CVD diamond coating on WC cutting tool using electrophoresis

被引:0
作者
Tsubota, T
Nagata, M
Okada, N
Ida, S
Matsumoto, Y
Yatsushiro, N
机构
[1] Kumamoto Ind Res Inst, Mat Dev Dept, Kumamoto 8620901, Japan
[2] Kumamoto Univ, Fac Engn, Dept Appl Chem & Biochem, Kumamoto 8608555, Japan
[3] Kumabou Met Co, Kumamoto 8620937, Japan
关键词
diamond; CVD; WC; electrophoresis; ECR; adhesion; heat treatment; pretreatment;
D O I
10.2109/jcersj.109.1273_782
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
CVD diamond films were deposited on commercial WC cutting tools. An electron cyclotron resonance microwave plasma chemical vapor deposition (ECR-MPCVD) apparatus was used to deposit diamond films. Methane and hydrogen were used as gaseous source for CVD, and WC-Co (JIS standard: K-10) was used as a substrate for CVD. Cobalt on the surface of the WC cutting tool prevented CVD diamond from depositing on the WC cutting tool. Scratching with diamond particles on the surface of the WC cutting tool, which is one of the most popular pretreatments for enhancing the nuclei density of CVD diamond, was ineffective on the WC cutting tool without removing surface cobalt. On the other hand, Electrophoresis treatment was effective for increasing diamond nuclei density on the WC cutting tool without removing surface cobalt. However, CVD diamond films synthesized on the WC cutting tool (from which surface cobalt was removed) using electrophoresis pretreatment separated from the surface of the WC cutting tool. To improve the adhesion between CVD diamond film and WC cutting tool, heat treatment was performed after electrophoresis pretreatment. The heat treatment condition was 500 degreesC for I h in Ar flow. The heat treatment after electrophoresis treatment was effective for improving adhesion between WC surface and CVD diamond film. Vickers hardness test was carried out for estimating the adhesion. The Vickers hardness of the CVD diamond film obtained by the electrophore sis -heat pretreatment, was as hard as that of a CVD diamond film obtained with conventional scratching pretreatment. From the results of Vickers hardness test, it was found that heat treatment after electrophoresis process is effective for improving the strength of the adhesion layer.
引用
收藏
页码:782 / 788
页数:7
相关论文
共 50 条
  • [21] Effect of Nanometer WC Coating on Thermal Conductivity of Diamond/6061 Composites
    Dong, Z. Y.
    Wang, D.
    Wang, W. G.
    Xiao, B. L.
    Ma, Z. Y.
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2023, 36 (01): : 118 - 126
  • [22] Recycling technique for CVD diamond coated cutting tools
    Liu, H
    Hanyu, H
    Murakami, Y
    Kamiya, S
    Saka, M
    SURFACE & COATINGS TECHNOLOGY, 2001, 137 (2-3) : 246 - 248
  • [23] Effect of coating roughness on performance of small CVD diamond coated tools
    Quadrini, F.
    Tagliaferri, V.
    Polini, R.
    MACHINING SCIENCE AND TECHNOLOGY, 2008, 12 (03) : 390 - 404
  • [24] Technology Features of Diamond Coating Deposition on a Carbide Tool
    Ashkinazi, Evgeny
    Fedorov, Sergey
    Khomich, Alexander
    Rogalin, Vladimir
    Bolshakov, Andrey
    Sovyk, Dmitry
    Grigoriev, Sergey
    Konov, Vitaly
    C-JOURNAL OF CARBON RESEARCH, 2022, 8 (04):
  • [25] CVD synthesis of nanometer SiC coating on diamond particles
    Zheng, Xutong
    Liu, Yongsheng
    Cao, Yejie
    Wang, Jing
    Zhang, Yunhai
    CERAMICS INTERNATIONAL, 2021, 47 (11) : 16162 - 16169
  • [26] CVD diamond coating for erosion protection at elevated temperatures
    Vesselin Shanov
    Raj N. Singh
    Widen Tabakoff
    Journal of Materials Engineering and Performance, 2002, 11 : 220 - 225
  • [27] Nanocrystalline CVD diamond coatings for drilling of WC-Co parts
    Almeida, F. A.
    Carrapichano, J. M.
    Fernandes, A. J. S.
    Sacramento, J.
    Silva, R. F.
    Oliveira, F. J.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2011, 29 (05) : 618 - 622
  • [28] Adhesion and wear resistance of CVD diamond coatings on laser treated WC-Co substrates
    Barletta, M.
    Rubino, G.
    Gisario, A.
    WEAR, 2011, 271 (9-10) : 2016 - 2024
  • [29] Diamond films grown on cemented WC-Co dental burs using an improved CVD method
    Ahmed, W
    Sein, H
    Ali, N
    Gracio, J
    Woodwards, R
    DIAMOND AND RELATED MATERIALS, 2003, 12 (08) : 1300 - 1306
  • [30] Finite element analysis of damage properties in scratch test of TiN/WC-Co coating cutting tool
    Xu, Li
    Jiang, Xiaoyu
    TRANSFERABILITY AND APPLICABILITY OF CURRENT MECHANICS APPROACHES, 2009, : 347 - 351