High-temperature mechanical properties and thermal recovery of balsa wood

被引:50
作者
Goodrich, Thomas [2 ]
Nawaz, Nadia [1 ]
Feih, Stefanie [1 ]
Lattimer, Brian Y. [2 ]
Mouritz, Adrian P. [1 ]
机构
[1] RMIT Univ, Sch Aerosp Mech & Mfg Engn, Melbourne, Vic 3001, Australia
[2] Virginia Polytech Inst & State Univ, Dept Mech Engn, Blacksburg, VA 24061 USA
关键词
Balsa; Thermal; Mechanical properties; Decomposition; MATRIX COMPOSITE PANELS; SANDWICH PANELS; STRUCTURAL INTEGRITY; GLASS-TRANSITION; FIRE; BEHAVIOR; LIGNIN; HEAT; GRADIENTS; CELLULOSE;
D O I
10.1007/s10086-010-1125-2
中图分类号
S7 [林业];
学科分类号
0829 ; 0907 ;
摘要
This article presents an experimental study into thermal softening and thermal recovery of the compression strength properties of structural balsa wood (Ochroma pyramidale). Balsa is a core material used in sandwich composite structures for applications where fire is an ever-present risk, such as ships and buildings. This article investigates the thermal softening response of balsa with increasing temperature, and the thermal recovery behavior when softened balsa is cooled following heating. Exposure to elevated temperatures was limited to a short time (15 min), representative of a fire or postfire scenario. The compression strength of balsa decreased progressively with increasing temperature from 20A degrees to 250A degrees C. The degradation rates in the strength properties over this temperature range were similar in the axial and radial directions of the balsa grains. Thermogravimetric analysis revealed only small mass losses (< 2%) in this temperature range. Environmental scanning electron microscopy showed minor physical changes to the wood grain structure from 190A degrees to 250A degrees C, with holes beginning to form in the cell wall at 250A degrees C. The reduction in compression properties is attributed mostly to thermal viscous softening of the hemicellulose and lignin in the cell walls. Post-heating tests revealed that thermal softening up to 250A degrees C is fully reversible when balsa is cooled to room temperature. When balsa is heated to 250A degrees C or higher, the post-heating strength properties are reduced significantly by decomposition processes of all wood constituents, which irreversibly degrade the wood microstructure. This study revealed that the balsa core in sandwich composite structures must remain below 200A degrees-250A degrees C when exposed to fire to avoid permanent heat damage.
引用
收藏
页码:437 / 443
页数:7
相关论文
共 24 条
[1]   Response of a sandwich panel subject to fire or elevated temperature on one of the surfaces [J].
Birman, V ;
Kardomateas, GA ;
Simitses, GJ ;
Li, R .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2006, 37 (07) :981-988
[2]   Thermally induced bending and wrinkling in large aspect ratio sandwich panels [J].
Birman, V .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2005, 36 (10) :1412-1420
[3]  
Boonstra MJ, 2007, ANN FOREST SCI, V64, P679, DOI 10.1051/forest:2007048
[4]   ON THE MECHANICS OF BALSA AND OTHER WOODS [J].
EASTERLING, KE ;
HARRYSSON, R ;
GIBSON, LJ ;
ASHBY, MF .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 1982, 383 (1784) :31-&
[5]  
Esteves BM, 2009, BIORESOURCES, V4, P370
[6]   Modeling compressive skin failure of sandwich composites in fire [J].
Feih, S. ;
Mathys, Z. ;
Gibson, A. G. ;
Mouritz, A. P. .
JOURNAL OF SANDWICH STRUCTURES & MATERIALS, 2008, 10 (03) :217-245
[7]  
Furuta Y, 1999, MOKUZAI GAKKAISHI, V45, P193
[8]   Designing polymer matrix composite panels for structural integrity in fire [J].
Gu, Pei ;
Asaro, R. J. .
COMPOSITE STRUCTURES, 2008, 84 (04) :300-309
[9]   Wrinkling of sandwich polymer matrix composite panels under transverse thermal gradients [J].
Gu, Pei ;
Asaro, R. J. .
FIRE SAFETY JOURNAL, 2008, 43 (02) :151-160
[10]   Distortion of polymer matrix composite panels under transverse thermal gradients [J].
Gu, Pei ;
Asaro, R. J. .
COMPOSITE STRUCTURES, 2008, 82 (03) :413-421