Amorphous Si-B-C-N coatings for high-temperature oxidation protection of the γ-TiAl alloy

被引:9
|
作者
Simova, Veronika [1 ]
Knittel, Stephane [2 ]
Cavarroc, Marjorie [3 ]
Martinu, Ludvik [1 ]
Klemberg-Sapieha, Jolanta-Ewa [1 ,4 ]
机构
[1] Polytech Montreal, Dept Engn Phys, Montreal, PQ H3T 1J4, Canada
[2] SAFRAN Aircraft Engines, Site Evry Corbeil Rue Henri Auguste Desbrueres,BP8, F-91003 Evry, France
[3] SAFRAN Tech, Rue Jeunes Bois,CS 80112, F-78772 Magny Les Hameaux, France
[4] Polytech Montreal, Dept Engn Phys, 2900 Boul Edouard Montpetit, Montreal, PQ H3T 1J4, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
THERMAL-STABILITY; INTERMETALLIC COATINGS; NANOCOMPOSITE COATINGS; BEHAVIOR; RESISTANCE; FILMS; MICROSTRUCTURE; TI-45AL-8NB; KINETICS;
D O I
10.1016/j.surfcoat.2022.128544
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The present work focuses on the preparation of amorphous Si-B-C-N coatings to protect gamma-TiAl intermetallic alloys against oxidation above 750 ? that otherwise leads to surface degradation and embrittlement. The film fabrication process included the deposition of an amorphous Si interlayer at a temperature of 700 ? to promote adhesion. Subsequently, Si-B-C-N coatings were prepared by pulsed dc and rf magnetron co-sputtering from Si and B4C targets in Ar + N-2 gas mixtures. Specifically, we studied the oxidation behavior of the coatings and the evolution of the microstructure, composition, and mechanical properties upon an isothermal oxidation test performed in laboratory air at 800 ? for 100 h. We found that an optimized Si(4)0B(5)C(2)N(47) (at.%) coating protects the gamma-TiAl alloy substrate against oxidation by a combination of several effects: a) Interdiffusion of Si and Ti results in the formation of Ti(x)Si(y )phases on the film-substrate interface promoting adhesion of the coating, b) Diffusion of Ti to the surface is effectively inhibited and no fast-growing TiO2 is formed at the outer surface, and c) Stable amorphous structure of Si-B-C-N coatings hinders inward oxidation of O. Investigation of the oxidation kinetics at 800 ? up to 1000 h proved that Si-B-C-N coating serves as an efficient oxidation barrier demonstrated by the significantly reduced mass gain and the parabolic oxidation rate constant (1.05 x 10(-13) g(2).cm(-4).s(-1)) compared to the uncoated gamma-TiAl alloy (5.65 x 10(-13) g(2).cm(-4).s(-1)).
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Microstructure characterization of high-temperature, oxidation-resistant Si-B-C-N films
    He, Jie
    Zhang, Minghui
    Jiang, Jiechao
    Vlcek, Jaroslav
    Zeman, Petr
    Steidl, Petr
    Meletis, Efstathios I.
    THIN SOLID FILMS, 2013, 542 : 167 - 173
  • [2] Impact of Si on the high-temperature oxidation of AlCr(Si)N coatings
    Jaeger, Nikolaus
    Meindlhumer, Michael
    Zitek, Michal
    Spor, Stefan
    Hruby, Hynek
    Nahif, Farwah
    Julin, Jaakko
    Rosenthal, Martin
    Keckes, Jozef
    Mitterer, Christian
    Daniel, Rostislav
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 100 : 91 - 100
  • [3] Thermal stability and high-temperature oxidation behavior of Si-Cr-N coatings with high content of silicon
    Mikula, M.
    Grancic, B.
    Drienovsky, M.
    Satrapinskyy, L.
    Roch, T.
    Hajovska, Z.
    Gregor, M.
    Plecenik, T.
    Cicka, R.
    Plecenik, A.
    Kus, P.
    SURFACE & COATINGS TECHNOLOGY, 2013, 232 : 349 - 356
  • [4] Structure and High-Temperature Oxidation Performance of Si-Co Diffusion Coatings Prepared on a TiAl-Nb Alloy
    Tian, Jin
    Zhang, Conghui
    Lv, Wei
    Li, Xuan
    Tian, Wei
    COATINGS, 2023, 13 (08)
  • [5] Glass coatings on stainless steels for high-temperature oxidation protection: Mechanisms
    Chen, Minghui
    Li, Wenbo
    Shen, Mingli
    Zhu, Shenglong
    Wang, Fuhui
    CORROSION SCIENCE, 2014, 82 : 316 - 327
  • [6] High-temperature stability of the mechanical and optical properties of Si-B-C-N films prepared by magnetron sputtering
    Kalas, J.
    Vernhes, R.
    Hreben, S.
    Vlcek, J.
    Klemberg-Sapieha, J. E.
    Martinu, L.
    THIN SOLID FILMS, 2009, 518 (01) : 174 - 179
  • [7] Effect of nitrogen content on high-temperature stability of hard and optically transparent amorphous Hf-Y-Si-B-C-N coatings
    Farhadizadeh, A.
    Vlcek, J.
    Houska, J.
    Haviar, S.
    Cerstvy, R.
    Cervena, M.
    Zeman, P.
    Matas, M.
    CERAMICS INTERNATIONAL, 2023, 49 (04) : 6086 - 6093
  • [8] Corrosion, oxidation and high-temperature tribological properties of Ti-B-N coatings
    Asempah, Isaac
    Yu, Lihua
    Ju, Hongbo
    Yu, Dian
    Xu, Junhua
    Miao, Ran
    SURFACE ENGINEERING, 2019, 35 (08) : 661 - 669
  • [9] Research Progress of High Temperature Oxidation Resistance Coatings on γ-TiAl Alloy
    Qu Jing
    Xie Faqin
    Wu Xiangqing
    Gao Guangrui
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (10) : 3929 - 3936
  • [10] High-temperature oxidation protection of γ-based TiAl by sputtered AlOF films
    Brown, Stephen
    Bergeron, Florence
    Loquai, Simon
    Cavarroc, Marjorie
    Knittel, Stephane
    Martinu, Ludvik
    Klemberg-Sapieha, Jolanta E.
    SURFACE & COATINGS TECHNOLOGY, 2022, 439