Defects and gallium contamination during focused ion beam micro machining

被引:0
作者
Lehrer, C [1 ]
Frey, L [1 ]
Petersen, S [1 ]
Mizutani, M [1 ]
Takai, M [1 ]
Ryssel, H [1 ]
机构
[1] Fraunhofer Inst Integrierte Schaltungen Bauelemen, D-91058 Erlangen, Germany
来源
2000 INTERNATIONAL CONFERENCE ON ION IMPLANTATION TECHNOLOGY, PROCEEDINGS | 2000年
关键词
D O I
暂无
中图分类号
TP3 [计算技术、计算机技术];
学科分类号
0812 ;
摘要
Low energy focused ion beam (FIB) systems are used for the modification of integrated circuits, the preparation of TEM samples, the processing of structures in the sub - 100 nm range, and for failure analysis. Focused gallium ion beams with diameters down to < 10 nm (Full Width at Half Maximum) allow high resolution secondary electron surface inspection as well as local removal and deposition of material with high accuracy by physical sputtering or ion induced chemistry. Besides beam diameter and shape, gallium implantation and defect generation limit the application of FIB micro machining towards minimum resolution and sensitive analysis. Even when the desired structural dimensions are achieved, functionality of the sample may be hindered by implanted gallium and introduced defects. In this paper, vertical gallium distribution and lateral contamination for highly focused ion beam applications are investigated. SIMS analysis and Monte Carlo simulation are used for the determination for doses ranging from FIB inspection (1.10(14) cm(-2)) to sputter removal at high doses (up to 1.10(18) cm(-2)). The measurements revealed surface concentrations of 1.10(18) cm(-3) up to 6.10(21) cm(-3) and deep ranging tails. At doses exceeding 1.10(17) cm(-2), the surface concentration reaches 6.10(21) cm(-3) and saturates, which is in agreement with simulations. Lateral contamination is determined by gallium background implantation due to inspection before processing and by non scanned neutrals. Defect generation was investigated by TEM. Even for typical FIB inspection at low doses (30 keV, 1.10(14) cm(-2)) an amorphous layer is generated with a thickness of 50 nm.
引用
收藏
页码:695 / 698
页数:4
相关论文
共 50 条
[31]   Simulation of Material Sputtering and Gallium Implantation during Focused Ion Beam Irradiation of a Silicon Substrate [J].
O. V. Podorozhniy ;
A. V. Rumyantsev ;
R. L. Volkov ;
N. I. Borgardt .
Semiconductors, 2023, 57 :58-64
[32]   The effects of dwell time on focused ion beam machining of silicon [J].
Sabouri, A. ;
Anthony, C. J. ;
Bowen, J. ;
Vishnyakov, V. ;
Prewett, P. D. .
MICROELECTRONIC ENGINEERING, 2014, 121 :24-26
[33]   Focused Ion Beam Milling as a Method for Machining Explosive Crystals [J].
Stirrup, Kerry-Ann M. ;
Gilpin, Christopher J. ;
Chen, Weinong W. .
PROPELLANTS EXPLOSIVES PYROTECHNICS, 2024, 49 (12)
[34]   FOCUSED ION-BEAM MACHINING OF SI, GAAS, AND INP [J].
PELLERIN, JG ;
GRIFFIS, DP ;
RUSSELL, PE .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1990, 8 (06) :1945-1950
[35]   Development of a local vacuum system for focused ion beam machining [J].
Masuzawa, Tsuneaki ;
Yoshida, Yoshikazu ;
Ikeda, Hiromichi ;
Oguchi, Keigo ;
Yamagishi, Hikaru ;
Wakabayashi, Yuji .
REVIEW OF SCIENTIFIC INSTRUMENTS, 2009, 80 (07)
[36]   Atomistic simulations of focused ion beam machining of strained silicon [J].
Guenole, J. ;
Prakash, A. ;
Bitzek, E. .
APPLIED SURFACE SCIENCE, 2017, 416 :86-95
[37]   Effect of Machining of Small Tools by Means of Focused Ion Beam [J].
Miura, Kohichi ;
Satoh, Syou ;
Yamada, Takazo ;
Lee, Hwa-Soo .
ADVANCES IN ABRASIVE TECHNOLOGY XV, 2012, 565 :588-593
[38]   Nanoholes with Defects Fabricated by Focused Ion Beam Milling [J].
Jiang, Xiaoxiao ;
Gu, Qiongchan ;
Wang, Fengwen ;
Ma, Zhenhe ;
Lv, Jiangtao ;
Si, Guangyuan .
NANOTECHNOLOGY AND MATERIAL ENGINEERING RESEARCH, 2013, 661 :70-73
[39]   Fabrication of Freeform Micro Optics by Focused Ion Beam [J].
Sun, Jining ;
Luo, Xichun ;
Chang, Wenlong ;
Ritchie, James M. .
PROCEEDINGS OF PRECISION ENGINEERING AND NANOTECHNOLOGY (ASPEN2011), 2012, 516 :414-419
[40]   Application of a focused ion beam system to micro and nanoengineering [J].
Langford, RM ;
Petford-Long, AK ;
Rommeswinkle, M ;
Egelkamp, S .
MATERIALS SCIENCE AND TECHNOLOGY, 2002, 18 (07) :743-748