Damage/ablation morphology of laser conditioned sapphire under 1064 nm laser irradiation

被引:11
作者
Jiang, Y. [1 ,2 ]
Xiang, X. [1 ]
Wang, H. J. [2 ]
Yuan, X. D. [2 ]
He, S. B. [2 ]
Lv, H. B. [2 ]
Zheng, W. G. [2 ]
Zu, X. T. [1 ]
机构
[1] Univ Elect Sci & Technol China, Dept Appl Phys, Chengdu 610054, Peoples R China
[2] China Acad Engn Phys, Res Ctr Laser Fus, Mianyang 621900, Peoples R China
关键词
Sapphire; Laser conditioning; Damage/ablation morphology; INDUCED DAMAGE THRESHOLD; FEMTOSECOND LASER; FUSED-SILICA; ABLATION; NANOSECOND; MITIGATION; CO2-LASER; PULSES; GROWTH;
D O I
10.1016/j.optlastec.2011.11.003
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
The damage/ablation morphologies and laser induced damage threshold (LIDT) of three different sapphire samples: original, 1064 nm laser conditioned and 10.6 mu m CO2 laser polished substrates are investigated with ns pulses laser irradiation. The results indicate that the damage resistance capability cannot be enhanced by 1064 nm laser conditioning or CO2 laser polishing. The damage/ablation morphology of 1064 nm-laser conditioned samples is same as that of the original sapphire. But it is different from the damage/ablation morphology of the CO2 laser polished sapphire. The "gentle and strong" ablation phases are observed in this work and several phenomena are observed in the two ablation phases. Ripple is observed in the "gentle" ablation processes, while convex spots and raised rims are observed in the "strong" ablation processes. Meanwhile, stripe damage and pin-points are observed in the CO2 laser conditioned sapphire after ns laser irradiation. The formation mechanisms of the phenomena are also discussed for the explanation of related damage/ablation morphology. The results may be helpful for the damage/ablation investigation of sapphire in high power laser systems. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:948 / 953
页数:6
相关论文
共 50 条
[41]   Growth of laser-induced damage in fused silica under nanosecond laser irradiation [J].
Qiu, Rong ;
Wang, Junbo ;
Ren, Huan ;
Li, Xiaohong ;
Shi, Pengcheng ;
Liu, Hao ;
Ma, Ping .
Qiangjiguang Yu Lizishu/High Power Laser and Particle Beams, 2012, 24 (05) :1057-1062
[42]   The evolution of coating threshold damage to peeling off under femtosecond laser irradiation [J].
Shi Feng ;
Zhu Zhi-Wu ;
Cheng Xiang-Ai ;
Dai Yi-Fan .
JOURNAL OF INFRARED AND MILLIMETER WAVES, 2017, 36 (03) :361-366
[43]   Dislocation analysis of germanium wafers under 1080 nm laser ablation [J].
Sha, YinChuan ;
Jia, ZhiChao ;
Li, Zewen ;
Pan, YunXiang ;
Nan, Pengyu ;
Ni, XiaoWu .
APPLIED OPTICS, 2020, 59 (23) :6803-6808
[44]   Damage growth characteristics of different initial damage sites of fused silica under 355 nm small laser beam irradiation [J].
Ma, Bin ;
Ma, Hongping ;
Jiao, Hongfei ;
Cheng, Xinbin ;
Wang, Zhanshan .
OPTICS AND LASER TECHNOLOGY, 2014, 57 :136-144
[45]   Sapphire (0001) surface modifications induced by long-pulse 1054 nm laser irradiation [J].
Luo, Sheng-Nian ;
Peralta, Pedro D. ;
Ma, Chi ;
Paisley, Dennis L. ;
Greenfield, Scott R. ;
Loomis, Eric N. .
APPLIED SURFACE SCIENCE, 2007, 253 (24) :9457-9466
[46]   Damage mechanism and morphology characteristics of chromium film in femtosecond laser rear-side ablation [J].
Wang, Wenjun ;
Jiang, Gedong ;
Mei, Xuesong ;
Wang, Kedian ;
Shao, Jinyou ;
Yang, Chengjuan .
APPLIED SURFACE SCIENCE, 2010, 256 (11) :3612-3617
[47]   Dependence of silicon ablation regimes on fluence during ultrafast laser irradiation [J].
Polek, M. ;
Hassanein, A. .
LASER AND PARTICLE BEAMS, 2016, 34 (01) :143-150
[48]   Study on the Laser Decontamination of Metal Surface at 1064 and 532 nm [J].
Won, Hui-Jun ;
Jung, Sun-Hee ;
Jung, Chong-Hun ;
Choi, Byung Seon ;
Moon, Jei-Kwon ;
Lee, Kune-Woo .
ASIAN JOURNAL OF CHEMISTRY, 2012, 24 (09) :4136-4140
[49]   Laser conditioning of dielectric oxide mirror coatings at 1064 nm [J].
Zhao, YN ;
Shao, JD ;
Wang, T ;
Zhang, DP ;
Fan, SH ;
Huan, JB ;
Gao, WD ;
Fan, ZX .
FIFTH INTERNATIONAL CONFERENCE ON THIN FILM PHYSICS AND APPLICATIONS, 2004, 5774 :599-602
[50]   Beam diameter dependence of surface damage threshold of fused silica fibers and preforms for nanosecond laser treatment at 1064 nm wavelength [J].
Mann, Guido ;
Pentzien, Simone ;
Krueger, Joerg .
APPLIED SURFACE SCIENCE, 2013, 276 :312-316