HOT DEFORMATION BEHAVIOR OF NEAR-α Ti-Fe ALLOY IN (α plus β) TWO-PHASE REGION WITH DIFFERENT Fe CONTENT

被引:0
作者
Poorganji, Behrang [1 ]
Yamaguchi, Makoto [1 ]
Itsumi, Yoshio [1 ]
Matsumoto, Katsushi [1 ]
Tanaka, Tomofumi [1 ]
Asa, Yusuke [1 ]
Miyamoto, Goro [1 ]
Furuhara, Tadashi [1 ]
机构
[1] Inst Mat Res, Aoba Ku, 2-1-1 Katahira, Sendai, Miyagi 9808577, Japan
来源
THERMEC 2009, PTS 1-4 | 2010年 / 638-642卷
关键词
Hot deformation; titanium alloy; ultrafine grained structure; recrystallization; TITANIUM-ALLOYS; WORKING; TI-6AL-4V; MICROSTRUCTURE; EVOLUTION; FLOW; MAPS;
D O I
10.4028/www.scientific.net/MSF.638-642.310
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study, microstructure evolution of Ti-Fe alloys with different Fe content between 0.2-1.5mass% during hot deformation in (alpha+beta) two-phase region is studied with focusing on effect of phase volume fraction at different deformation temperatures and strain rates. Hot deformation was conducted on the specimens quenched after beta solutionizing at 1173K for 1.2ks at 1108, 1073 and 948K, by uniaxial compression by 50% at various strain rates ranged from 1 to 10(-4) s(-1). Initial structures are (alpha+beta) lamellar structures of fine interlamellar spacing and colony sizes. Increase in Fe content results in increasing the fraction of the beta phase at the given deformation temperature Either colony size or interlamellar spacing is coarser at higher temperatures. At the higher deformation temperature where beta phase fraction is larger, dynamic recovery of beta phase is a major deformation mechanism while at a lower temperature, i.e, a higher alpha fraction, dynamic recrystallization of a phase occurs predominantly. It is concluded that critical strain needed for occurrence of dynamic recrystallization is decreased by increasing fraction of the alpha phase at the same deformation temperature, i e., by decreasing Fe content. Furthermore, by increasing strain rate grain size of the recrystallized alpha is decreased
引用
收藏
页码:310 / +
页数:2
相关论文
共 15 条
  • [1] HUMPHREYS FJ, 2004, RECRYSTALLIZATION RE, P356
  • [2] Lutjering G., 2003, ENG MAT PRO, P289
  • [3] Microstructure evolution of near-α titanium alloys during thermomechanical processing
    Ma, FC
    Lu, WJ
    Qin, JN
    Zhang, D
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 416 (1-2): : 59 - 65
  • [4] POORGANJI B, 2008, P 17 C IFHT IN PRESS
  • [5] Formation of ultrafine grained ferrite by warm deformation of lath martensite in low-alloy steels with different carbon content
    Poorganji, Behrang
    Miyamoto, Goro
    Maki, Tadashi
    Furuhara, Tadashi
    [J]. SCRIPTA MATERIALIA, 2008, 59 (03) : 279 - 281
  • [6] Processing maps for hot working of titanium alloys
    Prasad, YVRK
    Seshacharyulu, T
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2): : 82 - 88
  • [7] DEFORMATION MAPS FOR TITANIUM AND ZIRCONIUM
    SARGENT, PM
    ASHBY, MF
    [J]. SCRIPTA METALLURGICA, 1982, 16 (12): : 1415 - 1422
  • [8] Flow behavior and globularization kinetics during hot working of Ti-6Al-4V with a colony alpha microstructure
    Semiatin, SL
    Seetharaman, V
    Weiss, I
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 263 (02): : 257 - 271
  • [9] Hot workability of titanium and titanium aluminide alloys - an overview
    Semiatin, SL
    Seetharaman, V
    Weiss, I
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2): : 1 - 24
  • [10] The effect of alpha platelet thickness on plastic flow during hot working of Ti-6Al-4V with a transformed microstructure
    Semiatin, SL
    Bieler, TR
    [J]. ACTA MATERIALIA, 2001, 49 (17) : 3565 - 3573