Defect initiation at subsurface grain boundary as a precursor of delamination in ultrahigh molecular weight polyethylene

被引:13
作者
Shibata, N
Tomita, N
Onmori, N
Kato, K
Ikeuchi, K
机构
[1] Kyoto Univ, Int Innovat Ctr, Sakyo Ku, Kyoto 6068501, Japan
[2] Natl Inst Ind Hlth, Tama Ku, Kawasaki, Kanagawa 214, Japan
[3] Doshisha Univ, Fac Engn, Kyoto 602, Japan
[4] Kyoto Univ, Inst Frontier Med Sci, Kyoto 6068501, Japan
来源
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A | 2003年 / 67A卷 / 01期
关键词
ultrahigh molecular weight polyethylene; delamination; subsurface defect; grain boundary; gamma irradiation;
D O I
10.1002/jbm.a.10133
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
In order to examine the initiation mechanism of delamination in ultrahigh molecular weight polyethylene (UHMWPE) knee components, a bi-directional sliding fatigue test was performed for three types of UHMWPE specimens: nonirradiated, gamma-irradiated (25 kGy) and gamma-irradiated (25 kGy) with 0.1% vitamin E added. Sliding surfaces of post-tested UHMWPE specimens were observed using an optical microscope and a scanning electron microscope. Also, surface roughness was measured at the sliding surfaces of UHMWPE specimens. Delamination was observed only in gamma-irradiated specimens. A networked structure of surface asperity that resembled grain boundary was observed prior to delamination in gamma-irradiated specimens. Surface roughness in the gamma-irradiated specimens, higher than in any other specimen, showed a rapid increase prior to delamination. Detailed observation using an optical microscope and a scanning electron microscope showed microscopic crack initiation along subsurface grain boundaries in gamma-irradiated specimens. These results suggest that subsurface crack initiation is a precursor of delamination and is accelerated by oxidative degradation due to gamma irradiation. Of the three types of specimens, UHMWPE with vitamin E added showed the lowest surface roughness values at all measuring points. The addition of vitamin E is effective in improving wear resistance and fatigue performance of UHMWPE. (C) 2003 Wiley Periodicals, Inc.
引用
收藏
页码:276 / 284
页数:9
相关论文
共 34 条
[11]  
Goldman M, 1997, J BIOMED MATER RES, V37, P43, DOI 10.1002/(SICI)1097-4636(199710)37:1<43::AID-JBM6>3.0.CO
[12]  
2-J
[13]  
Goldman M, 1998, J BIOMED MATER RES, V40, P378, DOI 10.1002/(SICI)1097-4636(19980605)40:3<378::AID-JBM6>3.0.CO
[14]  
2-C
[15]  
Heim CS, 1996, AAOS INSTR COURS LEC, V45, P303
[16]  
HIYOSHI N, 2000, J JPN SOC CLIN BIOME, V21, P361
[17]   A RAT MODEL OF RESORPTION OF BONE AT THE CEMENT-BONE INTERFACE IN THE PRESENCE OF POLYETHYLENE WEAR PARTICLES [J].
HOWIE, DW ;
VERNONROBERTS, B ;
OAKESHOTT, R ;
MANTHEY, B .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1988, 70A (02) :257-263
[18]   Contact analysis of ultrahigh molecular weight polyethylene articular plate in artificial knee joint during gait movement [J].
Ishikawa, H ;
Fujiki, H ;
Yasuda, K .
JOURNAL OF BIOMECHANICAL ENGINEERING-TRANSACTIONS OF THE ASME, 1996, 118 (03) :377-386
[19]  
KILGUS DJ, 1991, CLIN ORTHOP RELAT R, P223
[20]   Advances in the processing, sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty [J].
Kurtz, SM ;
Muratoglu, OK ;
Evans, M ;
Edidin, AA .
BIOMATERIALS, 1999, 20 (18) :1659-1688