Sulfide Capacity of CaO-SiO2-MgO-Al2O3-BaO-Na2O Slag at 1773 K

被引:9
作者
Liu, Wenguo [1 ]
Chen, Yanbiao [1 ]
Wang, Jingsong [1 ]
Zuo, Haibin [1 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
Blast furnace slag; Sulfide capacity; Na2O; BaO; SULFUR PARTITION RATIO; BLAST-FURNACE SLAG; EMISSIONS REDUCTION; VISCOSITY; IRONMAKING; SILICATE; BEHAVIOR; CAO;
D O I
10.1007/s40831-021-00411-w
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Employing low-quality raw materials to lower steel production costs is an effective way for many iron and steel enterprises to achieve the sustainable development in China. Meanwhile, this also raises higher requirement for the desulfurization ability of blast furnace slag with diverse components. In this work, the effect of Na2O on the sulfide capacity of CaO-SiO2-10wt% MgO-12wt% Al2O3-2wt% BaO slag was studied at 1773 K by employing the gas-slag equilibrium technique. The distribution of bridged oxygen (O-0), non-bridged oxygen (O-), and free oxygen (O2-) in slag was analyzed by XPS. The results indicated that the sulfide capacity increased constantly with Na2O content rising from 0 to 5wt% due largely to an increase in the activity of O2-. Na+ would be consumed to compensate preferentially the [AlO4]-tetrahedron structural units to maintain electrical neutrality of molten slag, releasing some Ca2+ ions for sulfur stabilization. Assuming that the activity of O2- and the stability of S2- in molten slag were proportional to the activity of CaO and the activity coefficient of CaS, respectively, the increased range of the activity of CaO was larger than that of the activity coefficient of CaS on the whole, which improved the sulfide capacity of slag. XPS analysis indicated that the relative fraction of free oxygen and non-bridged oxygen increased gradually, and bridged oxygen showed a decreasing trend, which supported the changes of sulfide capacity based on the dominant effect for free oxygen on sulfide capacity.
引用
收藏
页码:1169 / 1177
页数:9
相关论文
共 31 条
[21]   Sulfide Capacity of CaO-SiO2-FeO-Al2O3-MgOsatd. Slag [J].
Park, Youngjoo ;
Min, Dong Joon .
ISIJ INTERNATIONAL, 2016, 56 (04) :520-526
[22]   Hot Metal Desulfurization Kinetics by CaO-Al2O3-SiO2-MgO-TiO2-Na2O Slags [J].
Tong, Zhifang ;
Qiao, Jialong ;
Jiang, Xiyuan .
ISIJ INTERNATIONAL, 2017, 57 (02) :245-253
[23]   Rheological behavior of the CaO-Al2O3-based mold fluxes with different Na2O contents [J].
Wang, Wanlin ;
Shao, Hanqing ;
Zhou, Lejun ;
Luo, Hao ;
Wu, Houfa .
CERAMICS INTERNATIONAL, 2020, 46 (17) :26880-26887
[24]   Cyclic Use of Ladle Furnace Refining Slag for Desulfurization [J].
Wang, Yang ;
Yang, Shufeng ;
Li, Jingshe ;
Wang, Feng ;
Gu, Yu .
JOURNAL OF SUSTAINABLE METALLURGY, 2017, 3 (02) :274-279
[25]   A Review on Reclamation and Reutilization of Ironmaking and Steelmaking Slags [J].
Wang, Zhanjun ;
Sohn, Il .
JOURNAL OF SUSTAINABLE METALLURGY, 2019, 5 (01) :127-140
[26]   Effect of substituting CaO with BaO on the viscosity and structure of CaO-BaO-SiO2-MgO-Al2O3 slags [J].
Wang, Zhanjun ;
Sohn, Il .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2018, 101 (09) :4285-4296
[27]  
Waseda Y., 1998, The structure and properties of oxide melts, P1
[28]   Effect of MgO and K2O on High-Al Silicon-Manganese Alloy Slag Viscosity and Structure [J].
Xing, Xiangdong ;
Pang, Zhuogang ;
Zheng, Jianlu ;
Du, Yueli ;
Ren, Shan ;
Ju, Jiantao .
MINERALS, 2020, 10 (09) :1-12
[29]   Transition of Blast Furnace Slag from Silicate Based to Aluminate Based: Sulfide Capacity [J].
Yan, Zhiming ;
Lv, Xuewei ;
Pang, Zhengde ;
He, Wenchao ;
Liang, Dong ;
Bai, Chenguang .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2017, 48 (05) :2607-2614
[30]   Effects of (CaO + BaO)/Al2O3 Ratio on the Melting, Crystallization, and Melt Structure of CaO-Al2O3-10 wt% SiO2-Based Mold Fluxes for Advanced High-Strength Steels [J].
Zhang, Lei ;
Zhai, Bingyu ;
Wang, Wanlin ;
Sohn, Il .
JOURNAL OF SUSTAINABLE METALLURGY, 2021, 7 (02) :559-568