Analysis of {411} ⟨ 148 ⟩ recrystallisation texture in twin-roll strip casting of 4.5 wt% Si non-oriented electrical steel

被引:15
作者
Zu, Guoqing [1 ,2 ]
Zhang, Xiaoming [1 ]
Zhao, Jingwei [2 ]
Wang, Yuqian [1 ]
Cui, Yi [1 ]
Yan, Yi [2 ]
Jiang, Zhengyi [2 ]
机构
[1] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
[2] Univ Wollongong, Sch Mech Mat & Mechatron Engn, Wollongong, NSW 2522, Australia
关键词
Recrystallisation; Texture; Orientation pinning; Selective growth; Non-oriented electrical steel; Twin-roll strip casting; ORIENTATION; MICROSTRUCTURE; EVOLUTION; GROWTH;
D O I
10.1016/j.matlet.2016.04.091
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The evolution of {411} < 148 > texture in a promising twin-roll strip casting of 4.5 wt% Si electrical steel was skillfully investigated. The results show that the selective growth mechanism, caused by orientation pinning, is responsible for the formation of the sharp {411} < 148 > component which is beyond the preferred nucleus spectrum. (C) 2016 Published by Elsevier B.V.
引用
收藏
页码:63 / 67
页数:5
相关论文
共 17 条
[1]   On the influence of orientation pinning on growth selection of recrystallisation [J].
Engler, O .
ACTA MATERIALIA, 1998, 46 (05) :1555-1568
[2]   Progress in Strip Casting Technologies for Steel; Technical Developments [J].
Ge, Sa ;
Isac, Mihaiela ;
Guthrie, Roderick Ian Lawrence .
ISIJ INTERNATIONAL, 2013, 53 (05) :729-742
[3]   Recrystallized {311} ⟨136⟩ orientation in ferrite steels [J].
Gobernado, P. ;
Petrov, R. H. ;
Kestens, L. A. I. .
SCRIPTA MATERIALIA, 2012, 66 (09) :623-626
[4]   On {h,1,1}&lt;1/h,1,2&gt;, the recrystallisation texture of heavily cold rolled BCC steel [J].
Homma, H ;
Nakamura, S ;
Yoshinaga, N .
RECRYSTALLIZATION AND GRAIN GROWTH, PTS 1 AND 2, 2004, 467-470 :269-274
[5]   Orientation dependence of secondary recrystallisation in silicon-iron [J].
Homma, H ;
Hutchinson, B .
ACTA MATERIALIA, 2003, 51 (13) :3795-3805
[6]   The evolution of the Goss and Cube textures in electrical steel [J].
Kim, Jae Kyoum ;
Lee, Dong Nyung ;
Koo, Yang Mo .
MATERIALS LETTERS, 2014, 122 :110-113
[7]   Effect of cerium on the as-cast microstructure and tensile ductility of the twin-roll casting Fe-6.5 wt% Si alloy [J].
Li, Hao-Ze ;
Liu, Hai-Tao ;
Wang, Xiang-Long ;
Cao, Guang-Ming ;
Li, Cheng-Gang ;
Liu, Zhen-Yu ;
Wang, Guo-Dong .
MATERIALS LETTERS, 2016, 165 :5-8
[8]  
Liu H. B., 2012, MAT LETT
[9]   Development of {210} ⟨0 0 1⟩ recrystallization texture in Fe-6.5 wt.% Si thin sheets [J].
Liu, J. L. ;
Sha, Y. H. ;
Zhang, F. ;
Li, J. C. ;
Yao, Y. C. ;
Zuo, L. .
SCRIPTA MATERIALIA, 2011, 65 (04) :292-295
[10]   Evolution of recrystallization texture in nonoriented electrical steels [J].
Park, JT ;
Szpunar, JA .
ACTA MATERIALIA, 2003, 51 (11) :3037-3051