Microstructures in the 6060 aluminium alloy after various severe plastic deformation treatments

被引:50
作者
Adamczyk-Cieslak, Boguslawa [1 ]
Mizera, Jaroslaw [1 ]
Kurzydlowski, Krzysztof Jan [1 ]
机构
[1] Warsaw Univ Technol, Fac Mat Sci & Engn, PL-02507 Warsaw, Poland
关键词
Aluminium alloys; Severe plastic deformation; Microstructure; Precipitation hardening; MG-SI ALLOYS; AUTOMOTIVE INDUSTRY; GRAIN-REFINEMENT; PRECIPITATION;
D O I
10.1016/j.matchar.2011.01.009
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper presents the results concerning the microstructural refinement of the industrial 6060 aluminium alloy processed by severe plastic deformation (SPD). The high level of plastic deformation was achieved using the three methods: hydrostatic extrusion (HE), equal channel angular extrusion (ECAE) and extrusion torsion (ET), which differed in the dynamics of the loading, intensity and homogeneity of the plastic strain field. Microstructure analyses were performed before and after SPD deformation using a transmission (TEM) and a scanning electron microscope (SEM). The refined microstructures were examined qualitatively and quantitatively by the stereological methods and computer image analyses. The microstructure of the industrial 6060 aluminium alloy after deformation was characterized by an average grain size of about 0.4 mu m. The results show that the precipitates strongly affect the degree of refinement and the mechanism of microstructural transformations. During the SPD, the second phase particles break apart and homogenize. The HE method generates the largest increase of the volume fraction of the small primary particles. Moreover, the HE process is most effective in reducing the primary particle size. During HE and ECAE processes the second phase precipitates dissolve partially and change their shape. (C) 2011 Elsevier Inc. All rights reserved.
引用
收藏
页码:327 / 332
页数:6
相关论文
共 50 条
[31]   Development of severe plastic deformation by various asymmetric rolling processes [J].
Ji, Y. H. ;
Park, J. J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 499 (1-2) :14-17
[32]   Fine surface microstructure of Fe3Al alloy after severe plastic deformation [J].
Ren, Jiangwei ;
Li, Dong .
MATERIALS LETTERS, 2016, 171 :133-136
[33]   On the microstructure and texture of Cu-Cr-Zr alloy after severe plastic deformation by ECAP [J].
Abib, Khadidja ;
Munoz Balanos, Jairo Alberto ;
Alili, Baya ;
Bradai, Djamel .
MATERIALS CHARACTERIZATION, 2016, 112 :252-258
[34]   Mechanical properties, microstructure and thermal stability of a nanocrystalline CoCrFeMnNi high-entropy alloy after severe plastic deformation [J].
Schuh, B. ;
Mendez-Martin, F. ;
Voelker, B. ;
George, E. P. ;
Clemens, H. ;
Pippan, R. ;
Hohenwarter, A. .
ACTA MATERIALIA, 2015, 96 :258-268
[35]   Modeling the Hot Ductility of AA6061 Aluminum Alloy After Severe Plastic Deformation [J].
Khamei, A. A. ;
Dehghani, K. ;
Mahmudi, R. .
JOM, 2015, 67 (05) :966-972
[36]   Nanocrystallization of steels by various severe plastic deformation [J].
Umemoto, M ;
Todaka, Y ;
Tsuchiya, K .
PROCESSING AND PROPERTIES OF STRUCTURAL NANOMATERIALS, 2003, :125-132
[37]   Evolution in Microstructures and Mechanical Properties of Pure Copper Subjected to Severe Plastic Deformation [J].
Mingya Zhang ;
Li Liu ;
Shan Liang ;
Jinghui Li .
Metals and Materials International, 2020, 26 :1585-1595
[38]   Evolution in Microstructures and Mechanical Properties of Pure Copper Subjected to Severe Plastic Deformation [J].
Zhang, Mingya ;
Liu, Li ;
Liang, Shan ;
Li, Jinghui .
METALS AND MATERIALS INTERNATIONAL, 2020, 26 (10) :1585-1595
[39]   Severe plastic deformation of rheoforged aluminum alloy A356 [J].
Dodangeh, A. ;
Kazeminezhad, M. ;
Aashuri, H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 558 :371-376
[40]   On the natural aging behavior of Aluminum 6061 alloy after severe plastic deformation [J].
Farshidi, M. H. ;
Kazeminezhad, M. ;
Miyamoto, H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 580 :202-208