Effect of Sr addition on texture evolution of Mg-3Al-1Zn (AZ31) alloy during extrusion

被引:54
作者
Sadeghi, Alireza [1 ]
Hoseini, Majid [1 ]
Pekguleryuz, Mihriban [1 ]
机构
[1] McGill Univ, Dept Min & Mat Sci, Montreal, PQ H3A 2B2, Canada
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2011年 / 528卷 / 7-8期
基金
加拿大自然科学与工程研究理事会;
关键词
Mg alloys; Sr; Thermo-mechanical processing; Dynamic recrystallization; Texture evolution; MG-AL-SR; MECHANICAL-PROPERTIES; MAGNESIUM ALLOY; CREEP RESISTANCE; CA ALLOYS; MICROSTRUCTURE; RECRYSTALLIZATION; BEHAVIOR; STRONTIUM; DEFORMATION;
D O I
10.1016/j.msea.2010.12.091
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
An experimental investigation of texture evolution during the elevated temperature extrusion of AZ31 alloys containing strontium (Sr) additions is reported. The crystallographic texture of hot extruded alloys containing different levels of Sr has been examined. Hot compression tests have been carried out in order to investigate the hot deformation behavior of the as-cast alloys. It was seen that, at different extrusion temperatures and levels of Sr, different dynamic recrystallization (DRX) mechanisms become dominant which affect the final texture. At lower temperatures and at low levels of Sr, the bulging of grain boundaries was activated, resulting in a necklaced grain structure. Furthermore, a strong deformation texture of < 10.0 > parallel to extrusion direction was developed as a result of bulging at the grain boundaries. Twining which was activated in the early stages of deformation, acted as nucleation sites for DRX. In contrast, at high temperatures and high levels of Sr, particle stimulated nucleation (PSN) becomes significant resulting in the weakening of the overall texture with the recrystallization of new grains of random orientation. In order to prevent the surface cracking in the extruded sample, a limit for Sr concentration and deformation temperature was determined. A shoulder region was found in between the bulging and PSN-dominant areas where both mechanisms are active. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:3096 / 3104
页数:9
相关论文
共 34 条
[1]   Microstructure and corrosion behavior of Mg-Sn-Ca alloys after extrusion [J].
Abu Leil, T. ;
Hort, N. ;
Dietzel, W. ;
Blawert, C. ;
Huang, Y. ;
Kainer, K. U. ;
Rao, K. P. .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2009, 19 (01) :40-44
[2]  
Baril E, 2003, JOM-J MIN MET MAT S, V55, pA34
[3]   Effects of zinc, lithium, and indium on the grain size of magnesium [J].
Becerra, A. ;
Pekguleryuz, M. .
JOURNAL OF MATERIALS RESEARCH, 2009, 24 (05) :1722-1729
[4]   Microstructure and texture development during hydrostatic extrusion of magnesium alloy AZ31 [J].
Bohlen, J ;
Yi, SB ;
Swiostek, J ;
Letzig, D ;
Brokmeier, HG ;
Kainer, KU .
SCRIPTA MATERIALIA, 2005, 53 (02) :259-264
[5]   Effect of materials and temperature on the forward extrusion of magnesium alloys [J].
Chandrasekaran, M ;
John, YMS .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 381 (1-2) :308-319
[6]   Effects of extrusion ratio on the microstructure and mechanical properties of AZ31 Mg alloy [J].
Chen, Yongjun ;
Wang, Qudong ;
Peng, Jianguo ;
Zhai, Chunquan ;
Ding, Wenjiang .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 182 (1-3) :281-285
[7]   Microstructural analysis of the improved creep resistance of a die-cast magnesium-aluminium-rare earth alloy by strontium additions [J].
Dargusch, M. S. ;
Zhu, S. M. ;
Nie, J. F. ;
Dunlop, G. L. .
SCRIPTA MATERIALIA, 2009, 60 (02) :116-119
[8]  
Humphreys FJ., 2012, RECRYSTALLIZATION RE
[9]  
Jing B., 2006, MAT SCI ENG, VA419, P181
[10]   Effect of extrusion on microstructures, and mechanical and creep properties of Mg-Al-Sr and Mg-Al-Sr-Ca alloys [J].
Jing, Bai ;
Yangshan, Sun ;
Feng, Xue ;
Shan, Xue ;
Jing, Qiang ;
Tao Weijian .
SCRIPTA MATERIALIA, 2006, 55 (12) :1163-1166