Tailoring the mechanical properties of Mg-Zn magnesium alloy by calcium addition and hot extrusion process

被引:105
作者
Zareian, Z. [1 ]
Emamy, M. [1 ]
Malekan, M. [1 ]
Mirzadeh, H. [1 ]
Kim, W. J. [2 ]
Bahmani, A. [1 ]
机构
[1] Univ Tehran, Coll Engn, Sch Met & Mat Engn, POB 11155-4563, Tehran, Iran
[2] Hongik Univ, Dept Mat Sci & Engn, Sangsu Dong 72-1, Seoul 121791, South Korea
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 774卷 / 774期
关键词
Mg-Zn-Ca alloys; Grain refinement; Growth restriction factor; Electron backscattered diffraction (EBSD); Mechanical properties; GRAIN-REFINEMENT; HIGH-STRENGTH; AS-CAST; FRACTURE-TOUGHNESS; MICROSTRUCTURE; TEXTURE; DEFORMATION; CORROSION; BEHAVIOR; EVOLUTION;
D O I
10.1016/j.msea.2020.138929
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Grain refinement and enhanced mechanical properties of Mg-2Zn-xCa alloys (with a wide range of calcium contents from 0 to 5 wt%) were studied in both as-cast and extruded conditions. It was revealed that Ca addition can effectively refine the grain size of the ingots based on the growth restriction factor (GRF) mechanism, where at high Ca additions, the dendritic microstructure was obtained. By increasing the amount of Ca, the binary Mg-Zn phase was replaced by the Ca2Mg6Zn3 phase and at high Ca contents, the Mg2Ca phase appeared in the microstructure. The tensile properties were enhanced at low Ca additions (up to 0.3 wt%) due to the grain refinement but they were deteriorated at higher Ca additions due to the formation of grain boundary second phases. Accordingly, the ultimate tensile strength (UTS) of 228 MPa and total elongation of 20% was obtained for the as-cast Mg-2Zn-0.3Ca (ZX20) alloy. During hot extrusion, significant grain refinement and the fracturing and dispersion of second phase particles were observed. The grain size refinement beyond similar to 1 wt% Ca was negligible and extrusion defects were observed at higher Ca contents, and hence, the best combination of mechanical properties was obtained for the Mg-2Zn-1Ca (ZX21) alloy with UTS of 283 MPa and elongation to failure of 29%. This alloy showed a desirable work-hardening behavior and the best combination of tensile properties, where the product of tensile strength and total elongation reached as high as similar to 8000 MPa%. Finally, the yield stress of the alloys was correlated to the average grain size via the classical Hall-Petch plot with a slope of 228.5 MPa mu m(0.5).
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Unraveling the effects of Zn addition and hot extrusion process on the microstructure and mechanical properties of as-cast Mg-2Al magnesium alloy
    Razzaghi, Marjan
    Mirzadeh, Hamed
    Emamy, Massoud
    VACUUM, 2019, 167 : 214 - 222
  • [2] Mechanical properties of Mg-Gd-Zr alloy by Nd addition combined with hot extrusion
    Zheng, Liu-wei
    Zhuang, Yong-peng
    LI, Jun-jian
    Wang, Hong-xia
    LI, Hang
    Hou, Hua
    Wang, Li-fei
    Luo, Xiao-ping
    Shin, Kwang Seon
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2022, 32 (06) : 1866 - 1880
  • [3] Effect of Ca-addition on dynamic recrystallization of Mg-Zn alloy during hot deformation
    Hradilova, Monika
    Montheillet, Frank
    Fraczkiewicz, Anna
    Desrayaud, Christophe
    Lejcek, Pavel
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 580 : 217 - 226
  • [4] Microstructure and mechanical properties of Mg-Zn-Ca-Zr alloy fabricated by hot extrusion-shearing process
    Wang, Boning
    Wang, Feng
    Wang, Zhi
    Zhou, Le
    Liu, Zheng
    Mao, Pingli
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 795
  • [5] Tailoring the Microstructure and Properties of Mg-2.0Zn-0.4Mn-4.0Al Alloy by Hot Extrusion
    Xiong, Yi
    Tang, Jin-jin
    Zha, Xiao-qin
    Wang, Shu-bo
    Cao, Wei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (23) : 13132 - 13140
  • [6] Effects of backward extrusion on mechanical and degradation properties of Mg-Zn biomaterial
    Peng, Qiuming
    Li, Xuejun
    Ma, Ning
    Liu, Riping
    Zhang, Hongjie
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2012, 10 : 128 - 137
  • [7] Effect of extrusion process on microstructure and mechanical and corrosion properties of biodegradable Mg-5Zn-1.5Y magnesium alloy
    Jafari, Hassan
    Tehrani, Amir Houshang Mojiri
    Tehrani, Mojiri
    Heydari, Mahsa
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2022, 29 (03) : 490 - 502
  • [8] Microstructure and mechanical properties of Mg-4Zn-0.5Ca alloy fabricated by the combination of forging, homogenization and extrusion process
    Kang, Jin-wen
    Wang, Cui-ju
    Deng, Kun-kun
    Nie, Kai-bo
    Bai, Yan
    Li, Wei-jian
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 720 : 196 - 206
  • [9] The effect of Ca addition on age hardening behaviors and mechanical properties in Mg-Zn alloy
    Eom, JP
    Jin, QL
    Lim, SG
    Hur, BY
    Park, WW
    MAGNESIUM ALLOYS 2003, PTS 1 AND 2, 2003, 419-4 : 307 - 311
  • [10] Effect of calcium addition on microstructure, casting fluidity and mechanical properties of Mg-Zn-Ce-Zr magnesium alloy
    Fu Yu
    Wang Han
    Liu Xiaoteng
    Hao Hai
    JOURNAL OF RARE EARTHS, 2017, 35 (05) : 503 - 509