Fretting wear behavior of Ti/TiN multilayer film on uranium surface under various displacement amplitudes

被引:6
作者
Wu, Yan-ping [1 ]
Li, Zheng-yang [2 ]
Yang, Wen-jin [2 ]
Zhu, Sheng-fa [1 ]
Meng, Xian-dong [1 ]
Cai, Zhen-bing [2 ]
机构
[1] China Acad Engn Phys, Inst Mat, Mianyang 621900, Peoples R China
[2] Southwest Jiaotong Univ, Tribol Res Inst, Minist Educ, Key Lab Adv Mat Technol, Chengdu 610031, Sichuan, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti/TiN multilayer film; fretting wear; wear mechanism; displacement amplitude; MECHANICAL-PROPERTIES; HIGH-TEMPERATURE; PARTIAL SLIP; TI-TIN; COATINGS; ALLOY; ENVIRONMENTS; CRN;
D O I
10.1016/S1003-6326(18)64801-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Ti/TiN multilayer film was deposited on uranium surface by arc ion plating technique to improve fretting wear behavior. The morphology, structure and element distribution of the film were measured by scanning electric microscopy (SEM), X-ray diffractometry (XRD) and Auger electron spectroscopy (AES). Fretting wear tests of uranium and Ti/TiN multilayer film were carried out using pin-on-disc configuration. The fretting tests of uranium and Ti/TiN multilayer film were carried out under normal load of 20 N and various displacement amplitudes ranging from 5 to 100 mu m. With the increase of the displacement amplitude, the fretting changed from partial slip regime (PSR) to slip regime (SR). The coefficient of friction (COF) increased with the increase of displacement amplitude. The results indicated that the displacement amplitude had a strong effect on fretting wear behavior of the film. The damage of the film was very slight when the displacement amplitude was below 20 mu m. The observations indicated that the delamination was the main wear mechanism of Ti/TiN multilayer film in PSR. The main wear mechanism of Ti/TiN multilayer film in SR was delamination and abrasive wear.
引用
收藏
页码:1593 / 1601
页数:9
相关论文
共 26 条
[21]   Fretting wear behavior of Inconel 690 in hydrazine environments [J].
Zhang, Xiao-yu ;
Ren, Ping-di ;
Peng, Jin-fang ;
Zhu, Min-hao .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (02) :360-367
[22]   Fretting wear and friction oxidation behavior of 0Cr20Ni32AlTi alloy at high temperature [J].
Zhang Xiao-yu ;
Ren Ping-di ;
Zhong Fa-chun ;
Zhu Min-hao ;
Zhou Zhong-rong .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 (04) :825-830
[23]   Characterization of Fretting Fatigue Behavior of TiN/Ti Coating on Ti-811 Alloy at Increased Temperature [J].
Zhang, Xiaohua ;
Pan, Feng ;
Xiang, Dinggen .
PROCEEDINGS OF THE FIRST SYMPOSIUM ON AVIATION MAINTENANCE AND MANAGEMENT-VOL II, 2014, 297 :699-705
[24]   Cracking induced by fretting of aluminium alloys [J].
Zhou, ZR ;
Vincent, L .
JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 1997, 119 (01) :36-42
[25]   On the mechanisms of various fretting wear modes [J].
Zhu, M. H. ;
Zhou, Z. R. .
TRIBOLOGY INTERNATIONAL, 2011, 44 (11) :1378-1388
[26]   Microstructure and corrosion resistance of Cr/Cr2N multilayer film deposited on the surface of depleted uranium [J].
Zhu, Shengfa ;
Chen, Lin ;
Wu, Yanping ;
Hu, Yin ;
Liu, Tianwei ;
Tang, Kai ;
Wei, Qiang .
CORROSION SCIENCE, 2014, 82 :420-425