Relationship between test severity and wear mode transition in micro-abrasive wear tests

被引:49
作者
Cozza, R. C.
de Mello, J. D. B.
Tanaka, D. K.
Souza, R. M.
机构
[1] Univ Sao Paulo, Polytech Sch, Surface Phenomena Lab, Dept Mech Engn, BR-05508900 Sao Paulo, Brazil
[2] Univ Fed Uberlandia, Mech Engn Coll, Tribol & Mat Lab, BR-38400902 Uberlandia, MG, Brazil
关键词
micro-abrasive wear testing; wear modes; rolling abrasion; grooving abrasion; test severity;
D O I
10.1016/j.wear.2007.01.099
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Recently, the micro-scale abrasive wear test has gained large acceptance in universities and research centers, being widely used in studies on the abrasive wear of materials. The purpose of this work is to relate a quantity called test severity (S-test) with the abrasive wear mode transition. The analysis took into consideration the hardness of the materials; the contact pressure (P) between the specimen and the ball and the equipment configuration (fixed-ball or free-ball). Tests were conducted with balls of AISI 52100 steel and specimens of ISO P20 cemented carbide (WC-Co) and AISI M2 tool steel. The abrasive slurry was prepared with black silicon carbide (SiC) particles (average particle size of 5 mu m) and distilled water. The results were analyzed in plots of S-test and A(g)/A(p) as a function of test time (t) and V as a function of P, where A(g) is the projected area fraction with grooving abrasion; A(p) the total projected area and V is the volume of the worn crater. The results allowed observing that the value of S-test decreased from the beginning to the end of all tests, When the results obtained with fixed-ball and free-ball equipment were compared, this decrease in S-test was similar in the case of the WC-Co specimen, for which the hardness of the specimen (H-S) was larger than the hardness of the ball (H-b). The decrease in S-test was different in the case of the AISI M2 specimen, for which H-S < H-b. Tests were also associated with a decrease in the ratio Ag/Ap as a function of test time. A transition from mixed mode into pure rolling abrasion occurred at similar test times in the cases with similar severity evolution and, for the AISI M2 specimen, occurred earlier for the condition with lower test severity. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:111 / 116
页数:6
相关论文
共 37 条
[21]   Ball crater testing for the measurement of the unlubricated sliding wear of wear-resistant coatings [J].
Gee, MG ;
Wicks, MJ .
SURFACE & COATINGS TECHNOLOGY, 2000, 133 :376-382
[22]  
Izhevskyi V. A., 2004, Cerâmica, V50, P261, DOI 10.1590/S0366-69132004000300014
[23]   EFFECT OF RESIDUAL-STRESSES ON THE STRENGTH, ADHESION AND WEAR-RESISTANCE OF SIC COATINGS OBTAINED BY PLASMA-ENHANCED CHEMICAL-VAPOR-DEPOSITION ON LOW-ALLOY STEEL [J].
KATTAMIS, TZ ;
CHEN, M ;
SKOLIANOS, S ;
CHAMBERS, BV .
SURFACE & COATINGS TECHNOLOGY, 1994, 70 (01) :43-48
[24]   Sources of variability in the free-ball micro-scale abrasion test [J].
Kusano, Y ;
Hutchings, IM .
WEAR, 2005, 258 (1-4) :313-317
[25]  
Mergler YJ, 2003, TRIBOLOGICAL RESEARCH AND DESIGN FOR ENGINEERING SYSTEMS, P165
[26]  
OBERG E, 2000, MACH HDB
[28]   A micro-abrasive wear test, with particular application to coated systems [J].
Rutherford, KL ;
Hutchings, IM .
SURFACE & COATINGS TECHNOLOGY, 1996, 79 (1-3) :231-239
[29]  
Rutherford KL, 1997, J TEST EVAL, V25, P250, DOI 10.1520/JTE11487J
[30]   Dependence of microscale abrasion mechanisms of WC-Co hardmetals on abrasive type [J].
Shipway, PH ;
Hogg, JJ .
WEAR, 2005, 259 (1-6) :44-51