Effect of melt thermal history on solidification behavior and microstructural characteristics of a third-generation Ni-based single crystal superalloy

被引:17
作者
Wang, Haifeng [1 ]
Su, Haijun [1 ]
Zhang, Jun [1 ]
Li, Yafeng [1 ]
Liu, Lin [1 ]
Fu, Hengzhi [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金; 国家高技术研究发展计划(863计划);
关键词
Undercooling; Superheating temperature; Superheating time; Cooling rate; Superalloy;
D O I
10.1016/j.jallcom.2016.07.031
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The melt superheating treatment is performed on a third-generation Ni-based single crystal superalloy during directional solidification, aiming to investigate the influence of melt thermal history (melt superheating temperature, superheating time and cooling rate) on solidification behavior and microstructural characteristics. The results show that the nucleation undercooling increases nonlinearly with the increase of melt superheating temperature from 1450 to 1780 degrees C, but decreases when the melt superheating temperature further increases up to 1800 degrees C. The nucleation undercooling first has little change and then increases sharply with increasing the melt superheating time. The critical superheating time is obtained to be about 15 min. Moreover, it is found that the higher the cooling rate is, the larger the nucleation undercooling and liquidus-solidus range are. Additionally, the segregation is reduced, and the dendrite and gamma' phase are obviously refined when the superheating temperature increases from 1500 to 1700 degrees C. The influence mechanism of melt superheating treatment on the nucleation undercooling and solidification microstructure is discussed, which is helpful for optimizing the process parameters and improving the metallurgical quality of Ni-based single crystal superalloy. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:430 / 437
页数:8
相关论文
共 35 条
[21]   The breakdown of single-crystal solidification in high refractory nickel-base alloys [J].
Pollock, TM ;
Murphy, WH .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (04) :1081-1094
[22]   Alloys-By-Design: Application to nickel-based single crystal superalloys [J].
Reed, R. C. ;
Tao, T. ;
Warnken, N. .
ACTA MATERIALIA, 2009, 57 (19) :5898-5913
[23]   Physical properties of some iron based alloys in liquid and amorphous states [J].
Sidorov, VE ;
Calvo-Dahlborg, M ;
Dahlborg, U ;
Popel, PS ;
Chernoborodova, S .
JOURNAL OF MATERIALS SCIENCE, 2000, 35 (09) :2255-2262
[24]  
Stepanova NN, 2003, PHYS MET METALLOGR+, V95, P602
[25]  
Tian S.G., 2010, MAT SCI ENG A-STRUCT, V527, P5445
[26]   Abrupt discontinuous relationships between supercooling and melt overheating [J].
Tong, HY ;
Shi, FG .
APPLIED PHYSICS LETTERS, 1997, 70 (07) :841-843
[27]   Grain structure development in directional solidification of nickel-base superalloys [J].
Wagner, A ;
Shollock, BA ;
McLean, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 374 (1-2) :270-279
[28]  
Wang CS, 2011, RARE METAL MAT ENG, V40, P307
[29]   Microstructure evolution of directionally solidified DZ125 superalloy with melt superheating treatment [J].
Wang, Changshuai ;
Zhang, Jun ;
Liu, Lin ;
Fu, Hengzhi .
JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 508 (02) :440-445
[30]   Structure relaxation and crystallization of Al83Ni10Ce7 metallic glass [J].
Wang, S. H. ;
Bian, X. F. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 450 (1-2) :260-263