic single crowns
    Anna Winter
    Axel Schurig
    Engelke Rasche
    Franziska Rösner
    Lisa Kanus
    Marc Schmitter
    Journal of Materials Science: Materials in Medicine, 2020, 31
  • [9] The flexural strength of CAD/CAM polymer crowns and the effect of artificial ageing on the fracture resistance of CAD/CAM polymer and ceramic single crowns
    Winter, Anna
    Schurig, Axel
    Rasche, Engelke
    Roesner, Franziska
    Kanus, Lisa
    Schmitter, Marc
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2019, 31 (01)
  • [10] Fatigue performance of adhesively luted glass or polycrystalline CAD-CAM monolithic crowns
    Alves, Daniela Meira
    Cadore-Rodrigues, Ana Carolina
    Prochnow, Catina
    de Lima Burgo, Thiago Augusto
    Spazzin, Aloisio Oro
    Bacchi, Atais
    Valandro, Luiz Felipe
    Rocha Pereira, Gabriel Kalil
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 126 (01): : 119 - 127