Low temperature degradation of a Y-TZP dental ceramic

被引:177
|
作者
Cattani-Lorente, Maria [1 ]
Scherrer, Susanne S. [1 ]
Ammann, Patrick [2 ]
Jobin, Marc [3 ]
Wiskott, H. W. Anselm [1 ]
机构
[1] Univ Geneva, Sch Dent, Lab Biomat, CH-1205 Geneva, Switzerland
[2] Univ Geneva, HUG, Fac Med, Div Bone Dis, CH-1211 Geneva 14, Switzerland
[3] Univ Appl Sci Western Switzerland, EPIA, CH-1202 Geneva, Switzerland
关键词
Zirconia; Low temperature degradation; Tetragonal-to-monoclinic transformation; Dental ceramics; Mechanical properties; ATOMIC-FORCE MICROSCOPY; MONOCLINIC PHASE-TRANSFORMATION; TETRAGONAL ZIRCONIA; STABILIZED ZIRCONIA; MARTENSITIC-TRANSFORMATION; MECHANICAL-PROPERTIES; HYDROTHERMAL DEGRADATION; AGING SENSITIVITY; ZRO2; POLYCRYSTALS; FLEXURAL STRENGTH;
D O I
10.1016/j.actbio.2010.09.020
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Bars of Y-TZP ceramic for dental restorations were subjected to hydrothermal degradation via in vitro exposure to water steam at 140 degrees C for 7 days. X-ray diffraction, atomic force microscopy and scanning electron microscopy techniques were applied to observe and quantify the tetragonal-monoclinic (t-m) phase transformation associated with the process. Nanoindentation was used to assess the ceramic's mechanical properties before and after hydrothermal degradation. Texture associated with martensitic t-m transformation was observed at the grain surface. The t-m transformation followed nucleation-and-growth kinetics, with predominance of the nucleation process. The transformation occurred within a layer of 6 gm below the surface. Mechanical properties deteriorated with hydrothermal degradation, resulting in a 30% reduction of Young's modulus and hardness. A strong correlation was found between the increasing monoclinic fraction and the decline in mechanical response. It was thus concluded that the emergence of the monoclinic phase and the associated microcracking were the most likely causes for the degradation of mechanical properties. (C) 2010 Published by Elsevier Ltd. on behalf of Acta Materialia Inc.
引用
收藏
页码:858 / 865
页数:8
相关论文
共 50 条
  • [31] Study on the surface temperature of Y-TZP ceramic under dry friction
    Liang, XP
    Yang, ZF
    Zhao, SH
    Yuan, QM
    RARE METAL MATERIALS AND ENGINEERING, 2002, 31 : 194 - 197
  • [32] Low-temperature degradation of Y-TZP ceramics: A systematic review and meta-analysis
    Pereira, G. K. R.
    Venturini, A. B.
    Silvestri, T.
    Dapieve, K. S.
    Montagner, A. F.
    Soares, F. Z. M.
    Valandro, L. F.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 55 : 151 - 163
  • [33] Fracture of a Y-TZP ceramic femoral head
    Maccauro, G
    Piconi, C
    Burger, W
    Pilloni, L
    De Santis, E
    Muratori, E
    Learmonth, ID
    JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 2004, 86B (08): : 1192 - 1196
  • [34] Hydrothermal and corrosive degradation of Y-TZP ceramics
    Lawson, S
    Gill, C
    Dransfield, GP
    CORROSION OF ADVANCED CERAMICS, 1996, 113 : 207 - 213
  • [35] Low temperature fully densified nanostructured Y-TZP ceramics
    Duran, P
    Villegas, M
    Capel, F
    Moure, C
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1996, 15 (09) : 741 - 744
  • [36] Fracture toughness and hardness of a Y-TZP dental ceramic after mechanical surface treatments
    Traini, Tonino
    Gherlone, Enrico
    Parabita, Stefano Ferrari
    Caputi, Sergio
    Piattelli, Adriano
    CLINICAL ORAL INVESTIGATIONS, 2014, 18 (03) : 707 - 714
  • [37] Fracture toughness and hardness of a Y-TZP dental ceramic after mechanical surface treatments
    Tonino Traini
    Enrico Gherlone
    Stefano Ferrari Parabita
    Sergio Caputi
    Adriano Piattelli
    Clinical Oral Investigations, 2014, 18 : 707 - 714
  • [38] Mechanical behavior of a Y-TZP ceramic for monolithic restorations: effect of grinding and low-temperature aging
    Pereira, G. K. R.
    Silvestri, T.
    Camargo, R.
    Rippe, M. P.
    Amaral, M.
    Kleverlaan, C. J.
    Valandro, L. F.
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2016, 63 : 70 - 77
  • [39] Effect of sintering holding time on the properties and low-temperature degradation behaviour of manganese oxide-doped Y-TZP ceramic
    Kwa, S. M.
    Ramesh, S.
    Bang, L. T.
    Wong, Y. H.
    Chew, W. J. Kelvin
    Tan, C. Y.
    Purbolaksono, J.
    Misran, H.
    Teng, W. D.
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2015, 16 (02): : 193 - 198
  • [40] Effect of electrical discharge machining on dental Y-TZP ceramic-resin bonding
    Rona, Nergiz
    Yenisey, Murat
    Kucukturk, Gokhan
    Gurun, Hakan
    Cogun, Can
    Esen, Ziya
    JOURNAL OF PROSTHODONTIC RESEARCH, 2017, 61 (02) : 158 - 167