Removal of Mn(II) from hydrochloric acid leach liquors of nickel laterite ore through microbubble oxidation and acid leaching

被引:7
作者
Xu, Ziyang [1 ,2 ]
Wei, Guangye [1 ]
Yu, Zhihui [1 ]
Meng, Long [1 ]
Zheng, Shili [1 ]
Qu, Jingkui [1 ]
Qi, Tao [1 ]
机构
[1] Chinese Acad Sci, Natl Engn Res Ctr Green Recycling Strateg Met Res, Inst Proc Engn, Beijing 100190, Peoples R China
[2] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
Nickel laterite ore; Microbubble; Acid leach liquor; Purification; Oxygen mass transfer; SULFURIC-ACID; MANGANESE; EXTRACTION; METALS; DEGRADATION; REDUCTION; ABSENCE; COBALT;
D O I
10.1016/j.hydromet.2022.105862
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Leach liquor obtained from atmospheric acid leaching of nickel laterite with HCl solution contain large concentrations of Mn and Mg. This paper presents a method for separating large amounts of Mn and Mg from Ni and Co chloride solution by microbubble aeration oxidation and acid leaching processes. Such methods utilize the multiple advantages of the microbubble technology, such as large specific surface area, negatively charged surface, long stagnation, high oxygen mass transfer efficiency, and the ability to generate active oxygen. The effects of aeration pore size, oxygen flow rate, reaction temperature, stirring speed, and pH were studied. Under optimal experimental conditions (bubbling O-2 flow = 0.4 L/min, aeration aperture = 0.45 mu m, speed of agitation = 400 rpm, temperature = 50 ?, pH = 7), the recovery efficiency of Ni and Co were 99.3% and 89.0%, and the removal efficiency of Mn and Mg were 99.5% and 97.7%, respectively. Through XRD, XPS, and FTIR, it was found that soluble Mn was first oxidized to Mn3O4 and MnO2.H2O. In the acid dissolution process, Mn3O4 reacted with dilute sulfuric acid to form MnO2, which is insoluble in dilute acid, and was thus easily separated from Ni and Co. Analysis of the mass transfer process showed that the microbubble aeration method can greatly increase the oxygen mass transfer coefficient (0.073 s-1), accelerate the dissolution of O-2, and create conditions for the generation of active oxygen species.
引用
收藏
页数:9
相关论文
共 50 条
[21]   Selective leaching of nickel and cobalt from limonitic laterite using phosphoric acid: An alternative for value-added processing of laterite [J].
Li, Guanghui ;
Zhou, Qun ;
Zhu, Zhongping ;
Luo, Jun ;
Rao, Mingjun ;
Peng, Zhiwei ;
Jiang, Tao .
JOURNAL OF CLEANER PRODUCTION, 2018, 189 :620-626
[22]   Efficient removal of iron during partial neutralization of nickel laterite acid leach solution: DFT calculation and experimental verification of mechanism [J].
Mang, Changye ;
Li, Guanghui ;
Chen, Yanhu ;
Luo, Jun ;
Rao, Mingjun ;
Jiang, Tao .
HYDROMETALLURGY, 2023, 220
[23]   Collaborative extraction of valuable components from saprolitic laterite ore through two-stage nitric acid leaching [J].
Yu, Jiancheng ;
Ma, Baozhong ;
Shi, Longfei ;
Wang, Chengyan ;
Chen, Yongqiang .
JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2024, 138 :311-322
[24]   Enhanced extraction of nickel from limonitic laterite via improved nitric acid pressure leaching process [J].
He, Fei ;
Ma, Baozhong ;
Qiu, Zhijun ;
Wang, Chengyan ;
Chen, Yongqiang ;
Hu, Xiujuan .
MINERALS ENGINEERING, 2023, 201
[25]   Reagent selection for recovery of nickel and cobalt from nitric acid nickel laterite leach solutions by solvent extraction [J].
Hutton-Ashkenny, M. ;
Ibana, D. ;
Barnard, K. R. .
MINERALS ENGINEERING, 2015, 77 :42-51
[26]   Solvent Extraction Separation of Co(II) from Synthetic Leaching Sulfate Solution of Nickel Laterite Ore with High Magnesium Content [J].
Lee, Manseung ;
Kim, Sangbae ;
Choi, Youngyoon ;
Chae, Jonggwee .
MATERIALS TRANSACTIONS, 2011, 52 (06) :1211-1215
[27]   Optimization of the Atmospheric Acid Leaching Process for the Recovery of Nickel and Cobalt from Iron-Rich Lateritic Ore [J].
Ribeiro, Gabriela da Silva ;
Nascimento, Naiara de Deus ;
Ribeiro, Rodrigo da Silveira ;
Miranda, Marcelo de Paole Moreira ;
Martins, Paulo Roberto ;
Caetano, Gabriela Costa ;
de Andrade, Laiane Alves ;
Ostroski, Indianara Conceicao .
MINING METALLURGY & EXPLORATION, 2025, :1127-1140
[28]   Atmospheric acid leaching of powdery Ni-Co-Fe alloy derived from reductive roasting of limonitic laterite ore and recovery of battery grade iron phosphate [J].
Rao, Mingjun ;
Chen, Jing ;
Zhang, Tao ;
Hu, Meishi ;
You, Jinxiang ;
Luo, Jun .
HYDROMETALLURGY, 2023, 218
[29]   Thermodynamic analysis and application for preparing FePO4 from nitric acid pressure leach laterite residue by selective leaching in phosphoric acid and induced precipitation [J].
Cao, Zhihe ;
Ma, Baozhong ;
Wang, Chengyan ;
Shi, Bingding ;
Chen, Yongqiang .
HYDROMETALLURGY, 2022, 212
[30]   Separation of Co(II), Cu(II), Ni(II) and Mn(II) from synthetic hydrochloric acid leaching solution of spent lithium ion batteries by solvent extraction [J].
Viet Nhan Hoa Nguyen ;
Lee, Man Seung .
PHYSICOCHEMICAL PROBLEMS OF MINERAL PROCESSING, 2020, 56 (04) :599-610