Formation of Surface Impurities on Lithium-Nickel-Manganese-Cobalt Oxides in the Presence of CO2 and H2O

被引:30
作者
Fang, Zongtang [2 ]
Confer, Matthew P. [1 ]
Wang, Yixiao [2 ]
Wang, Qiang [3 ]
Kunz, M. Ross [2 ]
Dufek, Eric J. [3 ]
Liaw, Boryann [3 ]
Klein, Tonya M. [4 ]
Dixon, David A. [1 ]
Fushimi, Rebecca [2 ]
机构
[1] Univ Alabama, Dept Chem & Biochem, Tuscaloosa, AL 35487 USA
[2] Idaho Natl Lab, Biol & Chem Sci & Engn Dept, Idaho Falls, ID 83415 USA
[3] Idaho Natl Lab, Energy Storage & Adv Transportat Dept, Idaho Falls, ID 83415 USA
[4] Univ Alabama, Dept Chem & Biol Engn, Tuscaloosa, AL 35487 USA
关键词
INITIO MOLECULAR-DYNAMICS; TRANSITION-METAL OXIDE; CATHODE MATERIALS; 1ST CYCLE; CARBONATE; ADSORPTION; ELECTROLYTE; PERFORMANCE; STABILITY; EVOLUTION;
D O I
10.1021/jacs.1c03812
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Surface impurities involving parasitic reactions and gas evolution contribute to the degradation of high Ni content LiNixMnyCozO2 (NMC) cathode materials. The transient kinetic technique of temporal analysis of products (TAP), density functional theory, and infrared spectroscopy have been used to study the formation of surface impurities on varying nickel content NMC materials (NMC811, NMC622, NMC532, NMC433, NMC111) in the presence of CO2 and H2O. CO2 reactivity on a clean surface as characterized by CO2 conversion rate in the TAP reactor follows the order: NMC811 > NMC622 > NMC532 > NMC433 > NMC111. The capacity of CO2 uptake follows a different order: NMC532 > NMC433 > NMC622 > NMC811 > NMC111. Moisture pretreatment slows down the direct CO2 adsorption process and creates additional active sites for CO2 adsorption. Electronic structure calculations predict that the (012) surface is more reactive than the (1014) surface for CO2 and H2O adsorption. CO2 adsorption leading to carbonate formation is exothermic with formation of ion pairs. The average CO2 binding energies on the different materials follow the CO2 reactivity order. Water hydroxylates the (012) surface and surface OH groups favor bicarbonate formation. Water creates more active sites for CO2 adsorption on the (1014) surface due to hydrogen bonding. The composition of surface impurities formed in ambient air exposure is dependent on water concentration and the percentage of different crystal planes. Different surface reactivities suggest that battery performance degradation due to surface impurities can be mitigated by precise control of the dominant surfaces in NMC materials.
引用
收藏
页码:10261 / 10274
页数:14
相关论文
共 54 条
  • [51] Chemical stability and long-term cell performance of low-cobalt, Ni-Rich cathodes prepared by aqueous processing for high-energy Li-Ion batteries
    Wood, Marissa
    Li, Jianlin
    Ruther, Rose E.
    Du, Zhijia
    Self, Ethan C.
    Meyer, Harry M., III
    Daniel, Claus
    Belharouak, Ilias
    Wood, David L., III
    [J]. ENERGY STORAGE MATERIALS, 2020, 24 : 188 - 197
  • [52] Some Effects of Intentionally AddedWater on LiCoO2/Graphite Pouch Cells
    Xiong, D. J.
    Petibon, R.
    Madec, L.
    Hall, D. S.
    Dahn, J. R.
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2016, 163 (08) : A1678 - A1685
  • [53] First-principles prediction of redox potentials in transition-metal compounds with LDA + U -: art. no. 235121
    Zhou, F
    Cococcioni, M
    Marianetti, CA
    Morgan, D
    Ceder, G
    [J]. PHYSICAL REVIEW B, 2004, 70 (23) : 1 - 8
  • [54] Single-crystal based studies for correlating the properties and high-voltage performance of Li[NixMnyCo1-x-y]O2 cathodes
    Zhu, Jian
    Chen, Guoying
    [J]. JOURNAL OF MATERIALS CHEMISTRY A, 2019, 7 (10) : 5463 - 5474