Influence of a Prior Oxidation on the Reduction Behavior of Magnetite Iron Ore Ultra-Fines Using Hydrogen

被引:11
作者
Wolfinger, Thomas [1 ,2 ]
Spreitzer, Daniel [3 ]
Zheng, Heng [2 ]
Schenk, Johannes [1 ,2 ]
机构
[1] K1MET GmbH, Stahlstr 14, A-4020 Linz, Austria
[2] Univ Leoben, Chair Ferrous Met, FranzJosefStr 18, A-8700 Leoben, Austria
[3] Primet Technol Austria GmbH, Turinstr 44, A-4020 Linz, Austria
来源
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE | 2022年 / 53卷 / 01期
关键词
FLUIDIZED-BED REDUCTION; GASEOUS REDUCTION; SIZE DISTRIBUTION; GAS-COMPOSITION; HEMATITE FE2O3; PHASE-CHANGE; KINETICS; WUSTITE; STICKING; CONCENTRATE;
D O I
10.1007/s11663-021-02378-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The reduction behavior of raw and prior-oxidized magnetite iron ore ultra-fines with hydrogen was investigated. Reduction tests were conducted with a thermogravimetric analyzer in a temperature range from 873 K to 1098 K at 1.1 bar absolute, using hydrogen as reducing gas. The experimental results show that a prior oxidation of the magnetite has a positive effect on the reduction behavior because of changing morphology. The apparent activation energies show a turnaround to negative values, depending on the prior oxidation and degree of reduction. A multi-step kinetic analysis based on the model developed by Johnson-Mehl-Avrami was used to reveal the limiting mechanism during reduction. At 873 K and 948 K, the reduction at the initial stage is controlled by nucleation and chemical reaction and in the final stage by nucleation only, for both raw and pre-oxidized magnetites. At higher temperatures, 1023 K and 1098 K, the reduction of raw magnetite is mainly controlled by diffusion. This changes for pre-oxidized magnetite to a mixed controlled mechanism at the initial stage. Processing magnetite iron ore ultra-fines with a hydrogen-based direct reduction technology, lower reduction temperatures and a prior oxidation are recommended, whereby a high degree of oxidation is not necessary.
引用
收藏
页码:14 / 28
页数:15
相关论文
共 69 条
[31]   The applicability of Johnson-Mehl-Avrami model in the thermal analysis of the crystallization kinetics of glasses [J].
Malek, J .
THERMOCHIMICA ACTA, 1995, 267 :61-73
[32]   MECHANISMS OF POROUS IRON GROWTH ON WUSTITE AND MAGNETITE DURING GASEOUS REDUCTION [J].
MATTHEW, SP ;
CHO, TR ;
HAYES, PC .
METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1990, 21 (04) :733-741
[33]   MICROSTRUCTURAL CHANGES OCCURRING DURING THE GASEOUS REDUCTION OF MAGNETITE [J].
MATTHEW, SP ;
HAYES, PC .
METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1990, 21 (01) :153-172
[34]   Reduction of hematite (Fe2O3) to wustite (FeO) by carbon monoxide (CO) for chemical looping combustion [J].
Monazam, Esmail R. ;
Breault, Ronald W. ;
Siriwardane, Ranjani .
CHEMICAL ENGINEERING JOURNAL, 2014, 242 :204-210
[35]   Kinetics of the reduction of hematite (Fe2O3) by methane (CH4) during chemical looping combustion: A global mechanism [J].
Monazam, Esmail R. ;
Breault, Ronald W. ;
Siriwardane, Ranjani ;
Richards, George ;
Carpenter, Stephen .
CHEMICAL ENGINEERING JOURNAL, 2013, 232 :478-487
[36]   Thermogravimetric Analysis of Modified Hematite by Methane (CH4) for Chemical-Looping Combustion: A Global Kinetics Mechanism [J].
Monazam, Esmail R. ;
Breault, Ronald W. ;
Siriwardane, Ranjani ;
Miller, Duane D. .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2013, 52 (42) :14808-14816
[37]   MECHANISM OF WHISKER GROWTH IN THE REDUCTION OF WUSTITE [J].
NICOLLE, R ;
RIST, A .
METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1979, 10 (03) :429-438
[38]  
Nuber D, 2006, STAHL EISEN, V126, P47
[39]   Prediction of the granule size distribution of iron ore sinter feeds that contain concentrate and micropellets [J].
Nyembwe, A. M. ;
Cromarty, R. D. ;
Garbers-Craig, A. M. .
POWDER TECHNOLOGY, 2016, 295 :7-15
[40]   ESTIMATION OF ACTIVATION-ENERGY BY ISOCONVERSION METHODS [J].
OZAWA, T .
THERMOCHIMICA ACTA, 1992, 203 :159-165