Hydrolytic degradation of biodegradable poly(butylene adipate-co-terephthalate) (PBAT) - Towards an understanding of microplastics fragmentation

被引:43
作者
Deshoulles, Q. [1 ,2 ]
Le Gall, M. [1 ]
Benali, S. [3 ]
Raquez, J-M [3 ]
Dreanno, C. [2 ,4 ]
Arhant, M. [1 ]
Priour, D. [1 ]
Cerantola, S.
Stoclet, G. [5 ]
Le Gac, P. Y. [1 ,6 ]
机构
[1] Ctr Bretagne, Lab Comportement Struct Mer, Ifremer, F-29280 Plouzane, France
[2] Ctr Bretagne, Lab Detect Capteurs & Mesures, Ifremer, F-29280 Plouzane, France
[3] Univ Mons, Ctr Innovat & Res Mat & Polymers CIRMAP, Lab Polymer & Compos Mat LPCM, Pl Parc 23, B-7000 Mons, Belgium
[4] Univ Bretagne Occidentale, Serv Gen Plateformes, Plateforme RMN RPE, 6 Av Gorgeu,CS93837, F-29238 Brest 3, France
[5] Univ Lille, Unite Materiaux & Transformat, Cent Lille, INRAE,CNRS,UMR 8207,UMET, F-59000 Lille, France
[6] IFREMER, BP 70 29260, Plouzane, France
关键词
Hydrolysis; PBAT; Molar mass; Embrittlement; Biodegradable; Microplastics; BEHAVIOR; POLYMERS; FILMS; DUCTILE; PHASE; PET;
D O I
10.1016/j.polymdegradstab.2022.110122
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The long-term behaviour of PBAT subjected to hydrolytic ageing is investigated in this paper. Samples were aged in water at several temperatures ranging from 80 to 100 degrees C for different durations. Changes in physico-chemical properties were investigated through NMR, GPC, DSC and X-Ray analyses and embrittlement was assessed by tensile tests. It is demonstrated that hydrolysis of PBAT occurs first on the ester group located between the terephthalate and adipate groups leading to a decrease in molar mass. For longer ageing durations, the ester situated within the adipate group undergoes hydrolysis. An increase in crystallinity ratio and a decrease in amorphous layer thickness was observed as consequences of the chain scission process. Finally, a clear change in mechanical behaviour is noted; for the early stages of ageing, the polymer exhibits a ductile behaviour while for longer ageing durations, the polymer is brittle due to a lack of chain entanglement. This transition takes place once the molar mass of PBAT falls below 11 kg/mol, i.e. when a critical molar mass M'(c) is reached.
引用
收藏
页数:9
相关论文
共 31 条
[11]   A critical molar mass separating the ductile and brittle regimes as revealed by thermal oxidation in polypropylene [J].
Fayolle, B ;
Audouin, L ;
Verdu, J .
POLYMER, 2004, 45 (12) :4323-4330
[12]   Review: degradation-induced embrittlement in semi-crystalline polymers having their amorphous phase in rubbery state [J].
Fayolle, Bruno ;
Richaud, Emmanuel ;
Colin, Xavier ;
Verdu, Jacques .
JOURNAL OF MATERIALS SCIENCE, 2008, 43 (22) :6999-7012
[13]   An overview on properties and applications of poly(butylene adipate-co-terephthalate)-PBAT based composites [J].
Ferreira, Filipe V. ;
Cividanes, Luciana S. ;
Gouveia, Rubia F. ;
Lona, Liliane M. F. .
POLYMER ENGINEERING AND SCIENCE, 2019, 59 (s2) :E7-E15
[14]   Biodegradation Behavior of Poly(Butylene Adipate-Co-Terephthalate) (PBAT), Poly(Lactic Acid) (PLA), and Their Blend in Freshwater with Sediment [J].
Fu, Ye ;
Wu, Gang ;
Bian, Xinchao ;
Zeng, Jianbing ;
Weng, Yunxuan .
MOLECULES, 2020, 25 (17)
[15]  
Galgani F, 2015, MARINE ANTHROPOGENIC LITTER, P29, DOI 10.1007/978-3-319-16510-3_2
[16]   Molecular-Scale Understanding of the Embrittlement in Polyethylene Ocean Debris [J].
Garvey, Christopher J. ;
Imperor-Clerc, Marianne ;
Rouziere, Stephan ;
Gouadec, Gwenael ;
Boyron, Olivier ;
Rowenczyk, Laura ;
Mingotaud, Anne Francoise ;
ter Halle, Alexandra .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2020, 54 (18) :11173-11181
[17]   Characterization and degradation behavior of poly(butylene adipate-co-terephthalate)s [J].
Herrera, R ;
Franco, L ;
Rodríguez-Galán, A ;
Puiggalí, J .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 2002, 40 (23) :4141-4157
[18]   Polymer crystallinity and the ductile to brittle transition [J].
Hocker, Samuel J. A. ;
Kim, William T. ;
Schniepp, Hannes C. ;
Kranbuehl, David E. .
POLYMER, 2018, 158 :72-76
[19]   A fundamental study on photo-oxidative degradation of linear low density polyethylene films at embrittlement [J].
Hsu, Yu-Chieh ;
Weir, Michael P. ;
Truss, Rowan W. ;
Garvey, Christopher J. ;
Nicholson, Timothy M. ;
Halley, Peter J. .
POLYMER, 2012, 53 (12) :2385-2393
[20]   Hydrolytic ageing of polyamide 11. 1. Hydrolysis kinetics in water [J].
Jacques, B ;
Werth, M ;
Merdas, I ;
Thominette, F ;
Verdu, J .
POLYMER, 2002, 43 (24) :6439-6447