Passivation and dissociation of P b-type defects at a-SiO2/Si interface*

被引:2
作者
Liu, Xue-Hua [1 ]
Xie, Wei-Feng [1 ]
Liu, Yang [2 ,3 ]
Zuo, Xu [1 ,4 ,5 ]
机构
[1] Nankai Univ, Coll Elect Informat & Opt Engn, Tianjin 300350, Peoples R China
[2] China Acad Engn Phys, Microsyst & Terahertz Res Ctr, Chengdu 610200, Peoples R China
[3] China Acad Engn Phys, Inst Elect Engn, Mianyang 621999, Sichuan, Peoples R China
[4] Nankai Univ, Key Lab Photoelect Thin Film Devices & Technol Ti, Tianjin 300350, Peoples R China
[5] Nankai Univ, Engn Res Ctr Thin Film Optoelect Technol, Minist Educ, Tianjin 300350, Peoples R China
关键词
first-principles calculation; a-SiO2; Si interface; P (b)-type defects; equilibrium density; 100; SI/SIO2; (111)SI/SIO2 INTERFACE; HYPERFINE INTERACTIONS; H-2; PASSIVATION; HYDROGEN; KINETICS; CENTERS; STATE; SI;
D O I
10.1088/1674-1056/ac0e20
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
It is well known that in the process of thermal oxidation of silicon, there are P (b)-type defects at amorphous silicon dioxide/silicon (a-SiO2/Si) interface due to strain. These defects have a very important impact on the performance and reliability of semiconductor devices. In the process of passivation, hydrogen is usually used to inactivate P (b)-type defects by the reaction P (b) + H-2 -> P H-b + H. At the same time, P H-b centers dissociate according to the chemical reaction P (b) H -> P (b) +H. Therefore, it is of great significance to study the balance of the passivation and dissociation. In this work, the reaction mechanisms of passivation and dissociation of the P (b)-type defects are investigated by first-principles calculations. The reaction rates of the passivation and dissociation are calculated by the climbing image-nudged elastic band (CI-NEB) method and harmonic transition state theory (HTST). By coupling the rate equations of the passivation and dissociation reactions, the equilibrium density ratio of the saturated interfacial dangling bonds and interfacial defects (P (b), P (b0), and P (b1)) at different temperatures is calculated.
引用
收藏
页数:7
相关论文
共 34 条
[1]   DISSOCIATION KINETICS OF HYDROGEN-PASSIVATED (111) SI-SIO2 INTERFACE DEFECTS [J].
BROWER, KL .
PHYSICAL REVIEW B, 1990, 42 (06) :3444-3453
[2]   KINETICS OF H-2 PASSIVATION OF PB CENTERS AT THE (111) SI-SIO2 INTERFACE [J].
BROWER, KL .
PHYSICAL REVIEW B, 1988, 38 (14) :9657-9666
[3]   SI-29 HYPERFINE-STRUCTURE OF UNPAIRED SPINS AT THE SI/SIO2 INTERFACE [J].
BROWER, KL .
APPLIED PHYSICS LETTERS, 1983, 43 (12) :1111-1113
[4]   CHEMICAL-KINETICS OF HYDROGEN AND (111) SI-SIO2 INTERFACE DEFECTS [J].
BROWER, KL ;
MYERS, SM .
APPLIED PHYSICS LETTERS, 1990, 57 (02) :162-164
[5]   ESR CENTERS, INTERFACE STATES, AND OXIDE FIXED CHARGE IN THERMALLY OXIDIZED SILICON WAFERS [J].
CAPLAN, PJ ;
POINDEXTER, EH ;
DEAL, BE ;
RAZOUK, RR .
JOURNAL OF APPLIED PHYSICS, 1979, 50 (09) :5847-5854
[6]  
Cheng Y., 1977, PROG SURF SCI, V8, P181
[7]   HYPERFINE INTERACTIONS IN CLUSTER-MODELS OF THE PB DEFECT CENTER [J].
COOK, M ;
WHITE, CT .
PHYSICAL REVIEW B, 1988, 38 (14) :9674-9685
[8]   HYPERFINE INTERACTIONS OF THE PB CENTER AT THE SIO2 SI(111) INTERFACE [J].
COOK, M ;
WHITE, CT .
PHYSICAL REVIEW LETTERS, 1987, 59 (15) :1741-1744
[9]   A climbing image nudged elastic band method for finding saddle points and minimum energy paths [J].
Henkelman, G ;
Uberuaga, BP ;
Jónsson, H .
JOURNAL OF CHEMICAL PHYSICS, 2000, 113 (22) :9901-9904
[10]  
[Hong Zhuocheng 洪卓呈], 2020, [系统仿真学报, Journal of System Simulation], V32, P2362