Bending strength and crack-healing behavior of Al2O3/SiC composites ceramics

被引:41
作者
Kim, Hae Sook [3 ]
Kim, Mi Kyung [4 ]
Kang, Sun Bae [2 ]
Ahn, Seok Hwan [1 ]
Nam, Ki Woo [1 ]
机构
[1] Pukyong Natl Univ, Coll Engn, Pusan 608739, South Korea
[2] Pukyong Natl Univ, Joint Lab Expt & Res, Pusan 608739, South Korea
[3] Pukyong Natl Univ, Grad Sch, Pusan 608739, South Korea
[4] Kyoto Univ, Grad Sch, Uji, Kyoto 6110011, Japan
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2008年 / 483-84卷
关键词
Al2O3/SiC composite ceramics; bending strength (sigma(b)); crack healing; multi-composite ceramics; additive powder Y2O3;
D O I
10.1016/j.msea.2006.09.169
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Five kinds of ceramics were used to evaluate the bending strength under three-point bending. The bending test was carried out at room temperature. The crack-healing behavior and the bending strength of the crack-healed specimens were investigated from room temperature to 1723 K. The bending strength of Al2O3/SiC Composite ceramics is higher than that of Al2O3 monolithic. Al2O3/SiC composite ceramics could completely heal semicircular cracks with diameters 100 mu m. The bending strength of Al2O3/SiC composite ceramics significantly increased after heat treatment at 1573 K for 1 h in air. The crack-healing ability of Al2O3/SiC composite ceramics was the best in additive powder 3 wt.% Y2O3. (C) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:672 / 675
页数:4
相关论文
共 16 条
[1]   Effect of crack-healing and proof-testing procedures on fatigue strength and reliability of Si3N4/SiC composites [J].
Ando, K ;
Chu, MC ;
Matsushita, S ;
Sato, S .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (06) :977-984
[2]   Crack-healing behavior of Si3N4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature [J].
Ando, K ;
Takahashi, K ;
Nakayama, S ;
Saito, S .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (09) :2268-2272
[3]   (Crack-healing plus proof test): a new methodology to guarantee the structural integrity of a ceramics component [J].
Ando, K ;
Shirai, Y ;
Nakatani, M ;
Kobayashi, Y ;
Sato, S .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (01) :121-128
[4]   CRACK HEALING BEHAVIOR OF HOT-PRESSED SILICON-NITRIDE DUE TO OXIDATION [J].
CHOI, SR ;
TIKARE, V .
SCRIPTA METALLURGICA ET MATERIALIA, 1992, 26 (08) :1263-1268
[5]  
CHOI SR, 1976, SCRIPTA METALL MATER, V59, P259
[6]   Effect of sintering additives on the oxidation behavior of Si3N4 ceramics at 1300°C [J].
Houjou, K ;
Ando, K ;
Chu, MC ;
Liu, SP ;
Sato, S .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (05) :559-567
[7]  
*JAP STAND ASS, 1995, R1607 JAP STAND ASS
[8]  
Kim B. S., 2003, J SOC MAT SCI JPN, V52, P667
[9]   OXIDATION BEHAVIOR AND EFFECTS OF OXIDATION ON THE STRENGTH OF SIC-WHISKER REINFORCED ALUMINA [J].
KIM, HE ;
MOORHEAD, AJ .
JOURNAL OF MATERIALS SCIENCE, 1994, 29 (06) :1656-1661
[10]  
Kim HW, 1999, J AM CERAM SOC, V82, P1601