Anisotropic tensile behavior of Ti-47Al-2Cr-2Nb alloy fabricated by direct laser deposition

被引:54
作者
Zhang, Xinyu [1 ]
Li, Chuanwei [2 ]
Zheng, Mengyao [1 ]
Ye, Zhenhua [1 ]
Yang, Xudong [1 ]
Gu, Jianfeng [1 ,3 ]
机构
[1] Shanghai Jiao Tong Univ, Inst Mat Modificat & Modelling, Sch Mat Sci & Engn, Shanghai 200240, Peoples R China
[2] Shanghai Jiao Tong Univ, Mat Genome Initiat Ctr, Shanghai 200240, Peoples R China
[3] Shanghai Jiao Tong Univ, Shanghai Key Lab Mat Laser Proc & Modificat, Shanghai 200240, Peoples R China
基金
中国国家自然科学基金;
关键词
TiAl alloy; Direct laser deposition; Anisotropic tensile behavior; Deformation mechanism; Fracture mechanism; MECHANICAL-PROPERTIES; TI-45AL-2CR-5NB ALLOY; PHASE-TRANSFORMATION; EQUIAXED TRANSITION; TEXTURE EVOLUTION; GRAIN-REFINEMENT; CRYSTAL-GROWTH; HEAT-TREATMENT; TIAL ALLOYS; MICROSTRUCTURE;
D O I
10.1016/j.addma.2020.101087
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Additive manufacturing is emerging as an increasingly promising technology for TiAl alloys, which are attracting significant attention for their special microstructure and mechanical properties. In the present study, direct laser deposition was applied to fabricate single-track Ti-47Al-2Cr-2Nb alloy walls with a back-and-forth scanning strategy. The resulting alternative-band microstructure, comprising complicated microstructure bands and coarse lamellar colony bands, was characterized, and electronic back-scatter diffraction analysis showed that the lamellae in coarse colonies present a consistent orientation, nearly parallel to the substrate. The tensile properties of the as-deposited specimens varied greatly with the angle (theta) between the loading direction and the substrate. The specimens exhibited the best comprehensive tensile properties of the maximum ultimate strength and elongation (706 MPa and 0.51 %) with the loading direction parallel to the substrate (theta= 0 degrees). The ultimate strength and elongation dropped to minimum values of 273 MPa and 0.16 %, respectively, when the loading direction was perpendicular to the substrate (theta= 90 degrees). At the middle state of loading direction, theta= 45 degrees, the ultimate strength decreased to 358 MPa, and the elongation remained as high as 0.49 %. Transmission electron microscopy observations revealed that dislocations and deformation twinning were both activated under different loading modes, and their morphologies were dramatically different. The formation mechanism of the alternative-band microstructure was proposed from the aspects of rapid solidification and the cyclic heat-treatment effect, and its possible fracture mechanism and crack propagation mode were discussed.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Ti-48Al-2Cr-2Nb alloys prepared by electron beam selective melting additive manufacturing: Microstructural and tensile properties
    Feng, Jiawen
    Gui, Wanyuan
    Liu, Qian
    Bi, Wenya
    Ren, Xuechong
    Liang, Yongfeng
    Lin, Junpin
    Luan, Benli
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 9357 - 9369
  • [42] In situ Observation of the Initial Stage of γ Lamella Formation in Ti48Al2Cr2Nb Alloy
    Li, Xiaolei
    Li, Jinshan
    Kou, Hongchao
    Song, Lin
    ADVANCED ENGINEERING MATERIALS, 2017, 19 (05)
  • [43] Tensile properties of Ti-48Al-2Cr-2Nb alloy having similarly oriented lamellae with fine lamellar spacing facilitated by suction casting
    Xia, Zhizhou
    Cui, Yuyou
    Shen, Yingying
    Arroussi, Mohammed
    Liu, Ronghua
    Yang, Liang
    Jia, Qing
    Yang, Rui
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 830
  • [44] Microstructure and Mechanical Properties ofAs-forgedTi-47Al-2Cr-2Nb-Y Alloy
    Zhang, Shuzhi
    Kong, Fantao
    Chen, Yuyong
    Xiao, Shulong
    Cao, Chao
    ADVANCED MATERIALS AND PROCESSES, PTS 1-3, 2011, 311-313 : 1873 - +
  • [45] High cycle fatigue behaviors and deformation mechanisms in Ti47Al2Cr2Nb alloy at room temperature and 700 °C
    Yu, Wen
    Yin, Yajun
    Zhou, Jianxin
    Li, Wen
    Zuo, Jiabin
    Lin, Junpin
    Feng, Xin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 21 : 2642 - 2652
  • [46] Experimental and Thermal Stress Field Numerical Simulation Study on Laser Metal Deposition of Ti-48Al-2Cr-2Nb Alloy
    Li, Xiaolei
    Zhao, Sen
    Yuan, Gang
    Cui, Lujun
    Guo, Shirui
    Zheng, Bo
    Cui, Yinghao
    Chen, Yongqian
    Zhao, Yue
    Xu, Chunjie
    MATERIALS, 2024, 17 (10)
  • [47] High temperature tensile properties and fracture behavior of Y2O3-bearing Ti-48Al-2Cr-2Nb alloy
    Guo, Yingfei
    Xiao, Shulong
    Chen, Yuyong
    Tian, Jing
    Zheng, Zhuangzhuang
    Xu, Lijuan
    INTERMETALLICS, 2020, 126 (126)
  • [48] Grain refinement and improved tensile properties of Ti5Al2Sn2Zr4Mo4Cr titanium alloy fabricated by laser solid forming
    Zhang, Siyu
    Zhang, Qiang
    Zheng, Min
    Hu, Yunlong
    Sui, Shang
    Chen, Jing
    Lin, Xin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 800
  • [49] Microstructure, texture and tensile properties as a function of laser power of Ti48Al2Cr2Nb5Ta alloy prepared by laser additive manufacturing
    Liu, Zhanqi
    Yin, Guili
    Zhu, Xiaoou
    Zhou, Qi
    JOURNAL OF MANUFACTURING PROCESSES, 2022, 73 : 624 - 632
  • [50] Investigation on Cracking Behavior and Development of a Fracture Model of Ti-47Al-2Nb-2Cr Alloy During Hot Deformation
    Cao, Zhuohan
    Sun, Yu
    Wan, Zhipeng
    Hu, Lianxi
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (10) : 5360 - 5369