Effect of Titanium Substitution on Magnetic Properties and Microstructure of Nanocrystalline Monophase Nd-Fe-B Magnets

被引:6
作者
Wang Cong [2 ]
Guo ZhiMeng [2 ]
Sui YanLi [1 ]
Bao XiaoQian [1 ]
Chen ZhiAn [3 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met & Mat, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Dept Mat Engn, Beijing 100083, Peoples R China
[3] Beijing Zhong Ke San Huan Hitech Co Ltd, Beijing 100190, Peoples R China
基金
中国国家自然科学基金;
关键词
NB; CO;
D O I
10.1155/2012/425028
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Nd12.3Fe81.7-xTixB6.0 (x = 0.5-3.0) ribbons have been prepared by rapid quenching and subsequent annealing treatment. Effect of Ti substitution and annealing treatment on the microstructure, magnetic properties, and crystallization behavior of the ribbons was systematically investigated by the methods of differential scanning calorimeter (DSC), X-ray diffraction (XRD), transmission electron microscopy (TEM), and vibrating sample magnetometer (VSM). It is found that Ti addition may increase the crystallization temperature and stabilize the amorphous phase. Ti element inhibits the grain growth during crystallization process and finally refines the microstructure. The exchange coupling interactions and magnetic properties of the ribbons increase with increasing x from 0.5 to 1 and then decrease with further increasing x >= 1.5. Optimum magnetic properties with (BH)(max) = 151.6 kJ/m(3), H-ci = 809.2 kA/m, J(r) = 1.02 T are achieved in the Nd12.3Fe80.7Ti1B6.0 ribbons annealed at 600 degrees C for 10 min.
引用
收藏
页数:5
相关论文
共 50 条
[41]   Effect of cobalt substitution on magnetic properties and microstructure of nanocrystalline (NdDyTb)12.3(FeZrNbCu)81.7B6.0 ribbons [J].
Bao Xiaoqian ;
Gao Xuexu ;
Zhang Maocai ;
Zhu Jie ;
Zhou Shouzeng .
JOURNAL OF RARE EARTHS, 2009, 27 (03) :501-505
[42]   Anisotropic nanocomposite Nd-Fe-B magnets produced by hot deformation with assistance of Nd-Cu [J].
Hosokawa, Akihide ;
Takagi, Kenta .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2019, 489
[43]   Effect of DyF3 on the corrosion behavior of hot-pressed Nd-Fe-B permanent magnets [J].
Sueptitz, R. ;
Sawatzki, S. ;
Moore, M. ;
Uhlemann, M. ;
Gutfleisch, O. ;
Gebert, A. .
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2015, 66 (02) :152-157
[44]   Improvement of corrosion resistance in Nd-Fe-B sintered magnets by intergranular additions of Sn [J].
Ni, Junjie ;
Zhou, Shutai ;
Jia, Zhengfeng ;
Wang, Changzheng .
JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 588 :558-561
[45]   Strategy for optimizing the diffusion efficiency of hot-deformed Nd-Fe-B magnets [J].
Zhou, Qing ;
Zeng, Weiwei ;
Lei, Chao ;
He, Jiayi ;
Lu, Qiyun ;
Lu, Cifu ;
Tang, Renheng ;
Liao, Xuefeng .
JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
[46]   Temperature-dependent Dy diffusion processes in Nd-Fe-B permanent magnets [J].
Loeewe, K. ;
Brombacher, C. ;
Katter, M. ;
Gutfleisch, O. .
ACTA MATERIALIA, 2015, 83 :248-255
[47]   The properties and microstructure of Nd-Fe-B nanowires fabricated by electrochemical deposition using porous Alumina templates [J].
Kang, Licong ;
Cui, Chunxiang ;
Yang, Wei ;
Zhang, Yuanyuan ;
Guo, Manfei .
MATERIALS CHEMISTRY AND PHYSICS, 2020, 242
[48]   The effects of Co on the enhancement of magnetic properties by modifying the intergranular phase in Nd-Fe-B alloys [J].
Liang, Y. ;
Deng, Q. ;
Tan, X. H. ;
Li, H. ;
Xu, H. .
SCIENTIFIC REPORTS, 2019, 9 (1)
[49]   Influence of quenching rate and composition on optimal annealing temperature of Nd-Fe-B based nanocrystalline hard magnetic alloys [J].
Huyen, N. T. T. ;
Yen, N. H. ;
Thanh, P. T. ;
Huu, D. T. ;
Thuy, D. M. ;
Thuy, N. M. ;
Dan, N. H. .
MATERIALS SCIENCE AND TECHNOLOGY, 2012, 28 (08) :948-952
[50]   Synergistic influence mechanism of B-Ga content on microstructures and magnetic properties of Nd-Fe-B ribbons [J].
Wei, Weiguo ;
Jiang, Qingzheng ;
Li, Huixia ;
Yang, Guo ;
Kan, Mengping ;
Mo, Zixiang ;
Li, Jianming ;
Zhong, Zhenchen .
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1000