Microstructure and creep property of as-cast Mg-6Al-XSr(x=0, 2, 3) alloys

被引:1
作者
Wu, Yufeng [1 ]
Du, Wenbo [2 ]
Zhang, Yinan [2 ]
Zuo, Tieyong [1 ]
机构
[1] Beijing Univ Technol, Inst Recycling Econ 1, Beijing, Peoples R China
[2] Beijing Univ Technol, Coll Mat Sci & Engn, Beijing, Peoples R China
来源
MATERIALS AND DESIGN, PTS 1-3 | 2011年 / 284-286卷
关键词
magnesium alloy; Sr; creep; grain boundaries sliding; dislocation motion;
D O I
10.4028/www.scientific.net/AMR.284-286.1564
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microstructure and creep property of as-cast Mg-6Al-xSr(x=0, 2,3) alloys were studied. Results showed that the branch-like Al4Sr phase is the main precipitating phase in these alloys containing Sr. Their secondary creep rates under the applied stress of 70MPa at 175 degrees C decreased with the increasing in the content of Sr and reached the minimum value of 1.4 X 10(-8)s(-1) in the Mg-6Al-3Sr alloy, which is one thirtieth of secondary creep rates of the Mg-6Al alloy. It was mainly attributed to Al4Sr, which effectively hindered the grain boundaries sliding and dislocation motion in the creep.
引用
收藏
页码:1564 / +
页数:2
相关论文
共 6 条
  • [1] Elevated Temperature Mg-Al-Sr: Creep Resistance, Mechanical Properties, and Microstructure
    Eric Baril
    Pierre Labelle
    Mihriban Pekguleryuz
    [J]. JOM, 2003, 55 (11) : 34 - 39
  • [2] Identifiying creep mechanisms at low stresses
    Langdon, TG
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 283 (1-2): : 266 - 273
  • [3] Experimental study of the ternary magnesium-aluminium-strontium system
    Parvez, MA
    Medraj, M
    Essadiqi, E
    Muntasar, A
    Dénès, G
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 402 (1-2) : 170 - 185
  • [4] Creep resistant magnesium diecasting alloys based on alkaline earth elements
    Pekguleryuz, MO
    Baril, E
    [J]. MATERIALS TRANSACTIONS, 2001, 42 (07) : 1258 - 1267
  • [5] Susuki A., 2007, METALL MATER TRANS A, p[38, 420]
  • [6] Zhong Y, 2002, MAGNESIUM TECHNOLOGY 2002, P69