Infiltration of reinforcement materials in the oxidation behaviour and the mechanical properties to carbon fiber reinforced carbon matrix (C/C) composites

被引:0
作者
Jimenez, J. M. [1 ]
Calabres, R. [1 ]
Guzman, S. [1 ]
Mota, J. M. [1 ]
机构
[1] Univ Carlos III Madrid, Dpto Ciencia & Ingn Mat & Ingn Quim, Madrid 28911, Spain
来源
BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO | 2007年 / 46卷 / 04期
关键词
carbon/carbon composites; oxidation; mechanical properties; infiltration;
D O I
10.3989/cyv.2007.v46.i4.238
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the present study, attention was focused on the adaptation of different methods in order to incorporate reinforcement materials just like SiC and B,C to carbon fiber reinforced carbon matrix (C/C) composites. Hot petroleum pitch impregnation and also at room temperature, and toluene were used as drivers to, incorporate reinforcement materials and oxidation inhibitors, just like B2O3,H3BO3, and B4C to (C/C) matrix. Hermetic crucibles and graphite have been used in order to obtained carbonization process. Oxidizing atmospheres were used in order to improve the oxidation matrix after the carbonization process. Different methods of infiltration have been evaluated in order to test which of these produce bigger increment on mechanical properties and oxidation protection of the final materials. The different tested materials were studied by means of techniques like scanning electron microscopy (SEM) and micro-analysis by energy dispersive spectroscopy (EDS). Results of flexural test were finally compared.
引用
收藏
页码:205 / 212
页数:8
相关论文
共 15 条
  • [1] C/SiC composites for high temperature structural applications.: Part II:: Oxidation protection systems
    Aparicio, M
    Durán, A
    [J]. BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2001, 40 (01): : 7 - 15
  • [2] Bucley J.D., 1988, CERAM B, V67, P364
  • [3] INHIBITION OF THE OXIDATION OF CARBON CARBON COMPOSITE BY BORON-OXIDE
    EHRBURGER, P
    BARANNE, P
    LAHAYE, J
    [J]. CARBON, 1986, 24 (04) : 495 - 499
  • [4] JIQIAO L, 2002, CARBON, V40, P617
  • [5] SILICON-CARBIDE INFILTRATION OF POROUS C-C COMPOSITES FOR IMPROVING OXIDATION RESISTANCE
    LAMOUROUX, F
    BOURRAT, X
    NASLAIN, R
    THEBAULT, J
    [J]. CARBON, 1995, 33 (04) : 525 - 535
  • [6] Corrosion behaviour of 2124/SiC composite material
    López-Caballero, JA
    Martín, E
    Baile, MT
    Forn, A
    Bastidas, JM
    [J]. BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2005, 44 (06): : 393 - 398
  • [7] MARSH H, 1989, INTRODUCTION TO CARBON SCIENCE, P107
  • [8] BORATE TREATMENT OF CARBON-FIBERS AND CARBON-CARBON COMPOSITES FOR IMPROVED OXIDATION RESISTANCE
    MCKEE, DW
    [J]. CARBON, 1986, 24 (06) : 737 - 741
  • [9] OXIDATION-INHIBITION MECHANISMS IN COATED CARBON CARBON COMPOSITES
    NIXON, TD
    CAWLEY, JD
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (03) : 703 - 708
  • [10] Microestructure and mechanical properties of biomorphic SiC obtained from eucalyptus
    Presas, M
    Pastor, JY
    Llorca, J
    De Arellano-López, AR
    Martínez-Fernández, J
    Sepúlveda, YR
    [J]. BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2005, 44 (06): : 363 - 367