Optimisation of selective laser melting parameters for the Ni-based superalloy IN-738 LC using Doehlert's design

被引:99
作者
Perevoshchikova, Nataliya [1 ]
Rigaud, Jordan [2 ]
Sha, Yu [3 ]
Heilmaier, Martin [4 ]
Finnin, Barrie [3 ]
Labelle, Elena [3 ]
Wu, Xinhua [3 ]
机构
[1] Monash Univ, Dept Mat Sci & Engn, Clayton, Vic, Australia
[2] Ecole Natl Super Ingenieurs Arts, Chim & Technol, Toulouse, France
[3] Monash Univ, Monash Ctr Addit Mfg, Clayton, Vic, Australia
[4] Karlsruher Inst Technol, IAM, Karlsruhe, Germany
关键词
Additive manufacturing; Experimental design; Selective laser melting; Ni-based superalloys; Powder metallurgy; HEAT-AFFECTED ZONE; THERMO-CALC; ALLOY; MICROSTRUCTURE; LIQUATION; SLM; BEHAVIOR; DICTRA; GAMMA;
D O I
10.1108/RPJ-04-2016-0063
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Purpose -The Ni-based superalloy IN-738 LC is known to be susceptible to porosity and different types of cracking during the build-up process and, thus, challenging to manufacture using selective laser melting ( SLM). Determining a feasible set of operating parameters for SLM of nickel-based superalloys involves new approach to experimental design based on the Doehlert method that assists in determining an optimal ( feasible) set of operating parameters for SLM of IN-738 LC powder alloy. Design/methodology/approach - The SLM parameters are evaluated in terms of their effectiveness in obtaining the microstructure with a porosity content of <0.5 per cent and without micro-cracking. The experimental approach is exemplified with the Doehlert matrix response variable, relative density, by comparing Archimedes method with microstructural assessments of pores and cracks from image analysis. The effect of heat treatment ( HT) and hot isostatic pressing ( HIP) on the microstructure of the SLMed IN-738 LC powder alloy has been examined and the consequential tensile response characterised. Findings - By using optimised process parameters ( low heat input, medium scanning speed and small hatching distance) which provides medium energy density, samples of IN-738 LC with a macroscopic porosity <0.5 per cent and free of micro-cracks can be manufactured by SLM. The results indicate that HIP of SLMed material did not lead to a noticeable effect on mechanical properties compared to HT of SLMed material suggesting that the level of both porosity and crack density might be already below the detection limit for the mere heat-treated material. Originality/value - SLM processing parameters ( power, scan speed, hatching distance) for IN-738 LC were successfully optimised after only 14 experiments using Doehlert design. Two methods Archimedes method and image analysis were used in this study to assess relative density of SLM-produced samples with sets of processing parameters showing coherency in prediction with predicted response by Doehlert design.
引用
收藏
页码:881 / 892
页数:12
相关论文
共 36 条
[1]  
Alloy, 2017, IN738 INT NICK CO
[2]  
American Society for Testing and Materials (ASTM), 2014, B96213 ASTM
[3]   THERMO-CALC & DICTRA, computational tools for materials science [J].
Andersson, JO ;
Helander, T ;
Höglund, LH ;
Shi, PF ;
Sundman, B .
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2002, 26 (02) :273-312
[4]  
[Anonymous], 16 INT S EL SHANGH
[5]  
[Anonymous], [No title captured]
[6]   The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy [J].
Carter, Luke N. ;
Martin, Christopher ;
Withers, Philip J. ;
Attallah, Moataz M. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 615 :338-347
[7]   Investigations on the microstructure and crack formation of IN738LC samples processed by selective laser melting using Gaussian and doughnut profiles [J].
Cloots, Michael ;
Uggowitzer, Peter J. ;
Wegener, Konrad .
MATERIALS & DESIGN, 2016, 89 :770-784
[8]  
Dantzig J. A., 2009, SOLIDIFICATION
[9]  
Decker R. F., 1957, 57 U MICH ENG RES I
[10]  
DOEHLERT DH, 1970, ROY STAT SOC C-APP, V19, P231