Immersion Corrosion of Sn-Ag and Sn-Bi Alloys as Successors to Sn-Pb Alloy with Electronic and Jewelry Applications

被引:12
作者
Satizabal, Luz M. [1 ]
Poloni, Erik [2 ]
Bortolozo, Ausdinir D. [2 ]
Osorio, Wislei R. [1 ,2 ]
机构
[1] Univ Estadual Campinas, Sch Technol, BR-13484332 Limeira, SP, Brazil
[2] Univ Estadual Campinas, Res Grp Mfg Adv Mat, Sch Appl Sci FCA, Campus Limeira,1300,Pedro Zaccaria St, BR-13484350 Limeira, SP, Brazil
关键词
gold plating; green alloys; immersion corrosion; lead-free alloys; Sn-Ag alloys; Sn-Bi alloys; LEAD-FREE SOLDERS; ELECTROCHEMICAL CORROSION; MECHANICAL-PROPERTIES; TIN-LEAD; BEHAVIOR; MICROSTRUCTURE; ETHANOL; BOARD; STEEL; ACID;
D O I
10.5006/2039
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A comparative investigation on the degradation in two distinctive corrosive media (NaCl and ethanol) of Sn-2 wt% Ag, Sn-10 wt% Bi, and Sn-22 wt% Pb alloys and the traditional Sn-40 wt% Pb alloys is performed. The deterioration is represented by both weight variation and corrosion rate in both 0.9% NaCl solution and anhydrous ethanol. It is shown that both uncoated and gold-plated samples are more susceptible to deterioration in NaCl than ethanol medium. A mechanical-to-corrosion (M/C) ratio is determined for each examined alloy. Considering the relative weights and costs associated with both M/C ratio and environmentally-friendly aspects, the Sn-Bi alloy is a potential successor for the traditional Sn-Pb alloys.
引用
收藏
页码:1064 / 1080
页数:17
相关论文
共 50 条
  • [31] Evaluation of Solidification and Interfacial Reaction of Sn-Bi and Sn-Bi-In Solder Alloys in Copper and Nickel Interfaces
    Leal, Jaderson Rodrigo da Silva
    Reyes, Rodrigo Andre Valenzuela
    de Gouveia, Guilherme Lisboa
    Coury, Francisco Gil
    Spinelli, Jose Eduardo
    METALS, 2024, 14 (09)
  • [32] Investigating the Effects of Rapid Precipitation of Bi in Sn on the Shear Strength of BGA Sn-Bi Alloys
    Qichao Hao
    Xin F. Tan
    Stuart D. McDonald
    Keith Sweatman
    Tetsuya Akaiwa
    Kazuhiro Nogita
    Journal of Electronic Materials, 2024, 53 : 1223 - 1238
  • [33] Effect of addition of Cu on the properties of eutectic Sn-Bi solder alloy
    Alam, S. N.
    Jindal, N.
    Naithani, N.
    MATERIALS SCIENCE-POLAND, 2019, 37 (02) : 212 - 224
  • [34] Effects of Stacking Sequence of Electrodeposited Sn and Bi Layers on reflowed Sn-Bi Solder Alloys
    Lee, Seen Fang
    Goh, Yingxin
    Haseeb, A. S. M. A.
    2012 35TH IEEE/CPMT INTERNATIONAL ELECTRONICS MANUFACTURING TECHNOLOGY SYMPOSIUM (IEMT), 2012,
  • [35] Microalloying effects of Sb and Ag on the microstructural evolution of eutectic Sn-Bi alloys
    Fowler, Hannah N. N.
    Tay, Sui Xiong
    Blendell, John
    Handwerker, Carol A. A.
    MRS ADVANCES, 2023, 8 (14) : 763 - 767
  • [36] Mechanical properties of Sn-Ag lead-free solder alloys based on the dendritic array and Ag3Sn morphology
    Osorio, Wislei R.
    Leiva, Daniel R.
    Peixoto, Leandro C.
    Garcia, Leonardo R.
    Garcia, Amauri
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 562 : 194 - 204
  • [37] Synthesis of Sn-Ag binary alloy powders by mechanical alloying
    Zhang Hong
    Tang Wen-Ming
    Xu Guang-Qing
    Wu Yu-Cheng
    Zheng Zhi-Xiang
    MATERIALS CHEMISTRY AND PHYSICS, 2010, 122 (01) : 64 - 68
  • [38] Wetting Behavior and Mechanical Properties of Sn-Zn and Sn-Pb Solder Alloys
    Leonardo R. Garcia
    Wislei R. Osório
    Leandro C. Peixoto
    Amauri Garcia
    Journal of Electronic Materials, 2009, 38 : 2405 - 2414
  • [39] Interface analysis of pure Sn, pure Ag and Sn-Ag binary alloys in H2SO4
    Ameer, M. A.
    Ghoneim, A. A.
    Heakal, F.
    Fekry, A. M.
    SURFACE AND INTERFACE ANALYSIS, 2010, 42 (02) : 95 - 101
  • [40] Improvement of microstructure and tensile properties of Sn-Bi-Ag alloy by heterogeneous nucleation of β-Sn on Ag3Sn
    Yang, Tianqi
    Zhao, Xiuchen
    Xiong, Zishan
    Tan, Wei
    Wei, Yuhang
    Tan, Chengwen
    Yu, Xiaodong
    Wang, Yingchun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 785