The reduction of nickel from low-grade nickel laterite ore using a solid-state deoxidisation method

被引:123
作者
Li, Bo [1 ]
Wang, Hua [1 ]
Wei, Yonggang [1 ]
机构
[1] Kunming Univ Sci & Technol, Minist Educ, Engn Res Ctr Met Energy Conservat & Emiss Reduct, Kunming 650093, Peoples R China
基金
中国国家自然科学基金;
关键词
Nickel laterite ore; Conversion percentage; Metallic nickel; Solid state deoxidisation;
D O I
10.1016/j.mineng.2011.08.006
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The reduction of nickel from low-grade nickel laterite ore using a solid-state deoxidisation method was studied. The effects of temperature, time, reductant type and CaO content on the conversion percentage of the total nickel to metallic nickel (alpha(Ni)) in the nickel laterite ore reduction process were investigated. The results showed that alpha(Ni) was strongly influenced by the reaction temperature in both gas-solid and solid-solid reduction processes, and a higher temperature was more favourable for nickel reduction. Because the reduction mechanism of nickel laterite ore (NiO + CO -> CO2 + Ni) is indirect, a higher alpha(Ni) (>80%) can be obtained by increasing the CO and anthracite content. In the gas-solid reduction process, a longer reaction time favoured nickel reduction, and the conversion percentage decreased when a gaseous reductant was used at 850 degrees C because of phase transformation. In the solid-solid reduction process, the conversion percentage of the total nickel to metallic nickel first increased and then decreased with increasing reduction time and CaO content. In both reduction processes, taenite was found by XRD in the reduced ore because of iron oxide reduction and metallic nickel formation. SEM revealed that the nickel laterite ore was transformed from large granular and sandwich structures to small granular and flocculent structures during the reduction process. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1556 / 1562
页数:7
相关论文
共 16 条
[1]  
[Anonymous], 2010, T NONFERR METAL SOC
[2]  
[Anonymous], CHEM ENG SCI
[3]  
Antola O., 1995, Mineral Processing and Extractive Metallurgy Review, P169, DOI 10.1080/08827509508914195
[4]   Phase transformation in reductive roasting of laterite ore with microwave heating [J].
Chang Yong-feng ;
Zhai Xiu-jing ;
Fu Yan ;
Ma Lin-zhi ;
Li Bin-chuan ;
Zhang Ting-an .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2008, 18 (04) :969-973
[5]   Leaching behavior of metals from a limonitic nickel laterite using a sulfation-roasting-leaching process [J].
Guo, Xueyi ;
Li, Dong ;
Park, Kyung-Ho ;
Tian, Qinghua ;
Wu, Zhan .
HYDROMETALLURGY, 2009, 99 (3-4) :144-150
[6]  
Hua Y.X., 2004, KINETICS REACTIONS M
[7]   Calcination of low-grade laterite for concentration of Ni by magnetic separation [J].
Kim, Jungah ;
Dodbiba, Gjergj ;
Tanno, Hideaki ;
Okaya, Katsunori ;
Matsuo, Seiji ;
Fujita, Toyohisa .
MINERALS ENGINEERING, 2010, 23 (04) :282-288
[8]  
KRASUK JH, 1972, AICHE J, V18, P506, DOI 10.1002/aic.690180308
[9]   Physicochemical and mechanical properties of nickel laterite ore powder [J].
Li Bo ;
Wang Hua ;
Wei Yong-gang ;
Hu Jian-hang .
ENVIRONMENTAL BIOTECHNOLOGY AND MATERIALS ENGINEERING, PTS 1-3, 2011, 183-185 :1741-1745
[10]  
Li Z.K., 2009, FERRO ALLOYS, V40, P24