Contribution of mixture design to chemical and autogenous shrinkage of concrete at early ages

被引:142
作者
Holt, E [1 ]
机构
[1] Tech Res Ctr Finland, Espoo 02044, Finland
基金
美国国家科学基金会;
关键词
autogenous deformation; curing; fresh concrete; shrinkage;
D O I
10.1016/j.cemconres.2004.05.009
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this work, autogenous shrinkage at early ages (< 24 h) was accurately measured by linear displacements on slabs simulating field constructions. The best correlation of the amount of chemical to autogenous shrinkage was found at the time of 4 h after the final setting time. It was possible to account for test arrangement artifacts, such as thermal dilation, to get a measure of pure autogenous shrinkage. Many material parameters, such as superplasticizer (SP) and aggregate amount, effected the magnitude of autogenous shrinkage in secondary ways. These consequential effects, such as amount of bleed water and time of setting, were accounted for in the slab measurements. Recommendations are given for reducing the likelihood of cracking due to early age chemical and autogenous shrinkage. (c) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:464 / 472
页数:9
相关论文
共 22 条
[1]  
*ACI, 1997, 20992 ACI
[2]  
[Anonymous], 2001, THESIS U WASHINGTON
[3]  
[Anonymous], 1934, GROWTH MOVEMENT PORT
[4]  
[Anonymous], 1999, AUTOGEN SHRINKAGE CO
[5]  
BAROGHELBOUNY V, 1996, P SEM RILEM BENT MAT
[6]  
Bjontegaard O., 1999, THESIS NORWEGIAN U S
[7]  
Byfors J., 1980, 380 SWED CEM CONCR R
[8]  
Emborg M., 1989, THESIS LULEA U TECHN
[9]  
Hammer T., 1999, Autogenous shrinkage of concrete, P143
[10]  
HEDLUND H, 1996, THESIS LULEA U TECHN