Residual properties of steel slag coarse aggregate concrete after exposure to elevated temperatures

被引:91
作者
Ho, J. C. M. [1 ]
Liang, Y. [1 ]
Wang, Y. H. [2 ,3 ]
Lai, M. H. [1 ]
Huang, Z. C. [1 ]
Yang, D. [1 ]
Zhang, Q. L. [1 ]
机构
[1] Guangzhou Univ, Sch Civil Engn, Guangzhou, Guangdong, Peoples R China
[2] Chongqing Univ, Sch Civil Engn, Chongqing, Peoples R China
[3] Chongqing Univ, Minist Educ, Key Lab New Technol Construct Cities Mt Area, Chongqing, Peoples R China
基金
中国国家自然科学基金;
关键词
Elevated temperature; Green concrete; Replacement ratio; Residual properties; Steel slag; HIGH-STRENGTH CONCRETE; PACKING DENSITY; CEMENTITIOUS MATERIALS; MECHANICAL-PROPERTIES; BEHAVIOR; COLUMNS; FLOWABILITY; FILLERS; MGO;
D O I
10.1016/j.conbuildmat.2021.125751
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Steel slag, waste by-product during steelmaking process, has great potential in concrete production. Over the past few decades, extensive research studies were conducted on the mechanical behaviour and chemical property of concrete made with steel slag at ambient temperature. However, relatively little effort has been put to study the behaviour of concrete with steel slag after exposure to elevated temperatures. To fill up this research gap, an experimental study was conducted in which five concrete mixes with steel slag replacing natural coarse aggregate (crushed granite) were prepared. The effect of slag replacement ratio by volume (0%, 25%, 50%, 75% and 100%) on the heating behaviour, residual compressive strength, weight loss and surface texture of concrete under curing period of 28 and 91 days, after exposure to 25 degrees C (ambient temperature), 400 degrees C, 600 degrees C, 800 degrees C and 1000 degrees C was investigated. Besides, chemical deterioration behaviour was studied using X-ray diffraction analysis. From the test results, it is evident that with steel slag partially or totally replacing crushed granite, the heat insulation ability of concrete could be enhanced. Moreover, the residual strength of concrete with slag replacement ratio of 100% after exposure to elevated temperatures >= 600 degrees C would be comparable to concrete with crushed granite only. Lastly, the design model by EC2 was adopted to predict the residual strength of concrete with and without slag and results demonstrated that EC2 was conservative.
引用
收藏
页数:17
相关论文
共 88 条
[11]   Beam-column tests of cold-formed steel elliptical hollow sections [J].
Chen, Man-Tai ;
Young, Ben .
ENGINEERING STRUCTURES, 2020, 210
[12]  
Consolazio GR, 1998, ACI MATER J, V95, P525
[13]   Thermodynamic behaviour of grossular-andradite, Ca3(AlxFe1-x3+)2Si3O12, garnets: a calorimetric study [J].
Dachs, Edgar ;
Geiger, Charles A. .
EUROPEAN JOURNAL OF MINERALOGY, 2019, 31 (03) :443-451
[14]   Properties of concrete manufactured using steel slag [J].
Devi, V. Subathra ;
Gnanavel, B. K. .
12TH GLOBAL CONGRESS ON MANUFACTURING AND MANAGEMENT (GCMM - 2014), 2014, 97 :95-104
[15]   Characterization of high strength mortars with nano Titania at elevated temperatures [J].
Farzadnia, Nima ;
Ali, Abang Abdullah Abang ;
Demirboga, Ramazan ;
Anwar, Mohammed Parvez .
CONSTRUCTION AND BUILDING MATERIALS, 2013, 43 :469-479
[16]  
Feldman R.F., 1971, Cement and Concrete Research, V16, P607
[17]   Impact of High Temperature on Residual Properties of Concrete with Steel Slag Aggregate [J].
Grubesa, Ivanka Netinger ;
Rukavina, Marija Jelcic ;
Mladenovic, Ana .
JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2016, 28 (06)
[18]   Steel slag in China: Treatment, recycling, and management [J].
Guo, Jianlong ;
Bao, Yanping ;
Wang, Min .
WASTE MANAGEMENT, 2018, 78 :318-330
[19]   Effective usage of high strength steel tubes: Axial compressive behavior of hybrid FRP-concrete-steel solid columns [J].
Guo, Yong-Chang ;
Ye, Yu-Yi ;
Guan-Lin ;
Lv, Jun-Fan ;
Bai, Yu-Lei ;
Zeng, Jun-Jie .
THIN-WALLED STRUCTURES, 2020, 154
[20]   Behaviour of cement concrete at high temperature [J].
Hager, I. .
BULLETIN OF THE POLISH ACADEMY OF SCIENCES-TECHNICAL SCIENCES, 2013, 61 (01) :145-154