Low Temperature Bonding by Infiltrating Sn3.5Ag Solder into Porous Ag Sheet for High Temperature Die Attachment in Power Device Packaging

被引:12
作者
Hang, Chunjin [1 ]
He, Junjian [2 ]
Zhang, Zhihao [3 ]
Chen, Hongtao [2 ]
Li, Mingyu [1 ,2 ]
机构
[1] Harbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Heilongjiang, Peoples R China
[2] Harbin Inst Technol Shenzhen, Dept Mat Sci & Engn, Shenzhen 518055, Peoples R China
[3] Xiamen Univ, Dept Mat Sci & Engn, Coll Mat, Fujian Key Lab Adv Mat, Xiamen 361005, Peoples R China
来源
SCIENTIFIC REPORTS | 2018年 / 8卷
关键词
TRANSIENT LIQUID-PHASE; NANO-SILVER JOINTS; MECHANICAL-PROPERTIES; ELECTRONICS; STRENGTH; HARDNESS; SYSTEM; COPPER; PASTE; ZN;
D O I
10.1038/s41598-018-35708-6
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
We have proposed a high temperature die attach method with porous Ag sheet as an interlayer for power device packaging. Sn-3.5Ag solder paste can infiltrate into the porous Ag sheet through capillary forces and Sn can react with the porous Ag sheet and Ag metallizations at the interfaces to form Ag3Sn after reflow at 260 degrees C for 10 min. The large specific surface area and the high diffusion rates between Ag and Sn accelerate the Sn consumption in the porous Ag structure, thus significantly reducing the processing time. The difference of the melting points of the die attach material before and after reflow could be expanded as large as 259 degrees C. The bondlines show good electrical and thermal conductivities. Furthermore, the average shear strength of the bondlines at 300 degrees C is higher than 20 MPa. The porous Ag skeleton remained in the bondline would contribute greatly to the heat dissipation and the electrical signal transmission in power devices.
引用
收藏
页数:7
相关论文
共 41 条
  • [1] Transient liquid phase (TLP) bonding of Al7075 to Ti-6Al-4V alloy
    AlHazaa, A.
    Khan, T. I.
    Haq, I.
    [J]. MATERIALS CHARACTERIZATION, 2010, 61 (03) : 312 - 317
  • [2] Effect of powders on microstructures and mechanical properties for Sn-Ag transient liquid phase bonding in air
    Bao, Yudian
    Wu, Aiping
    Shao, Huakai
    Zhao, Yue
    Zou, Guisheng
    [J]. JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2018, 29 (12) : 10246 - 10257
  • [3] Cu@Sn Core-Shell Structure Powder Preform for High-Temperature Applications Based on Transient Liquid Phase Bonding
    Chen, Hongtao
    Hu, Tianqi
    Li, Mingyu
    Zhao, Zhenqing
    [J]. IEEE TRANSACTIONS ON POWER ELECTRONICS, 2017, 32 (01) : 441 - 451
  • [4] A comparative study of Cn/Sn/Cu and Ni/Sn/Ni solder joints for low temperature stable transient liquid phase bonding
    Chu, Kunmo
    Sohn, Yoonchul
    Moon, Changyoul
    [J]. SCRIPTA MATERIALIA, 2015, 109 : 113 - 117
  • [5] Microstructural studies and bonding strength of pressureless sintered nano-silver joints on silver, direct bond copper (DBC) and copper substrates aged at 300 °C
    Chua, S. T.
    Siow, K. S.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 687 : 486 - 498
  • [6] Overview of transient liquid phase and partial transient liquid phase bonding
    Cook, Grant O., III
    Sorensen, Carl D.
    [J]. JOURNAL OF MATERIALS SCIENCE, 2011, 46 (16) : 5305 - 5323
  • [7] Transient liquid phase bonding
    Gale, WF
    Butts, DA
    [J]. SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2004, 9 (04) : 283 - 300
  • [8] Elastic properties, hardness, and indentation fracture toughness of intermetallics relevant to electronic packaging
    Ghosh, G
    [J]. JOURNAL OF MATERIALS RESEARCH, 2004, 19 (05) : 1439 - 1454
  • [9] Greve H., 2017, P 2017 INT WORKSH IN, P1
  • [10] Microstructural Evolution of Transient Liquid Phase Sinter Joints in High Temperature Environmental Conditions
    Greve, Hannes
    Moeini, S. Ali
    McCluskey, F. Patrick
    Joshi, Shailesh
    [J]. 2016 IEEE 66TH ELECTRONIC COMPONENTS AND TECHNOLOGY CONFERENCE (ECTC), 2016, : 2561 - 2568