An EIS study on the capacity fades in MmNi3.6Al0.4Mn0.3Co0.7 metal-hydride electrodes

被引:20
作者
Raju, M. [1 ]
Manimaran, K. [1 ]
Ananth, Mx [1 ]
Renganathan, N. G. [1 ]
机构
[1] Cent Electrochem Res Inst, Karaikkudi 630006, Tamil Nadu, India
关键词
hydrogen storage alloys; Ni/MH batteries; cyclic stability; impedance measurements; electrochemical kinetics;
D O I
10.1016/j.ijhydene.2006.09.035
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Capacity fade, generally observed in metal-hydride electrodes of nickel metal-hydride batteries with prolonged cycling, is a problem of concern. To investigate the capacity fade, electrochemical impedance spectroscopy (EIS) measurements were performed in lanthanum rich mischmetal alloy (MmNi(3.6)Al(0.4)Mn(0.3)Co(0.7)) electrodes. The impedance measurements were conducted during charging at different stages of cycle life. A novel approach was made to. get reaction resistances and limiting currents from impedance data based on an equivalent circuit for finite spherical hydrogen diffusion. The main cause of the capacity fade occurring in metal-hydride electrodes with number of cycles was due to particle pulverization and consequent poor hydrogen desorption kinetics, thereby making it more difficult for hydrogenation to occur because of passivation and resistance of electron conduction between the alloy particles. (C) 2006 International Association for Hydrogen Energy. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1721 / 1727
页数:7
相关论文
共 29 条
[1]   The influence of cobalt on the electrochemical cycling stability of LaNi5-based hydride forming alloys [J].
Chartouni, D ;
Meli, F ;
Zuttel, A ;
Gross, K ;
Schlapbach, L .
JOURNAL OF ALLOYS AND COMPOUNDS, 1996, 241 (1-2) :160-166
[2]   Study of early cycling deterioration of a Ni/MH battery by electrochemical impedance spectroscopy [J].
Cheng, S ;
Zhang, JQ ;
Liu, H ;
Leng, YJ ;
Yuan, AB ;
Cao, CN .
JOURNAL OF POWER SOURCES, 1998, 74 (01) :155-157
[3]   Hydrogen storage properties of Zr0.8Ti0.2(Ni0.6Mn0.3-xV0.1+xCr0.05)2 (x=0.0, 0.05, 0.15, 0.2) alloys [J].
Du, YL ;
Yang, XG ;
Lei, YQ ;
Zhang, MS .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2002, 27 (06) :695-697
[4]   Pulverization and corrosion studies of bare and cobalt-encapsulated metal hydride electrodes [J].
Durairajan, A ;
Haran, BS ;
White, RE ;
Popov, BN .
JOURNAL OF POWER SOURCES, 2000, 87 (1-2) :84-91
[5]   Hydrogen adsorption of metal nickel and hydrogen storage alloy electrodes [J].
Gao, XP ;
Liu, J ;
Ye, SH ;
Song, DY ;
Zhang, YS .
JOURNAL OF ALLOYS AND COMPOUNDS, 1997, 253 :515-519
[6]   Determination of the hydrogen diffusion coefficient in metal hydrides by impedance spectroscopy [J].
Haran, BS ;
Popov, BN ;
White, RE .
JOURNAL OF POWER SOURCES, 1998, 75 (01) :56-63
[7]   Studies on cobalt-free AB5-type hydrogen storage alloys [J].
Hu, WK .
JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 289 (1-2) :299-305
[8]   A single particle investigation on the kinetics of metal hydride materials [J].
Johnsen, SE ;
Lindbergh, G ;
Lundqvist, A ;
Tunold, R .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (05) :A629-A637
[9]   Electrochemical behavior of metal hydrides [J].
Kleperis, J ;
Wójcik, G ;
Czerwinski, A ;
Skowronski, J ;
Kopczyk, M ;
Beltowska-Brzezinska, M .
JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2001, 5 (04) :229-249
[10]   ELECTROCHEMICAL IMPEDANCE AND DETERIORATION BEHAVIOR OF METAL HYDRIDE ELECTRODES [J].
KURIYAMA, N ;
SAKAI, T ;
MIYAMURA, H ;
UEHARA, I ;
ISHIKAWA, H ;
IWASAKI, T .
JOURNAL OF ALLOYS AND COMPOUNDS, 1993, 202 :183-197