Effects of Long-Term Service on Microstructure and Impact Toughness of the Weld Metal and Heat-Affected Zone in CrMoV Steel Joints

被引:5
作者
Sun, Qixing [1 ,2 ]
Li, Xiaogang [1 ,2 ]
Li, Kejian [1 ,2 ]
Cai, Zhipeng [1 ,2 ,3 ,4 ]
Han, Chaoyu [1 ,2 ]
Li, Shanlin [1 ,2 ]
Gao, Dangxun [5 ]
Pan, Jiluan [1 ,2 ]
机构
[1] Tsinghua Univ, Dept Mech Engn, Beijing 100084, Peoples R China
[2] Minist Educ, Key Lab Adv Mat Proc Technol, Beijing 100084, Peoples R China
[3] Tsinghua Univ, State Key Lab Tribol, Beijing 100084, Peoples R China
[4] Tsinghua Univ, Collaborat Innovat Ctr Adv Nucl Energy Technol, Beijing 100084, Peoples R China
[5] Tsinghua Univ, Fundamental Ind Training Ctr, Beijing 100084, Peoples R China
基金
中国国家自然科学基金;
关键词
weld metal; heat-affected zone; long-term service; phosphorus segregation; toughness; GRAIN-BOUNDARY SEGREGATION; TEMPER EMBRITTLEMENT; MECHANICAL-PROPERTIES; FRACTURE-TOUGHNESS; THERMAL HISTORY; PHOSPHORUS; TENSILE;
D O I
10.3390/met12020278
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure and impact toughness of weld metals (WMs) and heat-affected zones (HAZs) of a low-alloy CrMoV steel gas turbine rotor which had served for 14 years were investigated. The ex-service joints in the turbine part (serving at 500-540 degrees C) and the compressor part (serving below 300 degrees C) of the rotor were selected for comparative research. The microstructure of the WMs and HAZs between the turbine part and the compressor part was similar, indicating that there was no significant deterioration in microstructure of the turbine part during service. However, compared with the compressor part WM, the impact energy of the turbine part WM decreased significantly, and FATT(50) increased greatly. The degraded toughness of turbine part WM was related to more serious intergranular cracking caused by higher segregation level of phosphorus (P) at prior austenite grain (PAG) boundaries. Welding and post-weld heat treatment led to obvious segregation of P at PAG boundaries in WMs, and the segregation of P in turbine part WM was further aggravated during serving at 500-540 degrees C. Additionally, the inhomogeneous microstructure of the WMs also aggravated the segregation of P. The toughness of the HAZs in both turbine part and compressor part was high, which was because of fine grains. Furthermore, due to there being more grain boundaries and low P content, the segregation of P in HAZs was slight and its adverse effect on the toughness could be ignored.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Near-threshold fatigue crack growth behavior of the weld metal and heat-affected zone in an ex-service CrMoV steel joint
    Sun, Qixing
    Liu, Qu
    Li, Xiaogang
    Cai, Zhipeng
    Huo, Xin
    Fan, Manjie
    He, Yi
    Yao, Xinzhe
    Pan, Jiluan
    Li, Kejian
    INTERNATIONAL JOURNAL OF FATIGUE, 2022, 164
  • [2] A toughness study of the weld heat-affected zone of a 9Cr-1Mo steel
    Moitra, A
    Parameswaran, P
    Sreenivasan, PR
    Mannan, SL
    MATERIALS CHARACTERIZATION, 2002, 48 (01) : 55 - 61
  • [3] Microstructure and toughness of heat-affected zone of weld joint for pipeline steels with high deformability
    Jia S.
    Wang Y.
    Tan F.
    Liu Q.
    Cailiao Yanjiu Xuebao, 7 (517-523): : 517 - 523
  • [4] INFLUENCE OF MARTENSITIC ISLANDS ON FRACTURE-TOUGHNESS AND STRENGTH OF WELD HEAT-AFFECTED ZONE
    TAGAWA, T
    MIYATA, T
    AIHARA, S
    OKAMOTO, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1993, 79 (10): : 1176 - 1182
  • [5] Fracture Toughness Evaluation of the Heat-Affected Zone Under the Weld Overlay Cladding in Reactor Pressure Vessel Steel
    Ha, Yoosung
    Tobita, Tohru
    Takamizawa, Hisashi
    Katsuyama, Jinya
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 2023, 145 (02):
  • [6] Microstructure and Toughness of Simulated Heat-Affected Zone of Laser Welded Joint for 960 MPa Grade High Strength Steel
    Meng, Wei
    Li, Zhuguo
    Jiang, Xiaoxia
    Huang, Jian
    Wu, Yixiong
    Katayama, Seiji
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (10) : 3640 - 3648
  • [7] Eliminating the Brittleness Constituent to Enhance Toughness of the High-Strength Steel Weld Heat-Affected Zone Using Electropulsing
    Chen, Zhanglan
    Xiong, Yunfeng
    Li, Xiaowen
    Li, Zongmin
    MATERIALS, 2022, 15 (06)
  • [8] Effect of Mg Treatment on Refining the Microstructure and Improving the Toughness of the Heat-Affected Zone in Shipbuilding Steel
    Wang, Yan
    Zhu, Liguang
    Zhang, Qingjun
    Zhang, Caijun
    Wang, Shuoming
    METALS, 2018, 8 (08):
  • [9] Effect of weld thermal cycle on microstructure and fracture toughness of simulated heat-affected zone for a 800 MPa grade high strength low alloy steel
    Shi, Yaowu
    Han, Zhunxiang
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 207 (1-3) : 30 - 39
  • [10] MICROSTRUCTURE AND MECHANICAL PROPERTIES OF CRMOV STEEL AFTER LONG-TERM SERVICE
    Golanski, G.
    Pietryka, I.
    Slania, J.
    Mrozinski, S.
    Jasak, J.
    ARCHIVES OF METALLURGY AND MATERIALS, 2016, 61 (01) : 51 - 54