In vivo study of magnesium plate and screw degradation and bone fracture healing

被引:299
作者
Chaya, Amy [1 ,2 ,4 ]
Yoshizawa, Sayuri [1 ,3 ]
Verdelis, Kostas [1 ,3 ,4 ]
Myers, Nicole [1 ,3 ]
Costello, Bernard J. [1 ,4 ,5 ]
Chou, Da-Tren [1 ,2 ,4 ]
Pal, Siladitya [2 ]
Maiti, Spandan [2 ]
Kumta, Prashant N. [1 ,2 ,3 ,4 ]
Sfeir, Charles [1 ,2 ,3 ,4 ]
机构
[1] Univ Pittsburgh, Ctr Craniofacial Regenerat, Pittsburgh, PA USA
[2] Univ Pittsburgh, Dept Bioengn, Pittsburgh, PA USA
[3] Univ Pittsburgh, Dept Oral Biol, Pittsburgh, PA USA
[4] Univ Pittsburgh, McGowan Inst Regenerat Med, Pittsburgh, PA USA
[5] Univ Pittsburgh, Dept Oral & Maxillofacial Surg, Pittsburgh, PA USA
基金
美国国家科学基金会;
关键词
Magnesium; Fixation devices; Fracture fixation; MicroCT; ALLOY; CORROSION; IMPLANTS; BEHAVIOR; FIXATION; BIOCOMPATIBILITY; REMOVAL; VITRO;
D O I
10.1016/j.actbio.2015.02.010
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Each year, millions of Americans suffer bone fractures, often requiring internal fixation. Current devices, like plates and screws, are made with permanent metals or resorbable polymers. Permanent metals provide strength and biocompatibility, but cause long-term complications and may require removal. Resorbable polymers reduce long-term complications, but are unsuitable for many load-bearing applications. To mitigate complications, degradable magnesium (Mg) alloys are being developed for craniofacial and orthopedic applications. Their combination of strength and degradation make them ideal for bone fixation. Previously, we conducted a pilot study comparing Mg and titanium devices with a rabbit ulna fracture model. We observed Mg device degradation, with uninhibited healing. Interestingly, we observed bone formation around degrading Mg, but not titanium, devices. These results highlighted the potential for these fixation devices. To better assess their efficacy, we conducted a more thorough study assessing 99.9% Mg devices in a similar rabbit ulna fracture model. Device degradation, fracture healing, and bone formation were evaluated using microcomputed tomography, histology and biomechanical tests. We observed device degradation throughout, and calculated a corrosion rate of 0.40 +/- 0.04 mm/year after 8 weeks. In addition, we observed fracture healing by 8 weeks, and maturation after 16 weeks. In accordance with our pilot study, we observed bone formation surrounding Mg devices, with complete over-growth by 16 weeks. Bend tests revealed no difference in flexural load of healed ulnae with Mg devices compared to intact ulnae. These data suggest that Mg devices provide stabilization to facilitate healing, while degrading and stimulating new bone formation. (C) 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:262 / 269
页数:8
相关论文
共 42 条
[1]  
[Anonymous], 2011, Orthopedic Network News 2011 Trauma Update
[2]   Magnesium-based bone implants: Immunohistochemical analysis of peri-implant osteogenesis by evaluation of osteopontin and osteocalcin expression [J].
Bondarenko, A. ;
Angrisani, N. ;
Meyer-Lindenberg, A. ;
Seitz, J. M. ;
Waizy, H. ;
Reifenrath, J. .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2014, 102 (05) :1449-1457
[3]   FOREIGN-BODY REACTIONS TO FRACTURE FIXATION IMPLANTS OF BIODEGRADABLE SYNTHETIC-POLYMERS [J].
BOSTMAN, O ;
HIRVENSALO, E ;
MAKINEN, J ;
ROKKANEN, P .
JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 1990, 72 (04) :592-596
[4]   Magnesium in the murine artery: Probing the products of corrosion [J].
Bowen, Patrick K. ;
Drelich, Jaroslaw ;
Goldman, Jeremy .
ACTA BIOMATERIALIA, 2014, 10 (03) :1475-1483
[5]   Hardware removal: Indications and expectations [J].
Busam, ML ;
Esther, RJ ;
Obremskey, WT .
JOURNAL OF THE AMERICAN ACADEMY OF ORTHOPAEDIC SURGEONS, 2006, 14 (02) :113-120
[6]   Fracture Healing Using Degradable Magnesium Fixation Plates and Screws [J].
Chaya, Amy ;
Yoshizawa, Sayuri ;
Verdelis, Kostas ;
Noorani, Sabrina ;
Costello, Bernard J. ;
Sfeir, Charles .
JOURNAL OF ORAL AND MAXILLOFACIAL SURGERY, 2015, 73 (02) :295-305
[7]   In vitro and in vivo corrosion, cytocompatibility and mechanical properties of biodegradable Mg-Y-Ca-Zr alloys as implant materials [J].
Chou, Da-Tren ;
Hong, Daeho ;
Saha, Partha ;
Ferrero, Jordan ;
Lee, Boeun ;
Tan, Zongqing ;
Dong, Zhongyun ;
Kumta, Prashant N. .
ACTA BIOMATERIALIA, 2013, 9 (10) :8518-8533
[8]   Current insights on the regenerative potential of the periosteum: Molecular, cellular, and endogenous engineering approaches [J].
Colnot, Celine ;
Zhang, Xinping ;
Tate, Melissa L. Knothe .
JOURNAL OF ORTHOPAEDIC RESEARCH, 2012, 30 (12) :1869-1878
[9]   Influence of stress on the degradation behavior of Mg LAE442 implant systems [J].
Denkena, B. ;
Koehler, J. ;
Stieghorst, J. ;
Turger, A. ;
Seitz, J. ;
Fau, D. R. ;
Wolters, L. ;
Angrisani, N. ;
Reifenrath, J. ;
Helmecke, P. .
FIRST CIRP CONFERENCE ON BIOMANUFACTURING, 2013, 5 :189-195
[10]   Biomechanical testing and degradation analysis of MgCa0.8 alloy screws: A comparative in vivo study in rabbits [J].
Erdmann, Nina ;
Angrisani, Nina ;
Reifenrath, Janin ;
Lucas, Arne ;
Thorey, Fritz ;
Bormann, Dirk ;
Meyer-Lindenberg, Andrea .
ACTA BIOMATERIALIA, 2011, 7 (03) :1421-1428