Large plastic deformation blistering and helium retention in 5% tantalum doped tungsten under 60 keV helium ions implantation

被引:17
作者
Zhou, Hang [1 ]
Yu, Jiangang [1 ]
Han, Wenjia [1 ]
Cheng, Long [1 ]
Chen, Changan [2 ]
Zhu, Kaigui [1 ,3 ]
机构
[1] Beihang Univ, Dept Phys, Beijing 100191, Peoples R China
[2] Acad Engn Phys China, Jiangyou, Sichuan, Peoples R China
[3] Beihang Univ, Beijing Key Lab Adv Nucl Energy Mat & Phys, Beijing 100191, Peoples R China
基金
中国国家自然科学基金;
关键词
Helium ions implantation; Large plastic blisters; Tantalum atomic clusters; HenTakVm complexes; Helium retention; DEUTERIUM RETENTION; LOW-ENERGY; HYDROGEN; DAMAGE; MICROSTRUCTURE; IRRADIATION;
D O I
10.1016/j.fusengdes.2018.06.014
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
Tantalum (5 mass-% Ta) doped tungsten and pure tungsten in comparison were exposed to 60 keV helium ions implantation with a fluence of 1.04 x 10(22) ion m(-2). It was obvious that the W-5%Ta featured large plastic blisters both in number and in size were significantly reduced. The reason for this phenomenon was that vacancies and their complexes introduced by tantalum dopants reduced the diffusion coefficient of vacancy and vacancy-helium complexes. On the other hand, tantalum formed atomic clusters in the tungsten matrix, becoming a second phase with higher helium trapping ability, which inhibited migration and growth of helium bubbles, preventing the formation of large helium bubbles. Furthermore, helium ions form HenTakVm complexes in W-5%Ta during 60 keV helium ions implantation, which affected the characteristics of gas release in tungsten and the helium retention of W-5%Ta was larger than pure W.
引用
收藏
页码:43 / 50
页数:8
相关论文
共 27 条
[1]  
Abromeit C., 1986, VACANCIES INTERSTIT, P3
[2]   Deuterium retention in tungsten damaged with W ions to various damage levels [J].
Alimov, V. Kh. ;
Hatano, Y. ;
Tyburska-Pueschel, B. ;
Sugiyama, K. ;
Takagi, I. ;
Furuta, Y. ;
Dorner, J. ;
Fusseder, M. ;
Isobe, K. ;
Yamanishi, T. ;
Matsuyama, M. .
JOURNAL OF NUCLEAR MATERIALS, 2013, 441 (1-3) :280-285
[3]   The effect of displacement damage on deuterium retention in ITER-grade tungsten exposed to low-energy, high-flux pure and helium-seeded deuterium plasmas [J].
Alimov, V. Kh. ;
Tyburska-Pueschel, B. ;
Hatano, Y. ;
Roth, J. ;
Isobe, K. ;
Matsuyama, M. ;
Yamanishi, T. .
JOURNAL OF NUCLEAR MATERIALS, 2012, 420 (1-3) :370-373
[4]   Microstructure and helium irradiation performance of high purity tungsten processed by cold rolling [J].
Chen, Zhe ;
Han, Wenjia ;
Yu, Jiangang ;
Kecskes, Laszlo ;
Zhu, Kaigui ;
Wei, Qiuming .
JOURNAL OF NUCLEAR MATERIALS, 2016, 479 :418-425
[5]   Effect of 800 keV argon ions pre-damage on the helium blister formation of tungsten exposed to 60 keV helium ions [J].
Chen, Zhe ;
Han, Wenjia ;
Yu, Jiangang ;
Zhu, Kaigui .
JOURNAL OF NUCLEAR MATERIALS, 2016, 472 :110-117
[6]   Plasma-material interactions in current tokamaks and their implications for next step fusion reactors [J].
Federici, G ;
Skinner, CH ;
Brooks, JN ;
Coad, JP ;
Grisolia, C ;
Haasz, AA ;
Hassanein, A ;
Philipps, V ;
Pitcher, CS ;
Roth, J ;
Wampler, WR ;
Whyte, DG .
NUCLEAR FUSION, 2001, 41 (12R) :1967-2137
[7]   Thermal desorption and surface modification of He+ implanted into tungsten [J].
Fu, Z ;
Yoshida, N ;
Iwakiri, H ;
Xu, ZY .
JOURNAL OF NUCLEAR MATERIALS, 2004, 329 :692-696
[8]   Mass flow facilitates tungsten blistering under 60 keV helium ion implantation [J].
Han, Wenjia ;
Yu, Jiangang ;
Chen, Zhe ;
Lu, Guanghong ;
Zhu, Kaigui .
NUCLEAR FUSION, 2017, 57 (07)
[9]  
Kahn B.A., 1996, EFF RAD MAT 17 INT S, P1013
[10]   Microstructure development and helium behavior in nickel and vanadium base alloys [J].
Kalashnikov, AN ;
Chernov, II ;
Kalin, BA ;
Binyukova, SY .
JOURNAL OF NUCLEAR MATERIALS, 2002, 307 :362-366