Effect of water conditioning on the fracture behavior of PA12 composites processed by selective laser sintering

被引:35
作者
Seltzer, Rocio [1 ]
Martin de la Escalera, Federico [2 ]
Segurado, Javier [1 ]
机构
[1] IMDEA Mat Inst, Madrid Inst Adv Studies Mat, Madrid 28040, Spain
[2] Aernnova Engn Solut Iber, Madrid 28050, Spain
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2011年 / 528卷 / 22-23期
关键词
Mechanical characterization; Polymer; Composites; Sintering; Fracture; Water moisture; MECHANICAL-PROPERTIES; GLASS-FIBER; POLYAMIDE; TOUGHNESS;
D O I
10.1016/j.msea.2011.05.045
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study aims to elucidate the combined effects of reinforcing particles and water on PA12 processed by selective laser sintering (SLS). PA12 is one of the toughest polyamides. However, PA12 processed by SLS is rather brittle due to the presence of voids and the relative low molecular weight of the polymers used in SLS. It is demonstrated that humidity impoverishes the mechanical properties of neat PA12, including ductility and toughness. A ductile/brittle transition was detected, which was attributed to the competition between the plasticizing effect and the hydrolization of PA12 molecules plus the increase in crystallinity which counteracted this mechanism. It has been found that addition of hard particles, such as glass spheres and ceramic fibers, prevents the ductile/brittle transition by water conditioning at high temperature to happen. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:6927 / 6933
页数:7
相关论文
共 26 条
[1]   Experimental measurement and finite element modelling of the compressive properties of laser sintered Nylon-12 [J].
Ajoku, Uzorna ;
Hopkinson, Neil ;
Caine, Mike .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 428 (1-2) :211-216
[2]  
ASM International, 2003, CHAR FAIL AN PLAST
[3]  
ASTM, 2003, D63803 ASTM INT
[4]  
*ASTM INT, 2007, D504599 ASTM INT
[5]   EFFECT OF POLYMERIZATION CONDITIONS AND CRYSTALLINITY ON MECHANICAL-PROPERTIES AND FRACTURE OF SPHERULITIC NYLON-6 [J].
BESSELL, TJ ;
HULL, D ;
SHORTALL, JB .
JOURNAL OF MATERIALS SCIENCE, 1975, 10 (07) :1127-1136
[6]  
ELLIS TS, 1984, POLYM PREPR-ACS, V25, P197
[7]   Crystallization behavior of nylon 6 nanocomposites [J].
Fornes, TD ;
Paul, DR .
POLYMER, 2003, 44 (14) :3945-3961
[8]   EFFECT OF ANNEALING ON THERMAL-PROPERTIES AND CRYSTALLINE-STRUCTURE OF POLYAMIDES - NYLON-12 (POLYLAUROLACTAM) [J].
GOGOLEWSKI, S ;
CZERNIAWSKA, K ;
GASIOREK, M .
COLLOID AND POLYMER SCIENCE, 1980, 258 (10) :1130-1136
[9]   HYGROTHERMAL AGING STUDIES OF SHORT CARBON-FIBER-REINFORCED NYLON-6.6 [J].
ISHAK, ZAM ;
BERRY, JP .
JOURNAL OF APPLIED POLYMER SCIENCE, 1994, 51 (13) :2145-2155
[10]   Effects of ethanol content and temperature on the permeation of fuel through polyamide-12-based pipes [J].
Kallio, K. J. ;
Hedenqvist, M. S. .
POLYMER TESTING, 2010, 29 (05) :603-608