Effects of Long-Term Service on Microstructure and Impact Toughness of the Weld Metal and Heat-Affected Zone in CrMoV Steel Joints

被引:5
作者
Sun, Qixing [1 ,2 ]
Li, Xiaogang [1 ,2 ]
Li, Kejian [1 ,2 ]
Cai, Zhipeng [1 ,2 ,3 ,4 ]
Han, Chaoyu [1 ,2 ]
Li, Shanlin [1 ,2 ]
Gao, Dangxun [5 ]
Pan, Jiluan [1 ,2 ]
机构
[1] Tsinghua Univ, Dept Mech Engn, Beijing 100084, Peoples R China
[2] Minist Educ, Key Lab Adv Mat Proc Technol, Beijing 100084, Peoples R China
[3] Tsinghua Univ, State Key Lab Tribol, Beijing 100084, Peoples R China
[4] Tsinghua Univ, Collaborat Innovat Ctr Adv Nucl Energy Technol, Beijing 100084, Peoples R China
[5] Tsinghua Univ, Fundamental Ind Training Ctr, Beijing 100084, Peoples R China
基金
中国国家自然科学基金;
关键词
weld metal; heat-affected zone; long-term service; phosphorus segregation; toughness; GRAIN-BOUNDARY SEGREGATION; TEMPER EMBRITTLEMENT; MECHANICAL-PROPERTIES; FRACTURE-TOUGHNESS; THERMAL HISTORY; PHOSPHORUS; TENSILE;
D O I
10.3390/met12020278
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure and impact toughness of weld metals (WMs) and heat-affected zones (HAZs) of a low-alloy CrMoV steel gas turbine rotor which had served for 14 years were investigated. The ex-service joints in the turbine part (serving at 500-540 degrees C) and the compressor part (serving below 300 degrees C) of the rotor were selected for comparative research. The microstructure of the WMs and HAZs between the turbine part and the compressor part was similar, indicating that there was no significant deterioration in microstructure of the turbine part during service. However, compared with the compressor part WM, the impact energy of the turbine part WM decreased significantly, and FATT(50) increased greatly. The degraded toughness of turbine part WM was related to more serious intergranular cracking caused by higher segregation level of phosphorus (P) at prior austenite grain (PAG) boundaries. Welding and post-weld heat treatment led to obvious segregation of P at PAG boundaries in WMs, and the segregation of P in turbine part WM was further aggravated during serving at 500-540 degrees C. Additionally, the inhomogeneous microstructure of the WMs also aggravated the segregation of P. The toughness of the HAZs in both turbine part and compressor part was high, which was because of fine grains. Furthermore, due to there being more grain boundaries and low P content, the segregation of P in HAZs was slight and its adverse effect on the toughness could be ignored.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] Critical assessment 42: acicular ferrite formation and its influence on weld metal and heat-affected zone properties of steels
    Cho, Lawrence
    Tselikova, Anastasiya
    Holtgrewe, Kelsey
    De Moor, Emmanuel
    Schmidt, Rolf
    Findley, Kip O.
    MATERIALS SCIENCE AND TECHNOLOGY, 2022, 38 (17) : 1425 - 1433
  • [22] Effect of initial grain size on microstructure and toughness of intercritical heat-affected zone of a low carbon steel
    Eroglu, M.
    Aksoy, M.
    Materials Science and Engineering: A, 2000, 286 (02) : 289 - 297
  • [23] Microstructure model for the heat-affected zone of X80 linepipe steel
    Garcin, T.
    Militzer, M.
    Poole, W. J.
    Collins, L.
    MATERIALS SCIENCE AND TECHNOLOGY, 2016, 32 (07) : 708 - 721
  • [24] Steel 09Mn2SiA-A Welded Joints Heat-Affected Zone Microstructure and Properties
    Bazaras, Z.
    Timofeev, B.
    Bykovskiy, N.
    Vasilieva, N.
    MECHANIKA 2012: PROCEEDINGS OF THE 17TH INTERNATIONAL CONFERENCE, 2012, : 27 - +
  • [25] Metallurgical Effects of Niobium and Molybdenum on Heat-Affected Zone Toughness in Low-Carbon Steel
    Mohrbacher, Hardy
    APPLIED SCIENCES-BASEL, 2019, 9 (09):
  • [26] Effect of tempering heat treatment on the microstructure and impact toughness of a Ni-Cr-Mo-V steel weld metal
    Han, Chaoyu
    Liu, Qu
    Cai, Zhipeng
    Sun, Qixing
    Huo, Xin
    Fan, Manjie
    He, Yi
    Li, Kejian
    Pan, Jiluan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
  • [27] Toughness of heat-affected zone of 800 Mpa grade low alloy steel
    Zhao, L
    Zhang, XD
    Chen, WH
    ACTA METALLURGICA SINICA, 2005, 41 (04) : 392 - 396
  • [28] Microstructure of intercritical heat affected zone and toughness of microalloyed steel laser welds
    Derevyagina, L. S.
    Gordienko, A. I.
    Orishich, A. M.
    Malikov, A. G.
    Surikova, N. S.
    Volochaev, M. N.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 770
  • [29] Microstructure and Impact Toughness of Welding Heat-Affected Zones of a Fe-Cr-Ni-Mo High Strength Steel
    Wen Mingyue
    Dong Wenchao
    Pang Huiyong
    Lu Shanping
    ACTA METALLURGICA SINICA, 2018, 54 (04) : 501 - 511
  • [30] Role of Carbon Content on Microstructure Evolution and Impact Toughness in Coarse-Grained Heat-Affected Zone of High-Strength Steel
    Wang, Xuelin
    Xie, Zhenjia
    Su, Wenjuan
    Shang, Chengjia
    METALS, 2023, 13 (01)