A technique for the measurement of reinforcement fibre tensile strength at sub-millimetre gauge lengths

被引:27
作者
Thomason, JL
Kalinka, G
机构
[1] Owens Corning Sci & Technol Ctr, Granville, OH 43023 USA
[2] Fed Inst Mat Res & Testing, Berlin, Germany
关键词
glass fibres; strength; mechanical testing;
D O I
10.1016/S1359-835X(00)00122-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The strength of composite reinforcement fibres is normally measured on samples of much greater length than the actual residual fibre lengths found in many composite materials. This is due to a number of limitations of the standard techniques which are employed. We present a description of a technique which enables values for the tensile strength of composite reinforcement fibres at short gauge lengths to be obtained. The technique is based on an adaptation of a micro-mechanical test apparatus for fibre pullout measurements. Data is presented which was obtained at gauge lengths of 180-380 mum on E-glass and S-2 glass(R) fibres taken from different chopped reinforcement products. The technique can be used at gauge lengths as short as 20 mum. The data indicates that the values of average fibre strength in these products are significantly below the pristine glass strength values. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:85 / 90
页数:6
相关论文
共 24 条
[1]  
AKAY M, 1991, J MATER SCI, V26, P2731, DOI 10.1007/BF02387744
[2]   POLYPROPYLENE LOW-DENSITY POLYETHYLENE BLEND MATRICES AND SHORT GLASS-FIBERS BASED COMPOSITES .1. MECHANICAL DEGRADATION OF FIBERS AS A FUNCTION OF PROCESSING METHOD [J].
ARROYO, M ;
AVALOS, F .
POLYMER COMPOSITES, 1989, 10 (02) :117-121
[3]  
Bailey R., 1987, INT POLYM PROC, V2, P94, DOI DOI 10.3139/217.870094
[4]   PROCESSING PROPERTY CHARACTERISTICS FOR LONG GLASS-FIBER REINFORCED POLYAMIDE [J].
BAILEY, RS ;
DAVIES, M ;
MOORE, DR .
COMPOSITES, 1989, 20 (05) :453-460
[5]   STIFFNESS AND STRENGTH OF A POLYAMIDE THERMOPLASTIC REINFORCED WITH GLASS AND CARBON-FIBERS [J].
CURTIS, PT ;
BADER, MG ;
BAILEY, JE .
JOURNAL OF MATERIALS SCIENCE, 1978, 13 (02) :377-390
[6]   MECHANICAL DEGRADATION OF GLASS-FIBERS DURING COMPOUNDING WITH POLYPROPYLENE [J].
FISA, B .
POLYMER COMPOSITES, 1985, 6 (04) :232-241
[7]   FIBER DEGRADATION DURING PROCESSING OF SHORT FIBER REINFORCED THERMOPLASTICS [J].
FRANZEN, B ;
KLASON, C ;
KUBAT, J ;
KITANO, T .
COMPOSITES, 1989, 20 (01) :65-76
[8]   AN ADVANCED EQUIPMENT FOR SINGLE-FIBER PULL-OUT TEST DESIGNED TO MONITOR THE FRACTURE PROCESS [J].
HAMPE, A ;
KALINKA, G ;
MERETZ, S ;
SCHULZ, E .
COMPOSITES, 1995, 26 (01) :40-46
[9]   Fatigue fracture mechanisms and fractography of short-glassfibre-reinforced polyamide 6 [J].
Horst, JJ ;
Spoormaker, JL .
JOURNAL OF MATERIALS SCIENCE, 1997, 32 (14) :3641-3651
[10]   INVESTIGATION OF MORPHOLOGY-DEPENDENT FRACTURE-BEHAVIOR WITH THE SINGLE-FIBER PULL-OUT TEST [J].
MERETZ, S ;
AUERSCH, W ;
MAROTZKE, C ;
SCHULZ, E ;
HAMPE, A .
COMPOSITES SCIENCE AND TECHNOLOGY, 1993, 48 (1-4) :285-290