Using nanoindentation to investigate the temperature cycling of Sn-37Pb solders

被引:3
作者
Wen, Hua-Chiang [1 ]
Chou, Wu-Ching [1 ]
Lin, Po-Chen [2 ]
Jeng, Yeau-Ren [3 ]
Chen, Chien-Chang [4 ]
Chen, Hung-Ming [5 ]
Jiang, Don Son [6 ]
Cheng, Chun-Hu [7 ]
机构
[1] Natl Chiao Tung Univ, Dept Electrophys, Hsinchu 300, Taiwan
[2] Natl Chiao Tung Univ, Dept Mech Engn, Hsinchu 300, Taiwan
[3] Natl Chung Cheng Univ, Dept Mech Engn, Chiayi 621, Taiwan
[4] Natl Chiao Tung Univ, Res Grp Biomed Image Proc, Shing Tung Yau Ctr, Hsinchu 300, Taiwan
[5] Natl Chiao Tung Univ, Dept Elect Engn, Hsinchu 300, Taiwan
[6] Siliconware Precis Ind Co Ltd, Mat & Design Engn Div, Engn Ctr, Taichung 400, Taiwan
[7] Natl Taiwan Normal Univ, Dept Mechatron Engn, Taipei 106, Taiwan
关键词
Intermetallic compounds; Diffusion; Recrystallization; Electron microscopy; LOW-COST; RECRYSTALLIZATION; JOINTS; MICROSTRUCTURE; ALLOYS; INTERCONNECTIONS; MORPHOLOGY; EVOLUTION; STRESS;
D O I
10.1016/j.microrel.2017.05.004
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Using nanoindentation and energy dispersive X-ray spectrometry (EDS), we have conducted an investigation into corner failures to elucidate not only the nanomechanical properties of Sn-37Pb solder balls but also the effects of temperature cycling tests (TCTs). We found that the hardness of Sn-37Pb solder balls was greater in central locations [1.18 +/- 0.05 GPa for room-temperature (RT) sample; 1.3 +/- 0.05 GPa for TCT sample], but had standard values in corner locations (>0.2 +/- 0.02 GPa). The modulus increased after the TCTs. Nevertheless, the mechanical properties were closely related to the average area of the alpha-Pb phase. The average area of the Pb-rich region was more stable after the TCTs than that of the RT sample, due to the enhanced mechanical properties of the Sn-37Pb solder, suggesting good reliability. From an analysis of average areas in the RT sample, it appears that the Pb-rich solid solution that formed led to weak Sn-Pb bonds near the corner locations. Electron back scattered diffraction measurements revealed that grains with grain boundaries formed as a result of accelerated TCT cycling. We conclude that Sn-Pb recrystallization was initiated and propagated after the TCTs, followed by propagation to the interfacial region. (C) 2017 Published by Elsevier Ltd.
引用
收藏
页码:111 / 117
页数:7
相关论文
共 46 条
  • [1] Damping characteristics of Sn-3Ag-0.5Cu and Sn-37Pb solders studied by dynamic mechanical analysis
    Chang, S. H.
    Wu, S. K.
    SCRIPTA MATERIALIA, 2010, 63 (10) : 957 - 960
  • [2] Damage produced in model solder (Sn-37Pb) joints during thermomechanical cycling
    X. W. Liu
    W. J. Plumbridge
    Journal of Electronic Materials, 2003, 32 : 278 - 286
  • [3] Damage produced in model solder (Sn-37Pb) joints during thermomechanical cycling
    Liu, XW
    Plumbridge, WJ
    JOURNAL OF ELECTRONIC MATERIALS, 2003, 32 (04) : 278 - 286
  • [4] Effect of relative humidity on corrosion behavior of SAC305 and Sn-37Pb solders under polyvinyl chloride fire smoke atmosphere
    Li, Qian
    Lin, Jin
    Li, Changhai
    Lu, Shouxiang
    Chen, Xiao
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2020, 31 (22) : 19920 - 19930
  • [5] Influence of thermal shock cycles on Sn-37Pb solder bumps
    Gan, Guisheng
    Xia, Da-quan
    Liu, Xin
    Liu, Cong
    Cheng, Hanlin
    Ming, Zhongzhen
    Gao, Haoyang
    Yang, Dong-hua
    Wu, Yi-ping
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2019, 31 (02) : 85 - 92
  • [6] Deformation behavior and constitutive equation of Sn-37Pb solder alloy at cryogenic temperature
    Zhou, Ning
    Li, Shengli
    Wu, Lin
    Hang, Chunjin
    Zhang, Wei
    Tian, Yanhong
    Ding, Ying
    MATERIALS TODAY COMMUNICATIONS, 2024, 41
  • [7] Effect of cooling rate on microstructure and shear strength of pure Sn, Sn-0.7Cu, Sn-3.5Ag, and Sn-37Pb solders
    Maveety, JG
    Liu, P
    Vijayen, J
    Hua, F
    Sanchez, EA
    JOURNAL OF ELECTRONIC MATERIALS, 2004, 33 (11) : 1355 - 1362
  • [8] Effect of cooling rate on microstructure and shear strength of pure Sn, Sn-0.7Cu, Sn-3.5Ag, and Sn-37Pb solders
    J. G. Maveety
    P. Liu
    J. Vijayen
    F. Hua
    E. A. Sanchez
    Journal of Electronic Materials, 2004, 33 : 1355 - 1362
  • [9] Solid state interfacial reaction of Sn-37Pb and Sn-3.5Ag solders with Ni-P under bump metallization
    He, M
    Chen, Z
    Qi, GJ
    ACTA MATERIALIA, 2004, 52 (07) : 2047 - 2056
  • [10] Dependence of Electrical Resistivity on Temperature and Sn Content in Pb-Sn Solders
    Cadirli, E.
    Boyuk, U.
    Kaya, H.
    Marasli, N.
    Aksoz, S.
    Ocak, Y.
    JOURNAL OF ELECTRONIC MATERIALS, 2011, 40 (02) : 195 - 200