The Influence of the ZrO2 Solid Solution Amount on the Physicochemical Properties of Al2O3-ZrO2-Y2O3-CeO2 Powders

被引:13
作者
Smyrnova-Zamkova, M. Yu. [1 ]
Ruban, O. K. [1 ]
Bykov, O. I. [1 ]
Holovchuk, M. Ya. [2 ]
Mosina, T. V. [1 ]
Khomenko, O. I. [1 ]
Dudnik, E. V. [1 ]
机构
[1] Natl Acad Sci Ukraine, Frantsevich Inst Problems Mat Sci, Kiev, Ukraine
[2] Natl Acad Sci Ukraine, Karpenko Physicomech Inst, Lvov, Ukraine
关键词
Al2O3-ZrO2 (Y2O3; CeO2) system; ZTA composites; hydrothermal synthesis in alkaline environment; nanocrystalline powder; shape factor; ZrO2 solid solution; ZIRCONIA-TOUGHENED ALUMINA; ZTA; CE1-XZRXO2-DELTA; NANOCOMPOSITE; CERAMICS; CEO2;
D O I
10.1007/s11106-021-00222-4
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Alumina-based nanocrystalline powders with different ZrO2 amounts were produced for the first time by hydrothermal synthesis in an alkaline environment for designing zirconia toughened alumina (ZTA) composites. In ZTA composites, ZrO2 solid solution particles codoped with ceria and yttria are distributed in a rigid Al2O3 matrix. To examine the physicochemical properties, 90 wt.% Al2O3-10 wt.% ZrO2 (Y2O3, CeO2) and 58.5 wt.% Al2O3-42.5 wt.% ZrO2 (Y2O3, CeO2) powders were used. The ZrO2 solid solution had composition 90 mol.% ZrO2-2 mol.% Y2O3-8 mol.% CeO2. The hydrothermal powders were heat treated in the temperature range 400-1450 degrees C and examined by X-ray diffraction, differential thermal analysis, and electron microscopy. The powder specific surface area was determined by the BET method. The sizes of primary particles were determined with the Scherrer equation. The AMIC software (Automatic Microstructure Analyzer) was employed to process the morphology analysis results. The phase transformations and active sintering of the ZTA powders determined the dependences showing the sizes of primary particles and the specific surface area of the powders versus the heat treatment temperature. With higher ZrO2 content, temperature of the F-ZrO2 -> T-ZrO2 phase transformation decreased, the likelihood of M-ZrO2 to emerge increased, and the sequence of Al2O3 phase transformations changed after the boehmite had decomposed. The variation in the morphology and specific surface area of the powders in the heat treatment process indicated that their sintering activity increased. The dependence of the shape factor characterizing the nanocrystalline 90AZG and 58.5AZG powders on the heat treatment temperature was studied. The starting nanosized 90AZG and 58.5AZG powders had a similar distribution of agglomerates according to the shape factor. Round agglomerates and multifaceted regular agglomerates were predominant. The way in which the shape factor of the agglomerates varied with temperature was associated with a topochemical memory effect manifested by the 90AZG and 58.5AZG powders were examined. With increasing ZrO2 content, the microhardness of the ZTA composites decreased from 195 to 160 MPa, fracture toughness (KIc) increased from 6 to 8 MPa center dot m0.5, and Vickers hardness decreased from 8.3 to 5.6 GPa. The improvement in consolidation methods for ZTA composites will allow tool, structural, and functional ceramics with the required properties to be produced.
引用
收藏
页码:129 / 141
页数:13
相关论文
共 50 条
[41]   Interaction of SiC with Al2O3−(t + m)ZrO2(Y2O3) Oxide Composition [J].
M. G. Frolova ;
A. S. Lysenkov ;
S. N. Perevislov ;
N. V. Petrakova ;
K. A. Kim ;
M. A. Sevost’yanov ;
A. Yu. Ivannikov ;
M. D. Mel’nikov ;
Yu. F. Kargin .
Russian Journal of Inorganic Chemistry, 2023, 68 (8) :1077-1083
[42]   Directionally solidified eutectics in the Al2O3–ZrO2–Ln(Y)2O3 systems (Review) [J].
S. M. Lakiza .
Powder Metallurgy and Metal Ceramics, 2009, 48 :42-59
[43]   Effect of Adding Nanosize ZrO2 and Compaction Processing Parameters on Properties of Composites Based on Al2O3 and ZrO2 [J].
Zadorozhnaya, O. Yu. ;
Tiunova, O. V. ;
Bogaev, A. A. ;
Khabas, T. A. ;
Nepochatov, Yu. K. ;
Shkodkin, A. V. .
REFRACTORIES AND INDUSTRIAL CERAMICS, 2014, 54 (05) :392-396
[44]   Friction and wear properties of mullite/ZrO2/Al2O3 composites [J].
Tan, YF ;
Yu, AB ;
Liu, WM ;
Yan, J ;
Tan, H ;
Wang, XL .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2005, 15 (02) :464-467
[45]   Effect of Heat Treatment in the Temperature Range 400−1300°C on the Properties of Nanocrystalline ZrO2−Y2O3−CeO2 Powders [J].
I. O. Marek ;
O. V. Dudnik ;
S. A. Korniy ;
V. P. Red’ko ;
M. I. Danilenko ;
O. K. Ruban .
Powder Metallurgy and Metal Ceramics, 2021, 60 :385-395
[46]   Fabrication and characterization of spray dried Al2O3-ZrO2-Y2O3 powders treated by calcining and plasma [J].
Pan, Zhaoyi ;
Wang, You ;
Sun, Xiaoguang .
POWDER TECHNOLOGY, 2011, 212 (02) :316-326
[47]   Investigation into the solubility of nanopowders of the ZrO2-Y2O3-CeO2-Al2O3 system in the aqueous medium at various pH [J].
Makarova, E. N. ;
Antsiferova, I. V. .
RUSSIAN JOURNAL OF NON-FERROUS METALS, 2017, 58 (05) :525-529
[48]   Mechanical Properties of ZrO2 (Y2O3)-Al2O3 Nanocomposites with Addition of Hydroxyapatite Prepared by Spark Plasma Sintering [J].
Li, Shufeng ;
Lzui, Hiroshi ;
Okano, Michiharu ;
Zhang, Weihua ;
Watanabe, Taku .
MULTISCALE, MULTIFUNCTIONAL AND FUNCTIONALLY GRADED MATERIALS, 2010, 631-632 :413-+
[49]   MICROSTRUCTURE AND MECHANICAL PROPERTIES OF ZRO2(Y2O3)-AL2O3 NANO COMPOSITES PREPARED BY SPARK PLASMA SINTERING [J].
Li, Shufeng ;
Izui, Hiroshi ;
Okano, Michiharu ;
Zhang, Weihua ;
Watanabe, Taku .
MSEC 2008: PROCEEDINGS OF THE ASME INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE 2008, VOL 1, 2009, :111-116
[50]   Microwave hybrid sintering of Al2O3 and Al2O3-ZrO2 composites, and effects of ZrO2 crystal structure on mechanical properties, thermal properties, and sintering kinetics [J].
Khalid, Muhammad Waqas ;
Kim, Young Il ;
Haq, Muhammad Aneeq ;
Lee, Dongju ;
Kim, Bum Sung ;
Lee, Bin .
CERAMICS INTERNATIONAL, 2020, 46 (07) :9002-9010