Anticorrosion Behaviour of SS304 Microgroove Surfaces in Saline Water

被引:2
|
作者
Annakodi, Vivek Anand [1 ]
Arvind Singh, Ramachandra [2 ]
Jayalakshmi, Subramanian [2 ]
Zhang, Yupeng [2 ]
Srinivas Rao, Koppula [3 ]
Shabadi, Rajashekhara [4 ]
机构
[1] MLR Inst Technol, Dept Aeronaut Engn, Hyderabad 500043, India
[2] Wenzhou Univ, Sch Mech & Elect Engn, Wenzhou 325035, Peoples R China
[3] MLR Inst Technol, Dept Comp Sci & Engn, Hyderabad 500043, India
[4] Univ Lille, CNRS, UMR 8207, Unite Mat & Transformat,Cent Lille, F-59000 Lille, France
关键词
304 stainless steel; microgrooves; wettability; corrosion; saline water; surface roughness; CORROSION-RESISTANCE; FABRICATION;
D O I
10.3390/met11101543
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The 304 Stainless Steel (SS304) is severely affected by salt water corrosion due to its high surface wettability. By reducing its surface wettability, its corrosion can be reduced. To achieve this, topographical modification of the steel surface is an effective route. In this work, SS304 flat surfaces were topographically modified into microgrooves (ridge width 250 mu m to 500 mu m, groove width 200 mu m, width ratio = ridge width/groove width > 1). Wire cut electrical discharge machining was used to fabricate the microgrooves. Long-term wetting characteristics and long-term corrosion behaviour of flat surface and microgrooves were studied. The influence of the nature of wetting of the tested surfaces on their corrosion behaviour was examined. The sessile drop method and potentiodynamic polarization tests in sodium chloride (3.5 wt. % NaCl) solution (intermittent and continuous exposures for 168 h) were studied to characterize their wetting and corrosion behaviours, respectively. Topographical modification imparted long-term hydrophobicity and, as a consequence, long-term anticorrosion ability of the steel surface. Micropatterning reduced the corrosion rate by two orders of magnitude due to reduction in interfacial contact area with the corrosive fluid via composite wetting, i.e., solid-liquid-air interface. Microgrooves showed corrosion inhibition efficiency & GE;88%, upon long-term exposure to NaCl solution. By comparing the wetting and corrosion behaviours of the microgrooves with those of the previously studied microgrooves (ridge width/groove width < 1), it was found that the surface roughness of their ridges strongly influences their wetting and corrosion properties.</p>
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Deformation behaviours of SS304 tubes in pulsating hydroforming processes
    Yang, Lianfa
    Wang, Ninghua
    He, yulin
    STRUCTURAL ENGINEERING AND MECHANICS, 2016, 60 (01) : 91 - 110
  • [32] RESIDUAL-STRESS MEASUREMENT IN SS304 SEAMLESS TUBE
    KOVAC, M
    MIYANO, Y
    WOO, TC
    EXPERIMENTAL MECHANICS, 1989, 29 (02) : 209 - 213
  • [33] Preparation of DB film in the channel of SS304 bipolar plate to improve its water liquidity
    Li, Yuee
    Zhang, Dongming
    ENERGY, 2017, 128 : 19 - 27
  • [34] Measurement of outgassing rate for GTAW welded SS304 materials
    Bukhari, Mohsin
    Mukherjee, Samiran
    Panchal, Paresh
    Gangradey, Ranjana
    Shukla, Ajit Kumar
    INTERNATIONAL CONFERENCE ON ADVANCES IN MATERIALS AND MANUFACTURING APPLICATIONS (ICONAMMA-2016), 2016, 149
  • [35] Microwave hybrid heating based optimized joining of SS304/SS316
    Pal, Mainak
    Kumar, Virinder
    Sehgal, Shankar
    Kumar, Harmesh
    Saxena, Kuldeep K.
    Bagha, Ashok K.
    MATERIALS AND MANUFACTURING PROCESSES, 2021, 36 (13) : 1554 - 1560
  • [36] Microstructure and tribological behaviour of CoCrCuFeTi high entropy alloy reinforced SS304 through friction stir processing
    Radhika, N.
    Krishna, S. Aravind
    Basak, Animesh Kumar
    Adediran, Adeolu Adesoji
    SCIENTIFIC REPORTS, 2024, 14 (01)
  • [37] Microstructure and tribological behaviour of CoCrCuFeTi high entropy alloy reinforced SS304 through friction stir processing
    N. Radhika
    S. Aravind Krishna
    Animesh Kumar Basak
    Adeolu Adesoji Adediran
    Scientific Reports, 14
  • [38] Role of interfacial shear strength in nanotribological behaviour of PTA deposited Colmonoy 6 coating on SS304 steel
    Singh, Virendra Pratap
    Kumar, Deepak
    Mahesh, Vinyas
    Harursampath, Dineshkumar
    Kuriachen, Basil
    MATERIALS LETTERS, 2023, 353
  • [39] Comparative investigation of surface modification and corrosion behaviour on SS304 and SS316 Coated with Inconel 625 in Air and Molten Salt Environment
    Sundaram, Sabanayagam
    Singaravelu, Chockalingam
    Malaiperumal, Vikneswaran
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2022, 10 (04)
  • [40] Multiaxial ratcheting-fatigue interaction of SS304 stainless steel
    Liu, Yujie
    Kang, Guozheng
    Gao, Qing
    ENGINEERING STRUCTURAL INTEGRITY: RESEARCH, DEVELOPMENT AND APPLICATION, VOLS 1 AND 2, 2007, : 829 - 832