Effects of oxidation of SiC aggregates on the microstructure and properties of bauxite-SiC composite refractories

被引:24
作者
Ren Bo [1 ]
Sang Shaobai [1 ]
Li Yawei [1 ]
Xu Yibiao [1 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Peoples R China
关键词
Refractories; Silicon carbide; Bauxite; Active oxidation; HIGH-TEMPERATURE OXIDATION; PARTICLE-SIZE; BEHAVIOR; PRESSURE;
D O I
10.1016/j.ceramint.2014.10.114
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Bauxite-SiC composite refractories are widely used in the transition zone of cement rotary kilns, whose properties (e.g. strength, abrasion and thermal shock resistance) are mainly associated with the nature of the interfacial bonding between SiC and the matrix of refractories. In the present paper, the effects of oxidation of SiC aggregates on the microstructure, and properties of bauxite SiC composite refractories during the firing process were investigated by means of X-ray diffraction (XRD) and scanning electron microscopy (SEM) as well as the thermodynamics analysis. The results show that the oxidation of SiC aggregates is closely associated with oxygen partial pressure in preparation of bauxite-SiC specimens, and can markedly affect the microstructure and properties of bauxite SiC refractories. The active oxidation of SiC aggregates takes place when the oxygen partial pressure is lower than 10(-15) atm at 1500 degrees C. Consequently, large interstices between SiC aggregates and matrix of bauxite SiC specimens occur. However, strong interfacial bonding between SiC aggregates and matrix can be produced as Si, SiC powder and their combination are added. As a result, the strength of bauxite SiC specimens could be greatly improved. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:2892 / 2899
页数:8
相关论文
共 32 条
  • [1] Akira Y, 1993, PRACTICAL THERMODYNA, P39
  • [2] Investigation of alkali induced corrosion of SiC filter candles at high temperature, in gasification environment
    Blaesing, Marc
    Schaafhausen, Sarah
    Mueller, Michael
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2014, 34 (04) : 1041 - 1044
  • [3] High temperature oxidation of SiC under helium with low-pressure oxygen. Part 2: CVD β-SiC
    Charpentier, L.
    Balat-Pichelin, M.
    Glenat, H.
    Beche, E.
    Laborde, E.
    Audubert, F.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (12) : 2661 - 2670
  • [4] High temperature oxidation of SiC under helium with low-pressure oxygen-Part 1: Sintered α-SiC
    Charpentier, L.
    Balat-Pichelin, M.
    Audubert, F.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (12) : 2653 - 2660
  • [5] Influence of alumina on the passive oxidation at low oxygen pressure of hot-pressed α-SiC
    Charpentier, Ludovic
    Maitre, Alexandre
    Balat-Pichelin, Marianne
    Foucaud, Sylvie
    Audubert, Fabienne
    [J]. SCRIPTA MATERIALIA, 2009, 60 (07) : 481 - 484
  • [6] Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites
    Cheng, LF
    Xu, YD
    Zhang, LT
    Luan, XG
    [J]. CARBON, 2002, 40 (12) : 2229 - 2234
  • [7] Oxidation resistance of highly porous CVD-SiC coated Tyranno fiber composites
    Cocera, N.
    Remirez de Esparza, N.
    Ocana, I.
    Sanchez, J. M.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2011, 31 (06) : 1155 - 1164
  • [8] High temperature oxidation of SiC under helium with low-pressure oxygen. Part 3: β-SiC-SiC/PyC/SiC
    Dawi, K.
    Balat-Pichelin, M.
    Charpentier, L.
    Audubert, F.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (02) : 485 - 494
  • [9] Investigation of thermal oxidation of Al2O3-coated SiC powder
    Dey, Atanu
    Kayal, Nijhuma
    Molla, Atiar Rahaman
    Chakrabarti, Omprakash
    [J]. THERMOCHIMICA ACTA, 2014, 583 : 25 - 31
  • [10] Behavior of SiC at high temperature under helium with low oxygen partial pressure
    Eck, J.
    Balat-Pichelin, M.
    Charpentier, L.
    Beche, E.
    Audubert, F.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2008, 28 (15) : 2995 - 3004