Hydrogen embrittlement behavior of Inconel 718 alloy at room temperature

被引:36
作者
Li, Xinfeng [1 ]
Zhang, Jin [2 ]
Akiyama, Eiji [3 ]
Fu, Qinqin [4 ]
Li, Qizhen [1 ]
机构
[1] Washington State Univ, Sch Mech & Mat Engn, Pullman, WA 99164 USA
[2] SUNY Stony Brook, Dept Geosci, Stony Brook, NY 11794 USA
[3] Tohoku Univ, Inst Mat Res, Mat Design Div, Sendai, Miyagi 9808577, Japan
[4] Xi An Jiao Tong Univ, State Key Lab Mech Behav Mat, Sch Mat Sci & Engn, Xian 710049, Peoples R China
关键词
Embrittlement; Hydrogen in metals; Inconel; 718; alloy; Portevin-Le Chatelier effect; MECHANICAL-PROPERTIES; STRAIN; FRACTURE; DEFORMATION; MICROSTRUCTURE; PRECIPITATION; CRACKING; STRESS;
D O I
10.1016/j.jmst.2018.10.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hydrogen embrittlement of Inconel 718 alloy was investigated. Multi-scale observation technique were employed, comprising slow strain rate tensile tests, scanning electron microscopy and transmission electron microscopy analysis. The results demonstrate that hydrogen charging deteriorates mechanical properties of the alloy. Inconel 718 alloy shows partial Portevin-Le Chatelier (PLC) effect at room temperature when hydrogen charging current density is 220 mA cm(-2) and 590 mA cm(-2). Moreover, plastic deformation features with dislocation cells are detected in hydrogen-induced brittle zone. Thus, it is concluded that dragging effect of hydrogen atoms on dislocations contributes to PLC effect. (C) 2019 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:499 / 502
页数:4
相关论文
共 28 条
[11]   Slow Strain Rate Testing for Hydrogen Embrittlement Susceptibility of Alloy 718 in Substitute Ocean Water [J].
LaCoursiere, M. P. ;
Aidun, D. K. ;
Morrison, D. J. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (05) :2337-2345
[12]   Tensile mechanical properties and fracture behaviors of nickel-based superalloy 718 in the presence of hydrogen [J].
Li, Xinfeng ;
Zhang, Jin ;
Fu, Qinqin ;
Akiyama, Eiji ;
Song, Xiaolong ;
Wang, Yanfei ;
Li, Qizhen ;
Zou, Ning .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2018, 43 (43) :20118-20132
[13]   Effect of heat treatment on hydrogen-assisted fracture behavior of PH13-8Mo steel [J].
Li, Xinfeng ;
Zhang, Jin ;
Akiyama, Eiji ;
Li, Qizhen ;
Wang, Yanfei .
CORROSION SCIENCE, 2017, 128 :198-212
[14]   The dual role of shot peening in hydrogen-assisted cracking of PSI31080 high strength steel [J].
Li, Xinfeng ;
Zhang, Jin ;
Wang, Yanfei ;
Ma, Mingming ;
Shen, Sicong ;
Song, Xiaolong .
MATERIALS & DESIGN, 2016, 110 :602-615
[15]   Effect of aging treatment on hydrogen embrittlement of PH 13-8 Mo martensite stainless steel [J].
Li, Xinfeng ;
Zhang, Jin ;
Chen, Jing ;
Shen, Sicong ;
Yang, Gongxian ;
Wang, Tianjian ;
Song, Xiaolong .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 651 :474-485
[16]   Effect of pre-strain on hydrogen embrittlement of high strength steels [J].
Li, Xinfeng ;
Wang, Yanfei ;
Zhang, Peng ;
Li, Bo ;
Song, Xiaolong ;
Chen, Jing .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 616 :116-122
[17]   Effects of precipitation phases on the hydrogen embrittlement sensitivity of Inconel 718 [J].
Liu, Liufa ;
Tanaka, Katsumi ;
Hirose, Akio ;
Kobayashi, Kojiro F. .
SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2002, 3 (04) :335-344
[18]  
LORIA EA, 1992, JOM-J MIN MET MAT S, V44, P33
[19]   Microstructure and Strain-Stress Analysis of the Dynamic Strain Aging in Inconel 625 at High Temperature [J].
Maj, P. ;
Zdunek, J. ;
Mizera, J. ;
Kurzydlowski, K. J. ;
Sakowicz, B. ;
Kaminski, M. .
METALS AND MATERIALS INTERNATIONAL, 2017, 23 (01) :54-67
[20]   Statistical analysis of the Portevin-Le Chatelier effect in Inconel 718 at high temperature [J].
Maj, P. ;
Zdunek, J. ;
Gizynski, M. ;
Mizera, J. ;
Kurzydlowski, K. J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 619 :158-164