Leaching behaviour of electrode materials of spent nickel-cadmium batteries in sulphuric acid media

被引:54
作者
Nogueira, CA [1 ]
Margarido, F
机构
[1] INETI, Estrada Paco Lumiar, P-1649038 Lisbon, Portugal
[2] Univ Tecn Lisboa, CVRM, Geosyst Ctr, Inst Super Tecn, P-1049001 Lisbon, Portugal
关键词
Ni-Cd batteries; recycling; leaching; nickel; cadmium; cobalt;
D O I
10.1016/S0304-386X(03)00123-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The improving awareness of environmental problems associated with the toxicity of heavy metals keeps the recycling of spent nickel-cadmium batteries an important assignment due to the presence of cadmium, nickel and cobalt on the electrode material. While cadmium from batteries is one of the major sources of cadmium contamination of the environment, the other heavy metals contained on the electrode material have a considerable economic value. Therefore a complete and valorising solution to the management of this type of residues is not possible through the existing pyrometallurgical processes because the treatment of complex materials in order to recycle all materials is difficult. An integrated process based on physical and hydroelectrometallurgical operations seems to be more efficient because it is possible to recover the three metals, Cd, Ni and Co, present on the electrode material. The study here presented deals with the first chemical stage of an integrated process, the leaching of spent nickel-cadmium electrodes with sulphuric acid. The electrode materials essentially composed of Ni, Cd and Co hydroxides were readily solubilised in 0.5 h with low acid concentrations (pH similar to 1) at ambient temperature. At higher pH values the solubilisation of metal hydroxides was inefficient, except when using long residence times. The leaching of nickel present in the metallic form, in the electrodes, was more difficult due to kinetic constraints, applying high temperature (e.g. 95degreesC) and acid concentration (e.g. 2.5 M H2SO4) in order to obtain complete conversions in acceptable time (similar to 4 h). (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:111 / 118
页数:8
相关论文
共 11 条
  • [1] BARRING NE, 1979, P 2 INT CADM C CANN, P105
  • [2] BARRING NE, 1983, P 4 INT CADM C MUN M, P58
  • [3] Cavallini M, 2000, FOURTH INTERNATIONAL SYMPOSIUM ON RECYCLING OF METALS AND ENGINEERED MATERIALS, PROCEEDINGS, P471
  • [4] Espinosa DCR, 2001, EPD CONGRESS 2001, P173
  • [5] HANEWALD RH, 1998, P 4 INT BATT REC C H
  • [6] LIMCK F, 1998, P 4 INT BATT REC C H
  • [7] New flowsheet for the recovery of cadmium, cobalt and nickel from spent Ni-Cd batteries by solvent extraction
    Nogueira, CA
    Delmas, F
    [J]. HYDROMETALLURGY, 1999, 52 (03) : 267 - 287
  • [8] OHIRA Y, 1986, P 5 INT CADM C SAN F, P41
  • [9] PONS C, 1997, P 3 ASM INT C REC ME, P487
  • [10] Pourbaix M., 1966, ATLAS ELECTROCHEMICA