Investigation on the thermo-chemical reaction mechanism between yttria-stabilized zirconia (YSZ) and calcium-magnesium-alumino-silicate (CMAS)

被引:5
作者
Zhang, Dong-Bo [1 ]
Wang, Bin-Yi [1 ]
Cao, Jian [1 ]
Song, Guan-Yu [1 ]
Liu, Juan-Bo [1 ]
机构
[1] North China Elect Power Univ, Key Lab Condit Monitoring & Control Power Plant E, Minist Educ, Beijing 102206, Peoples R China
关键词
thermal barrier coating (TBC); yttria-stabilized zirconia (YSZ); calcium-magnesium-alumino-silicate (CMAS); thermo-chemical reaction; high temperature; THERMAL BARRIER COATINGS; HIGH-TEMPERATURE ATTACK; GLASSY DEPOSITS; DELAMINATION; DEGRADATION; DAMAGE; RESISTANT; SUBJECT; SYSTEMS;
D O I
10.1007/s11706-015-0275-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Thermal barrier coatings (TBCs) with Y2O3-stabilized ZrO2 (YSZ) top coat play a very important role in advanced turbine blades by considerably increasing the engine efficiency and improving the performance of highly loaded blades. However, at high temperatures, environment factors result in the failure of TBCs. The influence of calcium-magnesium-alumino-silicate (CMAS) is one of environment factors. Although thermo-physical effect is being paid attention to, the thermo-chemical reaction becomes the hot-spot in the research area of TBCs affected by CMAS. In this paper, traditional twolayered structured TBCs were prepared by electron beam physical vapor deposition (EBPVD) as the object of study. TBCs coated with CMAS were heated at 1240A degrees C for 3 h. Additionally, 15 wt.% simulated molten CMAS powder and YSZ powder were mixed and heated at 1240A degrees C or 1350A degrees C for 48 h. SEM and EDS were adopted to detect morphology and elements distribution. According to XRD and TEM results, it was revealed that CMAS react with YSZ at high temperature and form ZrSiO4, Ca0.2Zr0.8O1.8 and Ca0.15Zr0.85O1.85 after reaction, as a result, leading to the failure of TBCs and decreasing the TBC lifetime.
引用
收藏
页码:93 / 100
页数:8
相关论文
共 23 条
[1]   Novel thermal barrier coatings that are resistant to high-temperature attack by glassy deposits [J].
Aygun, Aysegul ;
Vasiliev, Alexander L. ;
Padture, Nitin P. ;
Ma, Xinqing .
ACTA MATERIALIA, 2007, 55 (20) :6734-6745
[2]   Role of environmental deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings [J].
Borom, MP ;
Johnson, CA ;
Peluso, LA .
SURFACE & COATINGS TECHNOLOGY, 1996, 86 (1-3) :116-126
[3]   Ceramic materials for thermal barrier coatings [J].
Cao, XQ ;
Vassen, R ;
Stoever, D .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (01) :1-10
[4]   Calcium-magnesium-alumina-silicate (CMAS) delamination mechanisms in EB-PVD thermal barrier coatings [J].
Chen, X .
SURFACE & COATINGS TECHNOLOGY, 2006, 200 (11) :3418-3427
[5]   Composition effects of thermal barrier coating ceramics on their interaction with molten Ca-Mg-Al-silicate (CMAS) glass [J].
Drexler, Julie M. ;
Ortiz, Angel L. ;
Padture, Nitin P. .
ACTA MATERIALIA, 2012, 60 (15) :5437-5447
[6]   Air-plasma-sprayed thermal barrier coatings that are resistant to high-temperature attack by glassy deposits [J].
Drexler, Julie M. ;
Shinoda, Kentaro ;
Ortiz, Angel L. ;
Li, Dongsheng ;
Vasiliev, Alexander L. ;
Gledhill, Andrew D. ;
Sampath, Sanjay ;
Padture, Nitin P. .
ACTA MATERIALIA, 2010, 58 (20) :6835-6844
[7]   Mitigation of damage from molten fly ash to air-plasma-sprayed thermal barrier coatings [J].
Gledhill, Andrew D. ;
Reddy, Kongara M. ;
Drexler, Julie M. ;
Shinoda, Kentaro ;
Sampath, Sanjay ;
Padture, Nitin P. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (24) :7214-7221
[8]   CMAS degradation of environmental barrier coatings [J].
Grant, Kendra M. ;
Kramer, Stephan ;
Lofvander, Jan P. A. ;
Levi, Carlos G. .
SURFACE & COATINGS TECHNOLOGY, 2007, 202 (4-7) :653-657
[9]   Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration [J].
Kraemer, S. ;
Faulhaber, S. ;
Chambers, M. ;
Clarke, D. R. ;
Levi, C. G. ;
Hutchinson, J. W. ;
Evans, A. G. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 490 (1-2) :26-35
[10]   A delamination mechanism for thermal barrier coatings subject to calcium-magnesium-alumino-silicate (CMAS) infiltration [J].
Mercer, C ;
Faulhaber, S ;
Evans, AG ;
Darolia, R .
ACTA MATERIALIA, 2005, 53 (04) :1029-1039