Stability of nanoparticles in water

被引:28
作者
Labille, Jerome [1 ,2 ]
Brant, Jonathan
机构
[1] CNRS, CEREGE, F-13545 Aix En Provence 04, France
[2] Aix Marseille Univ, F-13545 Aix En Provence 04, France
关键词
aggregation; dispersion; dissolution; hydrophobicity; surface charge; FULLERENE C-60 NANOPARTICLES; WALLED CARBON NANOTUBES; NATURAL ORGANIC-MATTER; AGGREGATION KINETICS; SURFACE-CHARGE; ZINC-OXIDE; AQUEOUS-SOLUTIONS; IONIC COMPOSITION; PARTICLE-SIZE; HUMIC-ACID;
D O I
10.2217/NNM.10.62
中图分类号
Q81 [生物工程学(生物技术)]; Q93 [微生物学];
学科分类号
071005 ; 0836 ; 090102 ; 100705 ;
摘要
Aqueous systems represent a likely carrier for manufactured nanoparticles upon their introduction into the natural environment. Their behavior in water, and in turn the risk that is posed by these materials to environmental and human communities, is a top concern. In terms of risk assessment, nanoparticle exposure to organisms is largely driven by their dispersion and behavior in aqueous systems, while their potential hazard, although not always well understood, is often related to their surface speciation. Both of these characteristics arise from the reactions that occur at the solid/liquid interface. The objective of this article is to establish the current state of the science with regard to the possible changes in surface properties and/or behavior of manufactured nanoparticles in different aqueous solutions of model and inorganic composition. The general reactions occurring at the nanoparticle/water interface, or between nanoparticles themselves, are first introduced. Following this, metal oxides, pure metals and carbon nanoparticles are considered on a case-by-case basis.
引用
收藏
页码:985 / 998
页数:14
相关论文
共 125 条
[1]   Correlation and prediction of the solubility of Buckminster-fullerene in organic solvents; estimation of some physicochemical properties [J].
Abraham, MH ;
Green, CE ;
Acree, WE .
JOURNAL OF THE CHEMICAL SOCIETY-PERKIN TRANSACTIONS 2, 2000, (02) :281-286
[2]  
Adamson A.W., 1967, Physical Chemistry of Surfaces
[3]   Nanotubes from carbon [J].
Ajayan, PM .
CHEMICAL REVIEWS, 1999, 99 (07) :1787-1799
[4]   ALIGNED CARBON NANOTUBE ARRAYS FORMED BY CUTTING A POLYMER RESIN-NANOTUBE COMPOSITE [J].
AJAYAN, PM ;
STEPHAN, O ;
COLLIEX, C ;
TRAUTH, D .
SCIENCE, 1994, 265 (5176) :1212-1214
[5]  
ANDRIEVSKY CV, 2002, CHEM PHYS LETT, V8, P3640
[6]   Is the C60 fullerene molecule toxic?! [J].
Andrievsky, G ;
Klochkov, V ;
Derevyanchenko, L .
FULLERENES NANOTUBES AND CARBON NANOSTRUCTURES, 2005, 13 (04) :363-376
[7]  
Andrievsky G.V., 1995, CHEM COMMUN, P1281
[8]   Study of the aggregation properties of a novel amphiphilic C60 fullerene derivative [J].
Angelini, G ;
De Maria, P ;
Fontana, A ;
Pierini, M ;
Maggini, M ;
Gasparrini, F ;
Zappia, G .
LANGMUIR, 2001, 17 (21) :6404-6407
[9]  
[Anonymous], 1948, Theory of the Stability of Lyophobic Colloids
[10]   In vitro interactions between DMSA-coated maghemite nanoparticles and human fibroblasts: A physicochemical and cyto-genotoxical study [J].
Auffan, Melanie ;
Decome, Laetitia ;
Rose, Jerome ;
Orsiere, Thierry ;
De Meo, Michel ;
Briois, Valerie ;
Chaneac, Corinne ;
Olivi, Luca ;
Berge-Lefranc, Jean-Louis ;
Botta, Alain ;
Wiesner, Mark R. ;
Bottero, Jean-Yves .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2006, 40 (14) :4367-4373