Deformation behavior of a zirconium based metallic glass during cylindrical indentation: in situ observations

被引:16
作者
Antoniou, A [1 ]
Bastawros, AF [1 ]
Lo, CCH [1 ]
Biner, SB [1 ]
机构
[1] Iowa State Univ, Ames Lab, Ames, IA 50011 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2005年 / 394卷 / 1-2期
基金
美国国家科学基金会;
关键词
indentation; metallic glass; shear bands;
D O I
10.1016/j.msea.2004.11.031
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
An experimental methodology was developed which is simple and yet accurately elucidates the stress-state dependency of the deformation behavior of metallic glasses or similar amorphous systems. The methodology includes in situ observations of the evolution of the deformation behavior of metallic glasses under a cylindrical indenter. The set-up not only collects information on the load-displacement response of the system to the deformation, but also resolves the much-needed information on the temporal and spatial evolution of the shear bands. By employing various indenter radii, the critical shear stress for the nucleation of the shear bands is obtained. Experimental results for a zirconium based metallic glass where found to be consistently independent of the indenter radius and in close agreement with the uniaxial yield values. (c) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:96 / 102
页数:7
相关论文
共 19 条
[1]  
BINER SB, 2003, SESS BULK MET GLASS
[2]   DEFORMATION-INDUCED NANOCRYSTAL FORMATION IN SHEAR BANDS OF AMORPHOUS-ALLOYS [J].
CHEN, H ;
HE, Y ;
SHIFLET, GJ ;
POON, SJ .
NATURE, 1994, 367 (6463) :541-543
[3]   PLASTIC-FLOW AND FRACTURE OF PD40NI40P20 METALLIC-GLASS UNDER AN INDENTOR [J].
DONOVAN, PE .
JOURNAL OF MATERIALS SCIENCE, 1989, 24 (02) :523-535
[4]  
GEER AL, IN PRESS MAT SCI E A
[5]   Serrated plastic flow during nanoindentation of a bulk metallic glass [J].
Golovin, YI ;
Ivolgin, VI ;
Khonik, VA ;
Kitagawa, K ;
Tyurin, AI .
SCRIPTA MATERIALIA, 2001, 45 (08) :947-952
[6]   Inhomogeneous deformation in metallic glasses [J].
Huang, R ;
Suo, Z ;
Prevost, JH ;
Nix, WD .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2002, 50 (05) :1011-1027
[7]   Subsurface deformation during Vickers indentation of bulk metallic glasses [J].
Jana, S ;
Ramamurty, U ;
Chattopadhyay, K ;
Kawamura, Y .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 375 :1191-1195
[8]   Effect of strain rate on the formation of nanocrystallites in an Al-based amorphous alloy during nanoindentation [J].
Jiang, WH ;
Pinkerton, FE ;
Atzmon, M .
JOURNAL OF APPLIED PHYSICS, 2003, 93 (11) :9287-9290
[9]   Rate dependence of serrated flow in a metallic glass [J].
Jiang, WH ;
Atzmon, M .
JOURNAL OF MATERIALS RESEARCH, 2003, 18 (04) :755-757
[10]  
Johnson KL., 1985, CONTACT MECH