Effect of thermocycling on the bond strength of composite resin to bur and laser treated composite resin

被引:58
|
作者
Bektas, Ozden Ozel [1 ]
Eren, Digdem [1 ]
Siso, Seyda Herguner [1 ]
Akin, Gulsah E. [1 ]
机构
[1] Cumhuriyet Univ, Dept Restorat Dent, Fac Dent, Sivas, Turkey
关键词
Er:YAG laser; Micro-shear bond strength; Thermocycling; Composite repair; SURFACE TREATMENTS; ADHESIVE SYSTEMS; ERYAG LASER; SHEAR; TENSILE; ENAMEL; AGENTS;
D O I
10.1007/s10103-011-0958-2
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The objective of this study was to investigate the effect of two different surface treatments (Er:YAG laser and bur) and three different numbers of thermal cycling (no aging, 1,000, 5,000, and 10,000 cycles) on the micro-shear bond strength of repaired composite resin. Ninety-six composite blocks (4 mm x 4 mm x 1 mm) obtained with a micromatrix hybrid composite were prepared. The composite blocks were then randomly divided into four groups (n = 24), according to the thermal cycling procedure: (1) stored in distilled water at 37A degrees C for 24 h (control group), (2) 1,000 cycles, (3) 5,000 cycles, and (4) 10,000 cycles. After aging, the blocks were further subdivided into two subgroups (n = 12), according to surface treatment. Bur and laser-treated composite surfaces were treated with an etch&rinse adhesive system. In addition, a microhybrid composite resin was bonded to the surfaces via polyethylene tubing. Specimens were subjected to micro-shear bond strength test by a universal testing machine with a crosshead speed of 0 and 5 mm/min. The data were analyzed using one-way analysis of variance and Tukey tests (alpha = 0.05) for micro-shear bond strengths. After conducting a bond strength test, it was found that the laser and bur-treated specimens had similar results. Aging with 10,000 thermocycles significantly affected the repair bond strength of composite resins.
引用
收藏
页码:723 / 728
页数:6
相关论文
共 50 条
  • [21] Bond Strength of Repaired Composite Resin Restorations
    de Araujo, Rodrigo Maximo
    Zanet, Caio Gorgulho
    Maximo de Araujo, Maria Amelia
    Di Nicolo, Rebeca
    da Rocha, Joao Carlos
    PESQUISA BRASILEIRA EM ODONTOPEDIATRIA E CLINICA INTEGRADA, 2007, 7 (02): : 155 - 160
  • [22] Evaluation of bond strength the composite resin to porcelain
    Carneiro, AM
    Carvalho, RCR
    Turbino, ML
    JOURNAL OF DENTAL RESEARCH, 1999, 78 (05) : 1000 - 1000
  • [23] Influence of Er:YAG laser on bond strength of composite resin.
    Barros, RX
    Tateigi, R
    Yatsuda, RA
    Eduardo, CP
    Matson, E
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B53 - B53
  • [24] TENSILE BOND STRENGTH OF A RESIN CEMENT TO ETCHED ENAMEL AND TO A COMPOSITE RESIN
    WILTSHIRE, WA
    VANWYK, CH
    FERREIRA, MR
    JOURNAL OF DENTAL RESEARCH, 1985, 64 (04) : 781 - 781
  • [25] Bond strength of a resin composite to a polyacid-modified resin composite under different conditions
    Benderli, YG
    Koray, F
    Turan, N
    QUINTESSENCE INTERNATIONAL, 2002, 33 (10): : 770 - 775
  • [26] Effect of the dental bur on the shear strength of the composite resin cemented to enamel bonding.
    Miranda, MS
    Gomes, B
    Silva, TMP
    Sampaio, H
    Dias, K
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : 146 - 146
  • [27] Effect of thermocycling on the bond strength of an aluminous ceramic to a resin cement.
    Andreatta Filho, O. D.
    Araujo, M. A. J.
    Camargo, F. P.
    Galhano, G. A. P.
    Yoshiga, S. R.
    Lopes, A. G.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B337 - B337
  • [28] Effect of surface treatments on the bond strength between composite resin and acrylic resin denture teeth
    Vergani, CE
    Machado, AL
    Giampaolo, ET
    Pavarina, AC
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2000, 13 (05) : 383 - 386
  • [29] The effect of thermocycling and dentine pre-treatment on the durability of the bond between composite resin and dentine
    Huang, MS
    Li, MT
    Huang, FM
    Ding, SJ
    JOURNAL OF ORAL REHABILITATION, 2004, 31 (05) : 492 - 499
  • [30] EFFECT OF ALCOHOL ON THE STRENGTH OF A COMPOSITE RESIN
    SNEED, WD
    DRAUGHN, RA
    OPERATIVE DENTISTRY, 1980, 5 (02) : 47 - 48